journal article·2021-02

Fabrication and joining mechanism of Nano-Cu/Si3N4 ceramic substrates

Chenglai Xin, Rong Yuan, Jiang Wu, Qingyuan Wang, Yanan Zhou

Ceramics International· Volume 47· Issue 3
Publisher page

Abstract

Abstract A novel method for fabricating a nano-Cu/Si3N4 ceramic substrate is proposed. The nano-Cu/Si3N4 ceramic substrate is first fabricated using spark plasma sintering (SPS) with the addition of nanoscale multilayer films (Ti/TiN/Ti/TiN/Ti) as transition layers. The microstructures of the nano-Cu metal layer and the interface between Cu and Si3N4 are investigated. The results show that a higher SPS temperature increases the grain size of the nano-Cu metal layer and affects the hardness. The microstructure of the transition layer evolves significantly after SPS. Ti in the transition layer can react with Si3N4 and with nano-Cu to form interfacial reaction layers of TiN and Ti–Cu, respectively; these ensure stronger bonding between nano-Cu and Si3N4. Higher SPS temperatures improve the diffusion ability of Ti and Cu, inducing the formation of Ti3Cu3O compounds in the nano-Cu metal layer and Ti2Cu in the transition layer. This study provides an important strategy for designing and constructing a new type of ceramic substrate.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Aluminum Alloys Composites Properties · Advanced ceramic materials synthesis · Advanced materials and composites

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (35)

Show source-provided references
1. Silver nanoparticle-based thermal interface materials with ultra-low thermal resistance for power electronics applications10.1016/j.scriptamat.2012.02.037 ↗
2. Analysis of the BGA solder Sn–3.0Ag–0.5Cu crack interface and a prediction of the fatigue life under tensile stress10.1016/j.ijfatigue.2016.02.003 ↗
3. Effect of mechanical properties of the ceramic substrate on the thermal fatigue of Cu metallized ceramic substrates
4. Effects of extreme temperature swings (−55 ◦C to 250 ◦C) on silicon nitride active metal brazing substrates10.1109/TDMR.2014.2320057 ↗
5. Morphology of thick film metallization on aluminum nitride ceramics and composition of interface layer10.1016/j.ceramint.2015.07.125 ↗
6. Microstructure evolution and mechanical properties of a vacuum-brazed Al2O3/Ti joint with Mo-coating on Al2O3 and Ti surfaces10.1016/j.ceramint.2019.01.163 ↗
7. Pressureless low-temperature sintering of plasma activated Ag nanoparticles for high-power device packaging10.1016/j.matlet.2019.126620 ↗
8. Interfacial investigation and mechanical properties of glass-Al-glass anodic bonding process10.1088/1361-6439/aa83c7 ↗
9. Strain rate sensitive stretchability and fracture behavior of nanocrystalline Cu films on flexible substrate10.1016/j.msea.2012.01.006 ↗
10. Failure by simultaneous grain growth, strain localization, and interface debonding in metal films on polymer substrates10.1557/JMR.2009.0048 ↗
11. Mechanical behavior of nanocrystalline metals and alloys10.1016/j.actamat.2003.08.032 ↗
12. Hardness and strain rate sensitivity of nanocrystalline Cu10.1016/j.scriptamat.2006.02.022 ↗
13. Hall-Petch relationship in pulsed laser deposited nickel films10.1557/jmr.2004.19.1.218 ↗
14. Some critical experiments on the strain-rate sensitivity of nanocrystalline nickel10.1016/S1359-6454(03)00365-3 ↗
15. Effect of nanocrystalline and ultrafine grain sizes on the strain rate sensitivity and activation volume: fcc versus bcc metals10.1016/j.msea.2004.03.064 ↗
16. Strengthening materials by engineering coherent internal boundaries at the nanoscale10.1126/science.1159610 ↗
17. Influence of Ti–TiN multilayer PVD-coatings design on residual stresses and adhesion10.1016/j.matdes.2015.03.007 ↗
18. Sheng · 2017
19. Effect of mechanical alloying and spark plasma sintering on the microstructure and mechanical properties of ODS Eurofer10.1016/j.matdes.2019.107849 ↗
20. Microstructural evaluation and mechanical properties of in-situ WC/W-Cu composites fabricated by rGO/W-Cu spark plasma sintering reaction10.1016/j.matdes.2018.11.004 ↗
21. Microstructure characteristic and mechanical property of transformable 9Cr-ODS steel fabricated by spark plasma sintering10.1016/j.matdes.2017.06.063 ↗
22. Fabrication of nano-grained Ti–Nb–Zr biomaterials using spark plasma sintering10.1016/j.matdes.2015.08.082 ↗
23. Lin · 2010
24. Thermodynamic evaluation of reaction products and layering in brazed alumina joints10.1557/JMR.1994.2244 ↗
25. Interfacial microstructure and improved wetting mechanism of SiO2f/SiO2 brazed with Nb by plasma treatment10.1016/j.vacuum.2017.06.041 ↗
26. Interfacial microstructure and mechanical properties of TiAl and C/SiC joint brazed with TiH2-Ni-B brazing powder10.1016/j.matchar.2013.02.010 ↗
27. Microstructures and mechanical properties of brazed Al2O3/Cu joints with bismuth glass10.1016/j.ceramint.2019.05.123 ↗
28. Microstructure evolution of Si3N4/Si3N4 joint brazed with Ag–Cu–Ti+SiCp composite filler10.1016/j.ceramint.2010.02.010 ↗
29. Microstructure andmechanical response of the SiO2f/SiO2 composite and Invar alloy joints brazed with an AgCuTi alloy10.1016/j.matdes.2016.08.075 ↗
30. Interfacial microstructure and mechanical property of brazed copper/SiO2 ceramic joint10.1016/j.vacuum.2017.03.037 ↗
31. Interfacial microstructure and mechanical properties of porous-Si3N4 ceramic and TiAl alloy joints vacuum brazed with AgCu filler10.1016/j.ceramint.2017.04.149 ↗
32. An analysis of deformation mechanism in the Si3N4–AgCuTi + SiCp–Si3N4 joints by digital image correlation10.1016/j.jeurceramsoc.2012.07.038 ↗
33. Nanostructure of wetting triple line in a Ag-Cu-Ti/Si3N4 reactive system10.1016/S1359-6454(98)00375-9 ↗
34. Ye · 2002
35. Microstructure and mechanical properties of BN-Si3N4 and AlON joints brazed with Ag-Cu-Ti filler alloy10.1016/j.jeurceramsoc.2017.10.001 ↗