Abstract

Abstract Although Si2BC3N ceramics have excellent oxidation resistance under high temperature (1000–1400 °C) in both dry and moist air, the oxidation resistance under higher temperatures (above 1400 °C) are still challenged due to the quick escape of volatile CO, B2O3 and SiO. Generally, the formation of stable and continuous protective layer is critical for improving the oxidation resistance under high temperature. Given the chemical compatibility and the formation of nonvolatile oxides after oxidation, the present work mainly investigated the influences of disilicides addition, including MoSi2, HfSi2 and TaSi2, on the phase composition and oxidation resistance of Si2BC3N ceramics sintered by SPS. The results showed that nano sized disilicides would transform into carbides (MoC, Mo5Si3, and TaC) and oxides (TaO, HfO2) during sintering process. The preferential oxidation of Mo and Hf related phases and the formation of much stable oxidation layer could improve the oxidation resistance significantly, where the oxidation layer thickness was less than 10 μm after testing at 1600 °C for 3 h.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advanced ceramic materials synthesis · MXene and MAX Phase Materials · Advanced materials and composites

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (47)

Show source-provided references
1. A silicoboron carbonitride ceramic stable to 2000 °C10.1038/382796a0 ↗
2. Synthesis, characterization, and ceramic conversion reactions of borazine/silazane copolymers: new polymeric precursors to silicon nitride carbide boride (SiNCB) ceramic composites10.1021/cm00028a024 ↗
3. Boron-containing polysilylcarbodi-imides: a new class of molecular precursors for Si-B-C-N ceramics10.1016/S0022-328X(97)00085-5 ↗
4. Polymer-derived ceramics: 40 years of research and innovation in advanced ceramics10.1111/j.1551-2916.2010.03876.x ↗
5. Processing and properties of C/Si-B-C-N fiber-reinforced ceramic matrix composites prepared by precursor impregnation and pyrolysis10.1016/j.actamat.2007.12.001 ↗
6. Metastable Si-B-C-N ceramics and their matrix composites developed by inorganic route based on mechanical alloying: fabrication, microstructures, properties and their relevant basic scientific issues10.1016/j.pmatsci.2018.05.006 ↗
7. Processing and characterization of SiB0.5C1.5N0.5 produced by mechanical alloying and subsequent spark plasma sintering10.1016/j.msea.2007.11.012 ↗
8. Microstructures and properties of SiB0.5C1.5N0.5 ceramics consolidated by mechanical alloying and hot pressing10.1016/j.msea.2007.12.010 ↗
9. Ablation behavior and mechanism of SiCf/Cf/Si-B-C-N ceramic composites with improved thermal shock resistance under oxyacetylene combustion flow10.1016/j.ceramint.2015.03.144 ↗
10. Effects of in situ amorphous graphite coating on ablation resistance of SiC fiber reinforced Si-B-C-N ceramics in an oxyacetylene flame10.1016/j.corsci.2016.10.002 ↗
11. Microstructure and mechanical properties of SiCf/Si-B-C-N ceramic matrix composites
12. Strengthening and toughening effects of MWCNTs on Si2BC3N ceramics sintered by SPS technique10.1016/j.msea.2017.10.089 ↗
13. Enhanced mechanical properties and thermal shock resistance of Si2BC3N ceramics with SiC coated MWCNTs10.1007/s40145-018-0300-6 ↗
14. Microstructure, oxidation and thermal shock resistance of graphene reinforced Si-B-C-N ceramics10.1016/j.ceramint.2015.11.127 ↗
15. Mechanical properties and thermal shock resistance of Si2BC3N ceramics with ternary Al4SiC4 additive10.1016/j.ceramint.2018.02.103 ↗
16. Effect of AlN and ZrO2 on the microstructure and property of the 2Si-B-3C-N ceramic10.1016/j.ceramint.2017.11.134 ↗
17. Microstructural evolution, mechanical and thermal properties of LaB6 embedded in Si-B-C-N prepared by spark plasma sintering10.1016/j.ceramint.2016.12.016 ↗
18. Influence of sol-gel derived ZrB2 additions on microstructure and mechanical properties of Si-B-C-N composites10.1016/j.ceramint.2016.12.083 ↗
19. Preparation, microstructures, mechanical properties and oxidation resistance of Si-B-C-N/ZrB2–ZrN ceramics by reactive hot pressing10.1016/j.jeurceramsoc.2015.08.010 ↗
20. Enhanced mechanical properties, thermal shock resistance and ablation resistance of Si2BC3N ceramics with nano ZrB2 addition10.1016/j.jeurceramsoc.2018.12.005 ↗
21. Enhanced mechanical properties, thermal shock resistance and oxidation resistance of Si2BC3N ceramics with Zr-Al addition10.1016/j.msea.2018.04.035 ↗
22. Progress of a novel non-oxide Si-B-C-N ceramic and its matrix composites10.1007/s40145-012-0017-x ↗
23. Progress of a novel amorphous and nanostructured Si-B-C-N ceramic and its matrix composites prepared by an inorganic processing route10.1360/N972014-00502 ↗
24. Amorphous silicoboron carbonitride monoliths resistant to flowing air up to 1800 °C10.1016/j.corsci.2016.03.026 ↗
25. High-temperature oxidation behavior of dense SiBCN monoliths: carbon-content dependent oxidation structure, kinetics and mechanisms10.1016/j.corsci.2017.05.013 ↗
26. Microstructures, mechanical properties and oxidation resistance of SiBCN ceramics with the addition of MgO, ZrO2 and SiO2 (MZS) as sintering additives10.1039/C5RA05605E ↗
27. High-temperature chemistry and oxidation of ZrB2 ceramics containing SiC, Si3N4, Ta5Si3, and TaSi210.1111/j.1551-2916.2008.02420.x ↗
28. Constructing self-healing ZrSi2-MoSi2 coating for C/C composites with enhanced oxidation protective ability10.1016/j.surfcoat.2018.05.002 ↗
29. A novel gradient SiC-ZrB2-MoSi2 coating for SiC coated C/C composites by supersonic plasma spraying10.1016/j.surfcoat.2017.01.019 ↗
30. Ultra-high temperature oxidation resistance of ZrB2-20SiC coating with TaSi2 addition on siliconized graphite10.1016/j.ceramint.2019.05.030 ↗
31. A MoSi2-based composite coating by supersonic atmospheric plasma spraying to protect Nb alloy against oxidation at 1500 °C10.1016/j.surfcoat.2018.07.091 ↗
32. A novel ultra-high-temperature oxidation protective MoSi2-TaSi2 ceramic coating for tantalum substrate10.1016/j.jeurceramsoc.2019.02.037 ↗
33. MoSi2/(Mo,Ti)Si2 dual-phase composite coating for oxidation protection of molybdenum alloy10.1016/j.jallcom.2017.08.173 ↗
34. Combined effects of boron carbide, silicon, and MWCNTs in alumina-carbon refractories on their microstructural evolution10.1111/jace.14543 ↗
35. Calculated C-MoSi2 and B-Mo5Si3 pseudo-binary phase diagrams or the use in advanced materials processing10.1016/S0921-5093(99)00593-6 ↗
36. Microstructure and ablation properties of a gradient Cf/C-XSi2-SiC (X = Mo,Ti) composite fabricated by reactive melt infiltration10.1016/j.jeurceramsoc.2016.04.006 ↗
37. Thermal oxidation kinetics of MoSi2-based powders10.1111/j.1151-2916.1999.tb02156.x ↗
38. High-temperature oxidation and plasma torch testing of MoSi2–HfB2–MoB ceramics with single-level and two-level structure10.1016/j.corsci.2019.07.001 ↗
39. Oxidation response determined by multiphase-dependent melting degree of plasma sprayed MoSi2 on Nb-based alloy10.1016/j.jallcom.2018.05.277 ↗
40. Atomic oxygen damage behavior of TaC coating-modified C/C composite
41. HfC nanowire-toughened TaSi2–TaC–SiC–Si multiphase coating for C/C composites against oxidation10.1016/j.corsci.2014.10.048 ↗
42. Oxidative protection of a carbon-bonded carbon fiber composite with double-layer coating of MoSi2-SiC whisker and TaSi2-MoSi2-SiC whisker by slurry method10.1016/j.ceramint.2017.04.140 ↗
43. Effects of TaC addition on microstructure and mechanical properties of SiBCN composite ceramics10.1016/j.ceramint.2019.07.231 ↗
44. Oxidation behavior of ZrB2 composites doped with various transition metal silicides10.1016/j.corsci.2014.02.026 ↗
45. Understanding the oxidation behavior of a ZrB2-MoSi2 composite at ultra-high temperatures10.1016/j.actamat.2018.03.042 ↗
46. TaB2-based ceramics: microstructure, mechanical properties and oxidation resistance10.1016/j.jeurceramsoc.2011.07.032 ↗
47. Super-strong materials for temperatures exceeding 2000 °C10.1038/srep40730 ↗