Corrosion mechanism of magnesia-chrome refractory bricks with FetO-SiO2-Cr2O3 copper converter slag

Xing Hou, Donghai Ding, Guoqing Xiao, Endong Jin, Xiaochuan Chong, Jiyuan Luo, Yunqin Gao

Ceramics International· Volume 49· Issue 10
Publisher page

Abstract

No abstract is available for this record. The assistant can identify its topic from the title, but cannot infer the study’s results.

Source: Not provided · Quality: missing

Research context

OpenAlex topics: Metallurgical Processes and Thermodynamics · Magnesium Oxide Properties and Applications · Advanced materials and composites

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (33)

Show source-provided references
1. Schlesinger · 2011
2. Preparation and evaluation of gypsum plaster composited with copper smelter slag10.1016/j.clet.2021.100084 ↗
3. Davenport · 2002
4. Sancho · 2000
5. Review of copper pyrometallurgical practice: today and tomorrow10.1016/j.mineng.2003.08.002 ↗
6. Li · 2012
7. Degradation mechanisms and use of refractory linings in copper production processes: a critical review10.1016/j.jeurceramsoc.2013.10.005 ↗
8. Refractories for the copper and lead industry
9. Corrosion mechanisms of magnesia-chrome refractories in copper slag and concurrent formation of hexavalent chromium10.1016/j.jallcom.2019.01.314 ↗
10. Chemical wear mechanism of magnesia-chromite refractory for an oxygen bottom-blown copper-smelting furnace: a post-mortem analysis10.1016/j.ceramint.2020.09.124 ↗
11. Reactions between magnesia-chrome refractories and copper converter slags: corrosion behavior and prevention by Fe-rich layer formation10.1016/j.ceramint.2022.02.018 ↗
12. Corrosion of magnesia-chrome brick in molten MgO-Al2O3-SiO2-CaO-FetO slag10.1016/j.matchemphys.2008.02.001 ↗
13. et al. Wear phenomean of basic brick linings in the copper industry, TMS (The Minerals, Metals & Materials Society)
14. Petkov · 2007
15. Local corrosion of magnesia–chrome refractories driven by marangoni convection at the slag-metal interface10.1006/jcis.2002.8504 ↗
16. Identification of magnesia–chromite refractory degradation mechanisms of secondary copper smelter linings10.1016/j.jeurceramsoc.2016.02.036 ↗
17. The reaction between the magnesia-chrome brick and the molten slag of MgO-Al2O3-SiO2-CaO-FetO and the resulting microstructure10.1016/j.ceramint.2008.08.008 ↗
18. Corrosion resistance of MgO-C refractory to smelting reduction slag containing titania10.1179/000705902225004392 ↗
19. Dissolution of MgO in stagnant CaO-FeO-SiO2 slags
20. The influence of ZnO in fayalite slag on the degradation of magnesia-chromite refractories during secondary Cu smelting10.1016/j.jeurceramsoc.2015.03.013 ↗
21. Effect of additives and temperature on the dissolution rate and diffusivity of MgO in CaO-Al2O3 slags under forced convection10.2355/isijinternational.46.1554 ↗
22. Corrosion of magnesia-chromite refractory by PbO-rich copper slags10.1016/j.corsci.2021.109949 ↗
23. Dissolution behavior of MgO based refractories in CaO-Al2O3-SiO2 slag10.1179/1743281215Y.0000000003 ↗
24. Degradation mechanisms of magnesia-chromite refractory materials used in oxygen side-blown reducing furnace10.1016/j.ceramint.2020.04.020 ↗
25. The effect of phase formation during use on the chemical corrosion of magnesia–chromite refractories in contact with a non-ferrous PbO-SiO2 based slag10.1016/j.jeurceramsoc.2013.12.026 ↗
26. Utility and problems of chrome-containing refractories
27. Solubility of Cr2O3 and speciation of chromium in soda-lime-silicate melts10.1111/j.1551-2916.2009.03581.x ↗
28. Effects of Cr2O3 content on viscosity and microstructure of copper smelting slag
29. Effects of La2O3 on the viscosity of copper smelting slag and corrosion resistance of magnesia refractory bricks10.1016/j.ceramint.2022.05.170 ↗
30. Effect of fluorspar on the interfacial reaction between electric arc furnace slag and magnesia refractory: competitive corrosion-protection mechanism of magnesiowüstite layer10.1016/j.ceramint.2021.04.047 ↗
31. Effect of Cr2O3 addition on viscosity and structure of Ti-bearing blast furnace slag10.2355/isijinternational.55.1367 ↗
32. Corrosion mechanism of magnesia-chrome and alumina-chrome refractories in E-scrap smelting10.1016/j.ceramint.2021.10.054 ↗
33. Interfacial reaction between magnesia refractory and “FeO”-rich slag: formation of magnesiowüstite layer10.1016/j.ceramint.2019.02.110 ↗