Mechanical properties and strengthening mechanism of SiCf/SiC mini-composites modified by SiC nanowires

Pengfei Wu, Yu Liu, Shenwei Xu, Zeyu Fu, Aimin Pang, Wei Li, Haitang Yang

Ceramics International· Volume 47· Issue 2
Publisher page

Abstract

Abstract The effects of the SiC nanowires (SiCNWs) and PyC interface layers on the mechanical and anti-oxidation properties of SiC fiber (SiCf)/SiC composites were investigated. To achieve this, the PyC layer was coated on the SiCf using a chemical vapour infiltration (CVI) method. Then, SiCNWs were successfully coated on the surface of SiCf/PyC using the electrophoretic deposition method. Finally, a thin PyC layer was coated on the surface of SiCf/PyC/SiCNWs. Three mini-composites, SiCf/PyC/SiC, SiCf/PyC/SiCNWs/SiC, and SiCf/PyC/SiCNWs/PyC/SiC, were fabricated using the typical precursor infiltration and pyrolysis method. The morphologies of the samples were examined using scanning electron microscopy and energy dispersive X-ray spectrometry. Tensile and single-fibre push-out tests were carried out to investigate the mechanical performance and interfacial shear strength of the composites before and after oxidization at 1200 °C. The results revealed that the SiCf/PyC/SiCNWs/SiC composites showed the best mechanical and anti-oxidation performance among all the composites investigated. The strengthening and toughening is mainly achieved by SiCNWs optimization of the interfacial bonding strength of the composite and its own nano-toughening. On the basis of the results, the effects of SiCNWs on the oxidation process and retardation mechanism of the SiCf/SiC mini-composites were investigated.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advanced ceramic materials synthesis · Aluminum Alloys Composites Properties · Diamond and Carbon-based Materials Research

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (41)

Show source-provided references
1. Intermediate temperature strength degradation in SiC/SiC composites10.1016/S0955-2219(02)00144-9 ↗
2. Advanced structural ceramics in aerospace propulsion10.1038/nmat4687 ↗
3. Oxidation resistance of SiC/SiC composites containing SiBC matrix fabricated by liquid silicon infiltration10.1016/j.jeurceramsoc.2017.09.004 ↗
4. Microhardness and microstructure correlations in SiC/SiC composites10.1016/j.matlet.2017.11.093 ↗
5. Experimental study and numerical simulation of dynamic recrystallization for a FGH96 superalloy during isothermal compression10.1016/j.jmrt.2020.03.026 ↗
6. Current status and recent research achievements in SiC/SiC composites10.1016/j.jnucmat.2014.06.003 ↗
7. Advanced ceramic matrix composite materials for current and future propulsion technology applications10.1016/j.actaastro.2004.05.052 ↗
8. The development of cladding materials for the accident tolerant fuel system from the Materials Genome Initiative10.1016/j.scriptamat.2017.07.030 ↗
9. Enhanced mechanical and dielectric properties of SiCf/SiC composites with silicon oxycarbide interphase10.1016/j.ceramint.2017.09.222 ↗
10. Mechanical behavior of SiCf/SiC composites with alternating PyC/SiC multilayer interphases10.1016/j.matdes.2012.07.073 ↗
11. Subcritical crack growth processes in SiC/SiC ceramic matrix composites10.1016/j.jeurceramsoc.2004.12.015 ↗
12. Effects of BN/SiC dual-layer interphase on mechanical and dielectric properties of SiCf/SiC composites10.1016/j.ceramint.2013.09.091 ↗
13. Microstructure and damage evolution of SiCf/PyC/SiC and SiCf/BN/SiC mini-composites: a synchrotron X-ray computed microtomography study10.1016/j.ceramint.2019.03.004 ↗
14. Microstructure and mechanical performance of SiCf/BN/SiC mini-composites oxidized at elevated temperature from ambient temperature to 1500°C in air10.1016/j.jeurceramsoc.2019.04.013 ↗
15. Oxidation resistance of SiCf/SiC composites with a PyC/SiC multilayer interface at 500°C to 1100°C10.1016/j.corsci.2020.108522 ↗
16. Effects of the single layer CVD SiC interphases on the mechanical properties of the SiCf/SiC composites fabricated by PIP process10.1016/j.ceramint.2010.05.014 ↗
17. Effect of pyrolysis temperature on the mechanical evolution of SiCf/SiC composites fabricated by PIP10.1016/j.ceramint.2019.09.087 ↗
18. Effect of frequency and environment on fatigue behavior of a CVI SiC/SiC ceramic matrix composite at 1200°C10.1016/j.compscitech.2010.11.008 ↗
19. BN/SiC coating on SiC tows prepared by chemical vapor infiltration
20. The microstructure and mechanical properties of silicon carbide fibers with boron nitride interphase
21. Ceramic matrix composites containing carbon nanotubes10.1007/s10853-009-3262-9 ↗
22. Fabrication and mechanical properties of multi-walled carbon nanotube reinforced reaction bonded silicon carbide composites
23. Interfacial optimization of SiC nanocomposites reinforced by SiC nanowires with high volume fraction10.1111/jace.16513 ↗
24. Process and mechanical properties of in situ silicon carbide‐nanowire‐reinforced chemical vapor infiltrated silicon carbide/silicon carbide composite10.1111/j.1551-2916.2004.01720.x ↗
25. Fabrication in-situ SiC nanowires/SiC matrix composite by chemical vapour infiltration process10.1016/j.matlet.2004.05.059 ↗
26. Nanobeam mechanics: elasticity, strength, and toughness of nanorods and nanotubes10.1126/science.277.5334.1971 ↗
27. Preparation of in situ grown silicon carbide nanofibers radially onto carbon fibers and their effects on the microstructure and flexural properties of carbon/carbon composites10.1016/j.carbon.2013.03.007 ↗
28. SiC nanowire reinforced carbon/carbon composites with improved interlaminar strength10.1016/j.msea.2015.10.114 ↗
29. Enhancement of the oxidation resistance of C/C composites by depositing SiC nanowires onto carbon fibers by electrophoretic deposition10.1016/j.jallcom.2014.08.209 ↗
30. Fabrication of CNT-SiC/SiC composites by electrophoretic deposition10.1016/j.jeurceramsoc.2009.07.027 ↗
31. In situ synthesis of homogeneously dispersed SiC nanowires in reaction sintered silicon-based ceramic powders10.1016/j.ceramint.2018.01.080 ↗
32. Effect of in-situ grown SiC nanowire and dense SiC on oxidation resistance of carbon fiber/SiC nanowire/SiC matrix composite in high temperature atmospheric environment10.1016/j.corsci.2018.02.034 ↗
33. SiC coating toughened by SiC nanowires to protect C/C composites against oxidation10.1016/j.ceramint.2011.05.159 ↗
34. Mechanical properties of SiCf/SiC composites with alternating PyC/BN multilayer interfaces10.1080/17436753.2017.1339517 ↗
35. Cyclic loading of a SiC-fiber reinforced ceramic matrix composite reveals damage mechanisms and thermal residual stress state10.1016/j.compositesa.2012.06.011 ↗
36. Subcritical crack growth processes in SiC/SiC ceramic matrix composites10.1016/j.jeurceramsoc.2004.12.015 ↗
37. Intermediate temperature strength degradationin SiC/SiC composites10.1016/S0955-2219(02)00144-9 ↗
38. Fatigue of three advanced SiC/SiC ceramic matrix composites at 1200°C in air and in steam10.1111/ijac.12773 ↗
39. Single fiber push-out characterization of interfacial mechanical properties in unidirectional CVI-C/SiC composites by the nano-indentation technique10.1016/j.apsusc.2015.10.018 ↗
40. Influence of surface fibre properties and textural organization of a pyrocarbon interphase on the interfacial shear stress of SiC/SiC minicomposites reinforced with Hi-Nicalon S and Tyranno SA3 fibres10.1016/j.jeurceramsoc.2013.08.027 ↗
41. Statistically sound application of fiber push-out method for the study of locally non-uniform interfacial properties of SiC-SiC fiber composites10.1016/j.jeurceramsoc.2019.11.041 ↗