journal article·2022-10

Damage behavior and removal mechanism of different yarn orientations 2.5D SiCf/SiC composites under single-abrasive scratch test

Zikang Zhang, Songmei Yuan, Weiwei Xu, Xinlu Ouyang, Jiaqi Zhang, Wenzhao An

Ceramics International· Volume 48· Issue 20
Publisher page

Abstract

No abstract is available for this record. The assistant can identify its topic from the title, but cannot infer the study’s results.

Source: Not provided · Quality: missing

Research context

OpenAlex topics: Advanced ceramic materials synthesis · Advanced Surface Polishing Techniques · Advanced machining processes and optimization

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (36)

Show source-provided references
1. A review of third generation SiC fibers and SiCf/SiC composites10.1016/j.jmst.2019.07.020 ↗
2. Effect of fiber directionality on the static and dynamic mechanical properties of 3D SiCf/SiC composites10.1016/j.msea.2016.02.006 ↗
3. Thermal stability of CVI and MI SiC/SiC composites with Hi-NicalonTM-S fibers10.1016/j.jeurceramsoc.2022.03.009 ↗
4. Flexural failure mechanism of 2.5D woven SiCf/SiC composites: combination of acoustic emission, digital image correlation and X-ray tomography10.1016/j.coco.2021.100921 ↗
5. High-temperature oxidation behavior and mechanism of the Si-based thermal protective coating for SiCf/SiC composites under static oxidation and H2O/O2/Na2SO4 corrosion oxidation10.1016/j.compositesb.2022.109906 ↗
6. Rotary ultrasonic machining of ceramic matrix composites: feasibility study and designed experiments10.1016/j.ijmachtools.2005.01.034 ↗
7. A study on grinding surface waviness of woven ceramic matrix composites10.1016/j.apsusc.2013.01.069 ↗
8. Effects of fiber volume fraction on the densification and mechanical properties of unidirectional SiCf/SiC-matrix composites10.1016/j.jeurceramsoc.2020.09.024 ↗
9. Microstructure and mechanical properties of SiC/SiC joints reinforced by in-situ growth SiC nanowires10.1016/j.matchar.2021.111315 ↗
10. Microhardness and microstructure correlations in SiC/SiC composites10.1016/j.matlet.2017.11.093 ↗
11. Hole exit quality and machined surface integrity of 2D Cf/SiC composites drilled by PCD tools10.1016/j.jeurceramsoc.2019.05.057 ↗
12. Mechanical properties evolution of SiCf/SiC composites with a BN/SiC multilayer interface oxidized at elevated temperature10.1016/j.apsusc.2021.151065 ↗
13. Influence factors on grinding force in surface grinding of unidirectional C/SiC composites10.1007/s10443-019-09767-5 ↗
14. A theoretical and experimental investigation on ultrasonic assisted grinding from the single-grain aspect10.1016/j.ijmecsci.2018.09.026 ↗
15. Analytical modelling of side grinding of orthogonal laminated -SiC f-/-SiC composites based on effective elastic properties
16. A study on the surface grinding of 2D C/SiC composites10.1007/s00170-017-0626-1 ↗
17. New observations of the fiber orientations effect on machinability in grinding of C/SiC ceramic matrix composite10.1016/j.ceramint.2018.04.240 ↗
18. Grinding performance of SiC-based ceramics composites by mounted wheel
19. Effect of fiber orientations on surface grinding process of unidirectional C/SiC composites10.1016/j.apsusc.2016.01.142 ↗
20. A scratching force model of diamond abrasive particles in wire sawing of single crystal SiC10.1016/j.mssp.2017.05.032 ↗
21. Material removal behavior in ultrasonic-assisted scratching of SiC ceramics with a single diamond tool10.1016/j.ijmachtools.2014.02.002 ↗
22. Some observations in grinding SiC and silicon carbide ceramic matrix composite material10.1007/s00170-019-03735-w ↗
23. Study on the machined depth when nanoscratching on 6H-SiC using Berkovich indenter: modelling and experimental study10.1016/j.apsusc.2016.02.032 ↗
24. Material removal mode and friction behaviour of RB-SiC ceramics during scratching at elevated temperatures10.1016/j.jeurceramsoc.2019.05.015 ↗
25. Influence of grinding fiber angles on grinding of the 2D–Cf/C–SiC composites10.1016/j.ceramint.2018.04.083 ↗
26. Transformation of fracture mechanism and damage behavior of ceramic-matrix composites during nano-scratching
27. Single diamond scribing of SiCf/SiC composite: force and material removal mechanism study10.1016/j.ceramint.2021.06.195 ↗
28. Effects of grinding speed on the material removal mechanism in single grain grinding of SiCf/SiC ceramic matrix composite10.1016/j.ceramint.2021.01.140 ↗
29. Influence of grit geometry and fibre orientation on the abrasive material removal mechanisms of SiC/SiC Ceramic Matrix Composites (CMCs)10.1016/j.ijmachtools.2020.103580 ↗
30. On understanding the microstructure of SiC/SiC Ceramic Matrix Composites (CMCs) after a material removal process10.1016/j.msea.2018.11.037 ↗
31. A 3D shear-lag model considering micro-damage and statistical strength prediction of unidirectional fiber-reinforced composites10.1016/S0266-3538(01)00079-3 ↗
32. Surface/subsurface damage and the fracture strength of ground ceramics10.1016/0924-0136(95)02090-X ↗
33. Grinding characteristics and removal mechanism of 2.5D-needled Cf/SiC composites10.1016/j.ceramint.2019.07.156 ↗
34. Investigations on grinding process of woven ceramic matrix composite based on reinforced fiber orientations10.1016/j.compositesb.2014.11.029 ↗
35. Understanding the machining characteristic of plain weave ceramic matrix composite in ultrasonic-assisted grinding10.1016/j.ceramint.2021.11.100 ↗
36. Size effect for specific energy in grinding of silicon nitride10.1016/S0043-1648(98)00406-2 ↗