A review of the research progress on the interface between oxide fiber and oxide ceramic matrix
Source abstract
Abstract
Abstract Oxide ceramics have excellent high temperature performance, superior thermal and chemical stability, which can be used in high temperature oxidizing environments, while oxide ceramics generally have low toughness and are prone to catastrophic damage... Oxide ceramics can be reinforced by high performance ceramic fibers to improve the fracture strength and fracture toughness, thus expanding its application in high-temperature components such as aero-engine combustion chambers and tail nozzles. The interface between fiber and matrix is an important factor that determines the performance of the composites. By tailoring the interface, the energy dissipation mechanisms such as fiber debonding and fiber pull-out can be brought into play to avoid the catastrophic damage of the composites. This review paper summarizes the recent research progress of the oxide fiber/oxide ceramic matrix composites interface. The mechanical properties of the interface and the design principles of the interface engineering are discussed, and types of interfaces and coating preparation methods are reviewed.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advanced ceramic materials synthesis · High-Temperature Coating Behaviors · Magnesium Oxide Properties and Applications
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (100+)
Show source-provided references
1. Alumina-mullite ceramics for structural applications10.1016/j.ceramint.2005.04.001 ↗
2. Structure and properties of mullite-A review10.1016/j.jeurceramsoc.2007.03.017 ↗
3. Processing of Cf/SiC composites by hot pressing using polymer binders followed by polymer impregnation and pyrolysis10.1016/j.jeurceramsoc.2019.09.047 ↗
4. Mechanical investigation of weak regions in a wound oxide-oxide ceramic matrix composite10.1016/j.jeurceramsoc.2018.05.009 ↗
5. Effect of a diffusion-enhancing hole on the densification of a thick-section 2D C/SiC composite10.1016/j.jeurceramsoc.2019.07.043 ↗
6. Time-dependent matrix fracture of carbon fiber-reinforced silicon carbide ceramic-matrix composites considering interface oxidation10.1080/09276440.2019.1667194 ↗
7. Computational study of micromechanical damage behavior in continuous fiber-reinforced ceramic composites10.1007/s10853-016-0120-4 ↗
8. Research progress on oxide/oxide ceramic matrix composites
9. Interface engineering in oxide fibre/oxide matrix composites10.1179/095066000101528359 ↗
10. Modeling strength degradation of fiber-reinforced ceramic-matrix composites under cyclic loading at room and elevated temperatures10.1016/j.msea.2017.04.035 ↗
11. Oxidation mechanisms and kinetics of SiC-matrix composites and their constituents10.1023/B:JMSC.0000048745.18938.d5 ↗
12. Influence of fibre content on the strength of carbon fibre reinforced HfC/SiC composites up to 2100 °C10.1016/j.jeurceramsoc.2019.04.049 ↗
13. Investigation of a single-layer EBC deposited on SiC/SiC CMCs: processing and corrosion behaviour in high-temperature steam10.1016/j.jeurceramsoc.2018.12.019 ↗
14. Oxidation and corrosion of ceramics and ceramic matrix composites10.1016/S1359-0286(01)00009-2 ↗
15. Carbon fiber reinforced ultra-high temperature ceramic matrix composites: a review10.1016/j.ceramint.2019.05.065 ↗
16. Alumina-mullite ceramics for structural applications10.1016/j.ceramint.2005.04.001 ↗
17. Structure and properties of mullite - a review10.1016/j.jeurceramsoc.2007.03.017 ↗
18. Synergistic effects of fiber debonding and fracture on matrix cracking in fiber-reinforced ceramic-matrix composites10.1016/j.msea.2016.11.077 ↗
19. Stress analysis of a crack in a fiber-reinforced layered composite10.1016/j.compstruct.2014.07.024 ↗
20. Processing, structure, and properties of mullite fiber/mullite matrix composites10.1016/0955-2219(95)00136-0 ↗
21. Degradation of oxide fibers by thermal overload and environmental effects10.1016/j.msea.2012.05.107 ↗
22. Precipitation coating of monazite on woven ceramic fibers: III-Coating without strength degradation using a phytic acid precursor10.1111/j.1551-2916.2009.03406.x ↗
23. Effects of sintering temperature on mechanical properties of 3D mullite fiber (ALF FB3) reinforced mullite composites10.1016/j.ceramint.2013.05.030 ↗
24. Preceramic paper-derived SiCf/SiCp composites obtained by spark plasma sintering: processing, microstructure and mechanical properties10.3390/ma13030607 ↗
25. Preparation and characterization of an oxide-oxide continuous fiber reinforced ceramic matrix composite with a zinc oxide interphase10.1016/j.ceramint.2017.09.133 ↗
26. Fabrication and properties of fibrous porous mullite-zirconia fiber networks with a quasi-layered structure10.1016/j.jeurceramsoc.2016.06.003 ↗
27. Micromechanical FE analysis of SiCf/SiC composite with BN interface10.1007/s12633-019-00119-3 ↗
28. Interface design for oxidation-resistant ceramic composites10.1111/j.1151-2916.2002.tb00505.x ↗
29. Interface controlled micro- and macro- mechanical properties of aluminosilicate fiber reinforced SiC matrix composites10.1016/j.jeurceramsoc.2016.10.003 ↗
30. Mullite fiber cloth-reinforced mullite composite fabricated via an optimized layer-by-layer assembly method10.1016/j.ceramint.2018.09.167 ↗
31. Research progress in oxide/oxide ceramic matrix composites and processing technologies
32. Fabrication of silicon carbide coating on mullite fiber-reinforced mullite matrix composite via dip-coating10.1016/j.ceramint.2017.09.185 ↗
33. Interface engineering in mullite fiber/mullite matrix composites10.1016/j.jeurceramsoc.2007.03.008 ↗
34. Influence of interfacial roughness on fiber sliding in oxide composites with La-Monazite interphases10.1111/j.1151-2916.2003.tb00016.x ↗
35. Ceramic filament fibers - a review10.1002/mame.201100364 ↗
36. High performance oxide fibers for metal and ceramic composites10.1016/S1359-835X(00)00176-7 ↗
37. Fine diameter ceramic fibres10.1016/S0955-2219(00)00090-X ↗
38. Single crystalline oxide fibres for heat-resistant composites10.1016/j.compscitech.2005.05.029 ↗
39. Mechanical properties of alumina Nextel (TM) 720 fibres at room and elevated temperatures: tensile bundle testing10.1016/S0921-5093(02)00794-3 ↗
40. Kinetics of mullite grain growth in Alumino silicate fibers10.1111/j.1551-2916.2005.00085.x ↗
41. Tension-compression fatigue of a Nextel (TM) 720/alumina composite at 1200 °C in air and in steam10.1007/s10443-016-9481-8 ↗
42. Creep in interlaminar shear of a Nextel (TM) 720/aluminosilicate composite at 1100 °C in air and in steam
43. Cyclic creep and recovery behavior of Nextel (TM) 720/alumina ceramic composite at 1200 degrees C, Mat10.1016/j.msea.2010.10.011 ↗
44. Degradation of oxide fibers by thermal overload and environmental effects10.1016/j.msea.2012.05.107 ↗
45. Microstructure and room temperature mechanical properties of mullite fibers after heat-treatment at elevated temperatures10.1016/j.msea.2013.04.089 ↗
46. Creep and microstructure of Nextel (TM) 720 fiber at elevated temperature in air and in steam10.1016/j.actamat.2013.06.053 ↗
47. Effects of heat treatments in HCl on the fiber bundle strength of a two-phase polycrystalline oxide fiber10.1111/j.1551-2916.2005.00851.x ↗
48. Effect of pyrolysis temperature on the properties of three-dimensional silica fiber reinforced nitride matrix composites10.1007/s11665-007-9146-8 ↗
49. Mechanical properties and microstructure of 3D 6-Directional braided SiO2f/SiO2 composites by Silicasol-Infiltration-Sintering method10.14233/ajchem.2013.12128 ↗
50. Effects of high-temperature annealing on microstructure and mechanical property of SiO2f/SiO2 composites10.1016/j.vacuum.2017.07.005 ↗
51. Preparation of three-dimensional silica fiber reinforced silicon nitride composites using perhydropolysilazane as precursor10.1016/j.matlet.2005.04.057 ↗
52. Effects of oxidation treatment on properties of SiO2f/SiO2-BN composites10.1007/s11771-012-0968-7 ↗
53. Effects of SiC contents on the dielectric properties of SiO2f/SiO2 composites fabricated through a sol-gel process10.1016/j.powtec.2013.02.021 ↗
54. Mechanical behavior of 2.5D (shallow straight-joint) and 3D four-directional braided SiO2f/SiO2 composites10.1016/j.ceramint.2012.01.083 ↗
55. High-Performance glass fiber development for composite applications10.1111/ijag.12053 ↗
56. Glass fibre StrengthA review with relation to composite recycling10.3390/fib4020018 ↗
57. Effects of sintering atmosphere on the densification and microstructure of yttrium aluminum garnet fibers prepared by sol-gel process10.1016/j.jeurceramsoc.2019.08.033 ↗
58. Preparation of polycrystalline YAG/alumina composite fibers and YAG fiber by sol-gel method10.1016/S1359-835X(01)00014-8 ↗
59. Preparation and grain-growth of chromia-yttrium aluminum garnet composites fibers by sol-gel method10.1007/s10971-017-4410-3 ↗
60. The manufacture of partially-stabilised and fully-stabilised zirconia fibres blow spun from an alkoxide derived aqueous sol-gel precursor10.1016/S0955-2219(00)00178-3 ↗
61. The influence of zirconia fibre on ablative composite materials10.1080/14658011.2019.1585099 ↗
62. Development of polycrystalline yttrium aluminum garnet (YAG) fibers10.1016/j.jeurceramsoc.2015.07.011 ↗
63. Preparation, structural and thermo-mechanical properties of lithium aluminum silicate glass-ceramics10.1016/j.ceramint.2008.07.019 ↗
64. Sintering densification, microstructure and transformation behavior of Al2O3/ZrO2(Y2O3) composites10.1016/j.msea.2007.06.058 ↗
65. Toughening mechanism of mullite matrix composites: a review10.3390/coatings10070672 ↗
66. Deformation and fracture behavior of an Al2O3/YAG composite from room temperature to 2023 K10.1016/S0266-3538(01)00159-2 ↗
67. Tension-compression fatigue of an oxide/oxide ceramic composite at elevated temperature10.1016/j.msea.2016.02.057 ↗
68. Effects of steam environment on creep behavior of Nextel (TM) 720/alumina ceramic composite at elevated temperature10.1016/j.msea.2008.06.036 ↗
69. Creep behavior of Nextel (TM) 720/alumina ceramic composite with +/- 45 degrees fiber orientation at 1200 degrees C10.1016/j.compscitech.2007.07.012 ↗
70. Effect of loading rate on the monotonic tensile behavior and tensile strength of an oxide-oxide ceramic composite at 1200 degrees C10.1016/j.msea.2008.03.006 ↗
71. Mechanical and dielectric properties of mullite fiber-reinforced mullite matrix composites with single layer CVD SiC interphases10.1111/ijac.12238 ↗
72. The design of the fibre-matrix interfacial zone in ceramic matrix composites10.1016/S1359-835X(97)00128-0 ↗
73. Conditions for matrix crack deflection at an interface in ceramic matrix composites10.1016/S0921-5093(98)00604-2 ↗
74. Li · 2020
75. Fibre-reinforced multifunctional SiC matrix composite materials10.1080/09506608.2016.1213939 ↗
76. The design of the fibre-matrix interfacial zone in ceramic matrix composites10.1016/S1359-835X(97)00128-0 ↗
77. Crack deflection at an interface between dissimilar elastic materials: role of residual stresses10.1016/0020-7683(94)90025-6 ↗
78. Criteria for crack deflection/penetration criteria for fiber-reinforced ceramic matrix composites10.1016/S0266-3538(98)00043-8 ↗
79. Effects of the single layer CVD SiC interphases on mechanical properties of mullite fiber-reinforced mullite matrix composites fabricated via a sol–gel process10.1016/j.ceramint.2013.09.012 ↗
80. Research progress on micro-mechanical property of continuous fiber-reinforced ceramic matrix composites10.15541/jim20170421 ↗
81. Oxide CMCs: interphase synthesis and novel fibre development10.1016/S0955-2219(99)00263-0 ↗
82. Effectiveness of monazite coatings in oxide/oxide composites after long-term exposure at high temperature10.1111/j.1151-2916.2003.tb00018.x ↗
83. Fatigue and creep behaviors of a SiC/SiC composite under combustion and laboratory environments10.1177/0021998315602323 ↗
84. A time-dependent vibration damping model of fiber-reinforced ceramic-matrix composites at elevated temperature10.1016/j.ceramint.2020.07.180 ↗
85. Damage assessment of oxide fibre reinforced oxide ceramic matrix composites using acoustic emission10.1016/j.ceramint.2005.11.016 ↗
86. Fracture behavior of monazite-coated alumina fiber-reinforced alumina-matrix composites at elevated temperature10.2109/jcersj.112.628 ↗
87. Damage assessment of alumina fibre-reinforced mullite ceramic matrix composites subjected to cyclic fatigue at ambient and elevated temperatures10.1016/S0955-2219(01)00320-X ↗
88. Effect of boron doping on waterproof and dielectric properties of polyborosiloxane coating on SiO2f/SiO2 composites10.1016/j.cja.2018.11.008 ↗
89. Processing and properties of unidirectional SiO2f/SiO2 composites10.1016/j.ceramint.2005.12.017 ↗
90. Effects of oxidation treatment on properties of SiO2f/SiO2-BN composites10.1007/s11771-012-0968-7 ↗
91. Alkyl ethoxylate assisted liquid phase exfoliation of BN nanosheet and its application as interphase for oxide/oxide composites10.1016/j.ceramint.2018.08.207 ↗
92. Effect of BNNTs/matrix interface tailoring on toughness and fracture morphology of hierarchical SiCf/SiC composites10.1007/s40145-019-0338-0 ↗
93. Evaluation of SiC/SiC minicomposites with yttrium disilicate fiber coating10.1111/jace.15170 ↗
94. Failure analysis of unidirectional ceramic matrix composite lamina and Cross-Ply laminate under fiber direction uniaxial tensile load: cohesive zone modeling and brittle fracture mechanics approach10.1007/s11665-020-04724-x ↗
95. Effect of interface properties on tensile and fatigue behavior of 2D woven SiC/SiC fiber-reinforced ceramic-matrix composites
96. Shape memory alloys for use in thermally activated clothing, protection against flame and heat10.1002/(SICI)1099-1018(199909/10)23:5<223::AID-FAM687>3.0.CO;2-K ↗
97. Developments in oxide fiber composites10.1111/j.1551-2916.2006.01342.x ↗
98. Fabrication and oxidation resistance of mullite/yttrium silicate multilayer coatings on C/SiC composites10.1007/s40145-017-0248-y ↗
99. The design of the fibre-matrix interfacial zone in ceramic matrix composites10.1016/S1359-835X(97)00128-0 ↗
100. Mechanical properties of 3D KD-I SiCf/SiC composites with engineered fibre-matrix interfaces10.1016/j.compscitech.2011.01.014 ↗