journal article·2021-02

Investigating the grinding performance of unidirectional and 2.5D-C/SiCs

Yuying Yang, Shuoshuo Qu, Yadong Gong

Ceramics International· Volume 47· Issue 4
Publisher page

Abstract

Abstract The grinding performances of unidirectional and 2.5D-C/SiCs were discussed in this paper. In particular, the effects of the grinding depth and fibre architecture on the grinding force, surface quality and grinding debris and the material removal mechanisms of C/SiCs were the main focuses of this investigation; these issues have not received much attention in previous studies. Therefore, this study attempted to analyze the grinding mechanism of C/SiCs and improve the corresponding grinding quality on the basis of discussing the grinding properties of C/SiCs with different fibre architectures. The grinding depth had a substantial influence on the grinding properties of the C/SiCs. Compared to the unidirectional C/SiCs, the 2.5D-C/SiCs sustained a higher grinding force under the same grinding parameters. Fibre pullout and fibre outcrop were the fundamental damage modes of the unidirectional C/SiCs. In contrast, interfacial debonding, matrix cracking, fibre pullout and fibre outcrop were the primary defect forms of the 2.5D-C/SiCs. The subsurface damage in the 2.5D-C/SiCs was shallower and wider than that in the unidirectional C/SiCs. In addition, there was a substantial difference between the debris from the unidirectional and 2.5D-C/SiCs. The grinding force, surface quality and grinding debris of C/SiCs with different fibre architectures can be predicted with the principles outlined in this study. Hence, this research can provide a reference for increasing the grinding performance of C/SiCs with different fibre architectures.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advanced Surface Polishing Techniques · Advanced ceramic materials synthesis · Advanced materials and composites

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (39)

Show source-provided references
1. Microstructure of friction surface developed on carbon fiber reinforced carbon-silicon carbide (Cf/C-SiC)10.1016/j.jeurceramsoc.2012.03.039 ↗
2. An investigation of carbon nanofluid minimum quantity lubrication for grinding unidirectional carbon fibre-reinforced ceramic matrix composites10.1016/j.jclepro.2019.119353 ↗
3. Si/SiC coated Cf/SiC composites via tape casting and reaction bonding: the effect of carbon content10.1016/j.ceramint.2016.07.048 ↗
4. Modeling the effects of reactor wall reaction on isothermal CVI process of C/SiC composites10.1016/j.commatsci.2006.05.005 ↗
5. Mechanical behavior of SiCf/SiC composites with alternating PyC/SiC multilayer interphases10.1016/j.matdes.2012.07.073 ↗
6. Effect of fiber orientations on surface grinding process of unidirectional C/SiC composites10.1016/j.apsusc.2016.01.142 ↗
7. Surface topography and roughness of silicon carbide ceramic matrix composites10.1016/j.ceramint.2018.05.104 ↗
8. Study on surface/subsurface breakage in ultrasonic assisted grinding of C/SiC composites10.1007/s00170-017-0012-z ↗
9. A study on grinding surface waviness of woven ceramic matrix composites10.1016/j.apsusc.2013.01.069 ↗
10. Criteria and properties of the asperity peaks on 3D engineering surfaces10.1016/j.wear.2013.09.010 ↗
11. Analysis of grinding mechanics and improved predictive force model based on material-removal and plastic-stacking mechanisms10.1016/j.ijmachtools.2017.06.002 ↗
12. Single fiber push-out characterization of interfacial mechanical properties in unidirectional CVI-C/SiC composites by the nano-indentation technique10.1016/j.apsusc.2015.10.018 ↗
13. Influence of grinding fiber angles on grinding of the 2D-C-f/C-SiC composites10.1016/j.ceramint.2018.04.083 ↗
14. New observations of the fiber orientations effect on machinability in grinding of C/SiC ceramic matrix composite10.1016/j.ceramint.2018.04.240 ↗
15. Enhancing the fracture resistance of carbon fiber reinforced SiC matrix composites by interface modification through a simple fiber heat-treatment process10.1016/j.carbon.2016.08.047 ↗
16. Experimental investigations on grinding characteristics and removal mechanisms of 2D–Cf/C-SiC composites based on reinforced fiber orientations10.1016/j.ceramint.2017.08.064 ↗
17. Study of material removal mechanisms in grinding of C/SiC composites via single-abrasive scratch tests10.1016/j.ceramint.2018.11.165 ↗
18. A force model in single grain grinding of long fiber reinforced woven composite10.1007/s00170-018-2719-x ↗
19. Study on minimum quantity lubrication (MQL) in grinding of carbon fiber-reinforced SiC matrix composites (CMCs)10.1007/s00170-017-1464-x ↗
20. Development of a novel ultrasonic unit for grinding of ceramic matrix composites10.1007/s00170-011-3347-x ↗
21. Intermittent grinding of ceramic matrix composites (CMCs) utilizing a developed segmented wheel10.1016/j.ijmachtools.2010.11.002 ↗
22. Fracture behaviors and mechanism of 2D C/SiC-BCx composite under tensile load10.1016/j.msea.2011.09.089 ↗
23. Experimental studies on drilling tool load and machining quality of C/SiC composites in rotary ultrasonic machining10.1016/j.jmatprotec.2014.06.015 ↗
24. Some observations in grinding SiC and silicon carbide ceramic matrix composite material10.1007/s00170-019-03735-w ↗
25. Damage behaviors of unidirectional CFRP in orthogonal cutting: A comparison between single- and multiple-pass strategies10.1016/j.compositesb.2020.107774 ↗
26. Effect of friction coefficient on chip thickness models in ductile-regime grinding of zirconia ceramics10.1007/s00170-019-03367-0 ↗
27. Experimental evaluation of the lubrication performance of mixtures of castor oil with other vegetable oils in MQL grinding of nickel-based alloy10.1016/j.jclepro.2016.10.073 ↗
28. Detailed modeling of cutting forces in grinding process considering variable stages of grain-workpiece micro interactions10.1016/j.ijmecsci.2016.11.016 ↗
29. Empirical modelling of grinding force based on multivariate analysis10.1016/j.jmatprotec.2007.10.058 ↗
30. Effect of friction coefficient on chip thickness models in ductile-regime grinding of zirconia ceramics10.1007/s00170-019-03367-0 ↗
31. Review of ultrasonic vibration-assisted machining in advanced materials10.1016/j.ijmachtools.2020.103594 ↗
32. A study on the surface grinding of 2D C/SiC composites10.1007/s00170-017-0626-1 ↗
33. Investigating minimum quantity lubrication in unidirectional C-f/SiC composite grinding10.1016/j.ceramint.2019.10.076 ↗
34. Predictive modeling of undeformed chip thickness in ceramic grinding10.1016/j.ijmachtools.2012.01.003 ↗
35. Maximum undeformed equivalent chip thickness for ductile-brittle transition of zirconia ceramics under different lubrication conditions10.1016/j.ijmachtools.2017.06.003 ↗
36. Predictive model for minimum chip thickness and size effect in single diamond grain grinding of zirconia ceramics under different lubricating conditions10.1016/j.ceramint.2019.04.226 ↗
37. Mechanical model and removal mechanism of unidirectional carbon fibre-reinforced ceramic composites10.1016/j.ijmecsci.2020.105465 ↗
38. Surface morphology evaluation of multi-angle 2D ultrasonic vibration integrated with nanofluid minimum quantity lubrication grinding10.1016/j.jmapro.2020.01.024 ↗
39. An experimental and numerical study of micro-grinding force and performance of sapphire using novel tructured micro abrasive tool10.1016/j.ijmecsci.2020.105741 ↗