High-volume natural volcanic pozzolan and limestone powder as partial replacements for portland cement in self-compacting and sustainable concrete
Source abstract
Abstract
A laboratory study demonstrates that high volume, 45% by mass replacement of portland cement (OPC) with 30% finely-ground basaltic ash from Saudi Arabia (NP) and 15% limestone powder (LS) produces concrete with good workability, high 28-day compressive strength (39 MPa), excellent one year strength (57 MPa), and very high resistance to chloride penetration. Conventional OPC is produced by intergrinding 95% portland clinker and 5% gypsum, and its clinker factor (CF) thus equals 0.95. With 30% NP and 15% LS portland clinker replacement, the CF of the blended ternary PC equals 0.52 so that 48% CO2 emissions could be avoided, while enhancing strength development and durability in the resulting self-compacting concrete (SCC). Petrographic and scanning electron microscopy (SEM) investigations of the crushed NP and finely-ground NP in the concretes provide new insights into the heterogeneous fine-scale cementitious hydration products associated with basaltic ash-portland cement reactions.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Concrete and Cement Materials Research · Innovative concrete reinforcement materials · Concrete Properties and Behavior
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (67)
Show source-provided references
1. The cement sustainability initiative: recycling concrete
2. U.S. Department of the Interior USGS. Mineral commodity summaries 2011. Reston, Virginia: U.S. Geological Survey; 2011.
3. Mehta · 2006
4. Reducing the environmental impact of concrete
5. IEA-WBCSD, Cement Technology Roadmap 2009 – Carbon emissions reductions up to 2050; 2009.
6. WBCSD-CSI, Cement Industry Energy and CO2 Performance “Getting the Numbers Right”. Washington, DC; 2009.
7. Tomkins · 2009
8. Malhotra · 2008
9. Sustainable cements and concrete for the climate change era – a review
10. Properties of natural pozzolan and its potential utilization in environmental friendly concrete10.1139/L10-112 ↗
11. High-volume natural pozzolan concrete for structural applications
12. Study of the hydration process of quaternary blended cements and durability of the produced mortars and concretes10.1016/j.conbuildmat.2008.11.015 ↗
13. Synergy between fly ash and limestone powder in ternary cements10.1016/j.cemconcomp.2010.09.006 ↗
14. Roobol · 2002
15. Broad accommodation of rift-related extension recorded by dyke intrusion in Saudi Arabia10.1038/ngeo966 ↗
16. Assessment of the industrial utilization of scoria materials in central Harrat Rahat, Saudi Arabia10.1016/S0013-7952(00)00024-7 ↗
17. State-of-the-art report on use of limestone in cements at levels of up to 15%
18. The role of calcium carbonate in cement hydration10.1016/j.cemconres.2006.10.013 ↗
19. Cement hydration in the presence of high filler contents10.1016/j.cemconres.2005.03.008 ↗
20. Limestone fillers conserve cement Part 2: Durability issues and the effects of limestone fineness on mixtures
21. Hooton · 2007
22. Carboaluminate phases formation during the hydration of calcite-containing portland cement10.1111/j.1551-2916.2010.04201.x ↗
23. Hawkins · 2003
24. Hydration products of C3A, C3S and Portland cement in the presence of CaCO310.1016/S0008-8846(00)00292-1 ↗
25. Influence of finely ground limestone on cement hydration10.1016/S0958-9465(98)00020-1 ↗
26. Limestone filler cement in low w/c concrete: a rational use of energy10.1016/S0008-8846(02)01087-6 ↗
27. Influence of limestone on the hydration of Portland cements10.1016/j.cemconres.2008.01.002 ↗
28. Effect of a high calcite filler addition upon microstructural, mechanical, shrinkage and transport properties of a mortar10.1016/j.cemconres.2008.02.007 ↗
29. Evaluation of Portland limestone cements for use in concrete construction10.1617/s11527-006-9143-7 ↗
30. Pozzolana and pozzolanic cements
31. Effects of the secondary minerals of the natural pozzolans on their pozzolanic activity10.1016/j.cemconres.2008.02.005 ↗
32. Supplementary cementitious materials10.2138/rmg.2012.74.6 ↗
33. Mid-Pleistocene pozzolanic volcanic ash in ancient Roman concretes10.1002/gea.20295 ↗
34. Evaluation of engineering properties of scoria in central Harrat Rahat, Saudi Arabia10.1007/s100640000061 ↗
35. Wenk · 2009
36. Palagonite – a review10.1007/s00531-001-0238-7 ↗
37. Effects of volcanic eruptions on the CO2 content of the atmosphere and the oceans: the 1996 eruption and flood within the Vatnajökull Glacier, Iceland10.1016/S0009-2541(02)00116-X ↗
38. The role of apatite in mantle enrichment processes and in the petrogenesis of some alkali basalt suites10.1016/0016-7037(82)90273-3 ↗
39. ASTM · 2007
40. ASTM · 2009
41. ASTM · 2010
42. Specimen and aggregate size effect on concrete compressive strength
43. Specimen shape and size effect on the compressive strength of higher strength concrete10.1016/S0008-8846(97)00104-X ↗
44. NORDTEST · 1999
45. ASTM. C948-81 Standard test method for dry and wet bulk density, water absorption, and apparent porosity of thin sections of glass-fiber reinforced concrete. 2009. p. 1–2.
46. RILEM TC 116-PCD:Permeability of Concrete as a Criterion of its Durability_Test for Gas Permeability of Concrete.pdf>
47. The determination of the permeability of concrete to oxygen by the Cembureau method – a recommendation10.1007/BF02472192 ↗
48. Performance-based specifications of self-consolidating concrete used in structural applications
49. Strength development of ternary blended cement with limestone filler and blast-furnace slag10.1016/S0958-9465(01)00056-7 ↗
50. Gjørv · 2009
51. Corrosion resistance and chloride diffusivity of volcanic ash blended cement mortar10.1016/j.cemconres.2003.10.021 ↗
52. The permeability of Portland limestone cement concrete10.1016/S0008-8846(03)00092-9 ↗
53. Determination of chloride diffusion coefficient and gas permeability of concrete and their relationship10.1016/S0008-8846(96)85015-0 ↗
54. The effect of mineral admixtures on the properties of high-performance concrete10.1016/S0958-9465(00)00031-7 ↗
55. The importance of gas permeability in addition to the compressive strength of concrete10.1680/macr.2000.52.1.1 ↗
56. Gas permeability of concrete in relation to its degree of saturation10.1007/BF02480405 ↗
57. Effect of stress on gas permeability in concrete
58. Compressive strength and shrinkage of mortar containing various amounts of mineral additions10.1016/j.conbuildmat.2011.03.055 ↗
59. High-volume fly ash concrete with high strength and low drying shrinkage10.1061/(ASCE)0899-1561(2003)15:2(153) ↗
60. Effect of phosphorus and fluorine on hydration process of tricalcium silicate and tricalcium aluminate10.1007/s11595-012-0462-y ↗
61. Taylor · 2004
62. Alkali sorption by C–S–H and C–A–S–H gels: Part II. Role of alumina10.1016/S0008-8846(02)00753-6 ↗
63. Assessment of material characteristics of ancient concretes, Grande Aula, Markets of Trajan, Rome10.1016/j.jas.2009.07.011 ↗
64. Cement microstructures and durability in ancient Roman seawater concretes
65. The judicious selection and preservation of tuff and travertine building stone in ancient Rome10.1111/j.1475-4754.2005.00215.x ↗
66. Limestone fillers to conserve cement in low w/cm concretes: An analysis based on Powers' model
67. Mechanical properties and durability of mortar and concrete containing natural pozzolana and limestone blended cements10.1016/j.cemconcomp.2007.04.009 ↗