Effect of Plastic Deformation on the Crystal Structure and Crystallization Activation Energy of Ni-W-P Alloy Coating
Source abstract
Abstract
Jet electrodeposition method was used to prepare Ni-W-P amorphous alloy coating and effects of plastic deformation on the crystal structure and crystallization kinetics were investigated. Based on the results of differential scanning calorimeter, x-ray diffractometer and transmission electron microscope, it can be seen that when the plastic deformation is up to 20%, the Ni-W-P amorphous alloy coating begins to crystallize. An increase of plastic deformation will lead to a decrease of crystallization temperature as well as a decrease of crystallization activation energy calculated by Kissinger equation. The effective activation energy is reduced from 268.63 kJ/mol in the as-deposited state to 246.63 kJ/mol in the cold deformation up to 40%. Analyses were presented to discuss the possible mechanism for the effect of plastic deformation on the crystallization kinetics of the Ni-W-P amorphous alloy coatings.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Electrodeposition and Electroless Coatings · Advanced materials and composites · Metallic Glasses and Amorphous Alloys
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (23)
Show source-provided references
1. R.Z. Valiev and T.G. Langdon, Principle of ECAP as a Processing Tool for Grain Refinement, Prog. Mater. Sci., 2006, 51, p 881–98110.1016/j.pmatsci.2006.02.003 ↗
2. Andrey. Belyakov, Kaneaki. Tsuzaki, and Yuuji. Kimura, Regularities of Deformation Microstructures in Ferrite Stainless Steel During Large Strain Cold Working, ISIJ Int., 2008, 48(8), p 1071–107910.2355/isijinternational.48.1071 ↗
3. T.F. Jing, Y.W. Gao, G.Y. Qiao, Q. Li, T.S. Wang, W. Wang, F.R. Xiao, D.Y. Cai, X.Y. Song, and X. Zhao, Nanocrystalline Processed by Severe Rolling Of Martensite, Mater. Sci. Eng. A, 2006, 432, p 216–32010.1016/j.msea.2006.06.047 ↗
4. M. Eskandari, A. Najafizadeh, and A. Kermanpur, Effect of Strain-Induced Martensite on the Formation of Nanocrystalline 316L Stainless Steel After Cold Rolling and Annealing, Mater. Sci. Eng. A, 2009, 519, p 46–5010.1016/j.msea.2009.04.038 ↗
5. Q. Li, T.F. Jing, Y.W. Gao, and H.B. Li, Investigation on the Preparation of the Ultrafine Grained Low-Carbon Steel by Warm Deformation, Phase Transit., 2012, 85(7), p 619–62910.1080/01411594.2011.651796 ↗
6. Y. Yoshizawa, S. Oguma, and K. Yamauchi, New Fe-Based Soft Magnetic Alloys Composed Of Ultrafine Grain Structure, J. Appl. Phys., 1988, 64(10), p 6044–604610.1063/1.342149 ↗
7. S. Zhang, F.H. Cao, L.R. Chang, J.J. Zheng, Z. Zhang, J.Q. Zhang, and C.N. Cao, Electrodeposition of High Corrosion Resistance Cu/Ni-P Coating on AZ91D Magnesium Alloy, Appl. Surf. Sci., 2011, 257(21), p 9213–922010.1016/j.apsusc.2011.06.006 ↗
8. A.P. Ordine, S.L. Diaz, I.C.P. Margarit, O.E. Barcia, and O.R. Mattos, Electrochemical Study on Ni-P Electrodeposition, Electrochim. Acta, 2006, 51(8-9), p 1480–148610.1016/j.electacta.2005.02.129 ↗
9. J.J. Liu, F. Wang, J.Y. Zhai, and J.J. Ji, Controllable Growth and Magnetic Characterization of Electrodeposited Nanocrystalline Ni-P Alloy Nanotube and Nanowire Arrays Inside AAO Template, J. Electroanal. Chem., 2010, 642, p 103–10810.1016/j.jelechem.2010.02.017 ↗
10. H. Yao, G.L. Zhu, and M. Du, The Research on Coating of Electroless Ni-W-P Ternary Alloys, Adv. Mater. Res., 2011, 189-193, p 373–37610.4028/www.scientific.net/AMR.189-193.373 ↗
11. J.K. Yu, T.F. Jing, J. Yang, and Q. Li, Determination of Activation Energy for Crystallizations in Ni-Sn-P Amorphous Alloys, J. Mater. Process. Technol., 2009, 209, p 14–1710.1016/j.jmatprotec.2008.01.021 ↗
12. M. Palaniapapa and S.K. Seshadri, Friction and Wear Behavior of Electroless Ni-P and Ni-W-P Alloy Coatings, Wear, 2008, 265, p 735–74010.1016/j.wear.2008.01.002 ↗
13. F.J. He, Y.Z. Fang, and S.J. Jin, The Study of Corrosion-Wear Mechanism of Ni-W-P Alloy, Wear, 2014, 311, p 14–2010.1016/j.wear.2013.12.024 ↗
14. H. Liu, H.L. Yao, F. Viejo, G. Harrison, G.E. Thompson, and Z. Liu, Laser Nanocrystallisation and Corrosion Behavior of Electroless Ni-W-P Coating, Trans. IMF, 2014, 93(4), p 212–21710.1179/0020296714Z.000000000171 ↗
15. H. Liu, R.X. Guo, and Z. Liu, Effect of Laser Nanocrystallisation on the Wear Behaviour of Electroless Ni-W-P Coatings, Surf. Coat. Technol., 2013, 219, p 31–4110.1016/j.surfcoat.2012.12.048 ↗
16. S. Xie and E.P. George, Hardness and Shear Band Evolution in Bulk Metallic Glasses After Plastic Deformation and Annealing, Acta Mater., 2008, 56(18), p 5202–521310.1016/j.actamat.2008.07.009 ↗
17. V.D. Papachristos, C.N. Panagopoulos, U. Wahlstrom, L.W. Christoffersen, and P. Leisner, Effect of Annealing on the Structure and Hardness of Ni-P-W Multilayered Alloy Coating Produced by Pulse Plating, Mater. Sci. Eng. A, 2000, 279, p 217–23010.1016/S0921-5093(99)00583-3 ↗
18. J.N. Balaraju, N.T. Manikandanath, and V.K. Willianm Grips, Phase Transformation Behavior of Nanocrystalline Ni-W-P Alloys Containing Various W and P Contents, Surf. Coat. Technol., 2012, 206, p 2682–268910.1016/j.surfcoat.2011.11.024 ↗
19. F.B. Wu, S.K. Tien, W.Y. Chen, and J.G. Duh, Microstructure Evaluation and Strengthening Mechanism of Ni-P-W Alloy Coatings, Surf. Coat. Technol., 2004, 177-178, p 312–31610.1016/j.surfcoat.2003.09.010 ↗
20. H. Liu, R.X. Guo, Y. Zong, B.Q. He, and Z. Liu, Comparative Study of Microstructure and Corrosion Resistance of Electroless Ni-W-P Coatings Treated by Laser and Furnace-Annealing, Trans. Nonferrous Met. Soc. China, 2010, 20, p 1024–103110.1016/S1003-6326(09)60252-1 ↗
21. S.K. Tien, J.G. Duh, and Y.I. Chen, Structure, Thermal Stability and Mechanical Properties of Electroless Ni-P-W Alloy Coating During Cycle Test, Surf. Coat. Technol., 2004, 177-178, p 532–53610.1016/j.surfcoat.2003.08.032 ↗
22. M. Palaniapapa and S.K. Seshadri, Structure and Phase Transformation Behavior of Electroless Ni-P and Ni-W-P Deposits, Mater. Sci. Eng. A, 2007, 460-461, p 638–64410.1016/j.msea.2007.01.134 ↗
23. W.Y. Chen and J.G. Duh, Thermal Stability of Sputtered Ni-P and Ni-P-Cr Coatings During Cycling Test and Annealing Treatment, Surf. Coat. Technol., 2004, 177-178, p 222–22610.1016/j.surfcoat.2003.09.036 ↗