journal article·2021-07Open access

A high-voltage, low-temperature molten sodium battery enabled by metal halide catholyte chemistry

Martha M. Gross, Stephen J. Percival, Rose Y. Lee, Amanda S. Peretti, Erik D. Spoerke, Leo J. Small

Cell Reports Physical Science· Volume 2· Issue 7

Abstract

Despite its promise as a safe, reliable system for grid-scale electrical energy storage, traditional molten sodium (Na) battery deployment remains limited by cost-inflating high-temperature operation. Here, we describe a high-performance sodium iodide-gallium chloride (NaI-GaCl3) molten salt catholyte that enables a dramatic reduction in molten Na battery operating temperature from near 300°C to 110°C. We demonstrate stable, high-performance electrochemical cycling in a high-voltage (3.65 V) Na-NaI battery for >8 months at 110°C. Supporting this demonstration, characterization of the catholyte physical and electrochemical properties identifies critical composition, voltage, and state of charge boundaries associated with this enabling inorganic molten salt electrolyte. Symmetric and full cell testing show that the catholyte salt can support practical current densities in a low-temperature system. Collectively, these studies describe the critical catholyte properties that may lead to the realization of a new class of low-temperature molten Na batteries.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Advanced Battery Materials and Technologies · Thermal Expansion and Ionic Conductivity · Advancements in Battery Materials

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (51)

Show source-provided references
1. Energy storage technologies and real life applications – a state of the art review10.1016/j.apenergy.2016.06.097 ↗
2. High-abundance and low-cost metal-based cathode materials for sodium-ion batteries: problems, progress, and key technologies10.1002/aenm.201803609 ↗
3. Challenges and perspectives on high and intermediate-temperature sodium batteries
4. Towards greener and more sustainable batteries for electrical energy storage10.1038/nchem.2085 ↗
5. High and intermediate temperature sodium–sulfur batteries for energy storage: development, challenges and perspectives10.1039/C8RA08658C ↗
6. 2020
7. Analyzing system safety in lithium-ion grid energy storage10.1016/j.jpowsour.2015.09.068 ↗
8. On the need for reliability and safety studies of grid-scale aqueous batteries10.1149/1945-7111/ab9406 ↗
9. Development of intermediate temperature sodium nickel chloride rechargeable batteries using conventional polymer sealing technologies10.1016/j.jpowsour.2017.02.059 ↗
10. An intermediate temperature garnet-type solid electrolyte-based molten lithium battery for grid energy storage10.1038/s41560-018-0198-9 ↗
11. Spatocco · 2015
12. Application of a Simplified Thermal-Electric Model of a Sodium-Nickel Chloride Battery Energy Storage System to a Real Case Residential Prosumer10.3390/en10101497 ↗
13. Development of sodium-sulfur batteries10.1111/j.1744-7402.2004.tb00179.x ↗
14. Advanced Na-NiCl2 battery using nickel-coated graphite with core–shell microarchitecture10.1021/acsami.7b00271 ↗
15. Decorating β″-alumina solid-state electrolytes with micron Pb spherical particles for improving Na wettability at lower temperatures10.1039/C8TA06745G ↗
16. “Ni-Less” cathodes for high energy density, intermediate temperature Na–NiCl2 batteries10.1002/admi.201701592 ↗
17. Bismuth islands for low-temperature sodium-beta alumina batteries10.1021/acsami.8b13954 ↗
18. An advanced Na-NiCl2 battery using bi-layer (dense/micro-porous) β″-alumina solid-state electrolytes10.1016/j.jpowsour.2018.06.039 ↗
19. Low temperature performance of sodium–nickel chloride batteries with NaSICON solid electrolyte10.1016/j.jelechem.2015.11.022 ↗
20. Novel ternary molten salt electrolytes for intermediate-temperature sodium/nickel chloride batteries10.1016/j.jpowsour.2012.07.089 ↗
21. Advanced intermediate temperature sodium-nickel chloride batteries with ultra-high energy density10.1038/ncomms10683 ↗
22. An advanced Na–FeCl2 ZEBRA battery for stationary energy storage application10.1002/aenm.201500357 ↗
23. Ni-less cathode with 3D free-standing conductive network for planar Na-NiCl2 batteries10.1016/j.cej.2020.124059 ↗
24. An intermediate-temperature high-performance Na–ZnCl2 battery10.1021/acsomega.8b02112 ↗
25. The effects of temperature on the electrochemical performance of sodium–nickel chloride batteries10.1016/j.jpowsour.2012.05.020 ↗
26. Liquid-metal electrode to enable ultra-low temperature sodium-beta alumina batteries for renewable energy storage10.1038/ncomms5578 ↗
27. A low-cost durable Na-FeCl2 battery with ultrahigh rate capability10.1002/aenm.201903472 ↗
28. Elucidating the role of anionic chemistry towards high-rate intermediate-temperature Na-metal halide batteries10.1016/j.ensm.2019.08.021 ↗
29. Tin-based ionic chaperone phases to improve low temperature molten sodium-NaSICON interfaces10.1039/D0TA03571H ↗
30. Low temperature molten sodium batteries10.1021/acsaem.0c02385 ↗
31. A high capacity, room temperature, hybrid flow battery consisting of liquid Na-Cs anode and aqueous NaI catholyte10.3390/batteries4040060 ↗
32. Room temperature, hybrid sodium-based flow batteries with multi-electron transfer redox reactions10.1038/srep11215 ↗
33. Ionic liquid redox catholyte for high energy efficiency, low-cost energy storage10.1002/aenm.201500271 ↗
34. Advanced intermediate temperature sodium copper chloride battery10.1016/j.jpowsour.2014.09.014 ↗
35. Next generation molten NaI batteries for grid scale energy storage10.1016/j.jpowsour.2017.06.038 ↗
36. Unlocking the capacity of iodide for high-energy-density zinc/polyiodide and lithium/polyiodide redox flow batteries10.1039/C6EE03554J ↗
37. Electrochemistry of the NaI-AlCl3 molten salt system for use as catholyte in sodium metal batteries10.1149/2.1191814jes ↗
38. GaCl3 in organic synthesis10.1002/ejoc.200500512 ↗
39. Electrochemistry of gallium in the Lewis acidic aluminum chloride-1-methyl-3-ethylimidazolium chloride room-temperature molten salt10.1149/1.1392469 ↗
40. Electrochemistry of gallium10.33961/JECST.2013.4.1.1 ↗
41. 2005
42. The Conductance and Ionization of Potassium Tri-iodide, and the Equilibrium Between Iodine, Iodide, and Polyiodides in Aqueous Solution10.1021/ja01926a004 ↗
43. Conductivity Analysis of Polyiodide Solutions10.1080/00945718808060545 ↗
44. An aqueous ZnCl2/Fe(bpy)3Cl2 flow battery with mild electrolyte10.1007/s11706-020-0523-7 ↗
45. High-capacity micrometer-sized Li2S particles as cathode materials for advanced rechargeable lithium-ion batteries10.1021/ja3052206 ↗
46. Experimental evaluation of the performance of the sodium metal chloride battery below usual operating temperatures10.1016/j.jpowsour.2013.11.046 ↗
47. Cell degradation of a Na–NiCl2 (ZEBRA) battery10.1039/c3ta13644b ↗
48. Advanced intermediate-temperature Na–S battery10.1039/C2EE23606K ↗
49. A novel low-cost sodium–zinc chloride battery10.1039/c3ee24244g ↗
50. An electrochemical study on the cathode of the intermediate temperature tubular sodium-sulfur (NaS) battery10.1149/2.0491902jes ↗
51. Sodium–sulfur flow battery for low-cost electrical storage10.1002/aenm.201701991 ↗