Abstract

Microbially induced corrosion (MIC) has been recognized as a major cause of performance degradation and service life reduction of concrete sewer system. However, the mechanisms for early-stage corrosion and bacterial attachment are not fully understood yet. Aiming at the correlation between surface acidification and the following MIC process, this study investigated the early-stage corrosion of alkali-activated slag (AAS) pastes under organic acid attack (acetic and propionic acids at pH 6 and 4) considering the effect of precursor, alkali content and modulus of activator. The changes in mechanical property, appearance, and microstructure of AAS were analyzed through three-point bending strength test, visual observation, solution and surface pH monitoring, combined with microscale characterizations. The results demonstrate that two organic acids effectively regulate the surface pH of AAS to a range conducive for bacterial attachment. Specifically, pH 4 solutions reduced the surface pH to 4~5 within 35 d, which triggered severe decalcification, hydration product decomposition and pore structure coarsening, leading to a mechanical strength loss of over 64%. In contrast, pH 6 solutions decreased the surface pH to 8~9, but it had a slight impact on the appearance, strength, and microstructure of AAS. At the same pH value, acetic acid solution exhibited slightly stronger corrosivity than that of propionic acid. The findings provide insights into the corrosion process before bacterial attachment and the precondition of MIC on AAS, which facilitates more precisely conducting accelerated simulation tests for large-scale MIC.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Microbial Applications in Construction Materials · Corrosion Behavior and Inhibition · Metal Extraction and Bioleaching

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (49)

Show source-provided references
1. Investigating sewer parameters leading to manhole corrosion: A case study from the city of Arlington, Texas[J]10.1061/JOEEDU.EEENG-7395 ↗
2. Microbially influenced corrosion—Any progress?[J]10.1016/j.corsci.2020.108641 ↗
3. Koch · 2002
4. Biogenic sulfuric acid attack on different types of commercially produced concrete sewer pipes[J]10.1016/j.cemconres.2009.10.002 ↗
5. Review on microbially influenced concrete corrosion[J]10.3390/microorganisms11082076 ↗
6. Converting portions of the Los Angeles outfall sewer into a septic tank[J]
7. The corrosion of concrete 1. Isolation of a species of bacterium associated with the corrosion of concrete exposed to atmospheres containing hydrogen sulphide[J]
8. Biochemical attack on concrete in wastewater applications: A state of the art review[J]10.1016/j.cemconcomp.2010.05.001 ↗
9. Quantifying microbially induced deterioration of concrete: initial studies[J]10.1016/S0964-8305(02)00049-5 ↗
10. Current understanding and future approaches for controlling microbially influenced concrete corrosion: a review[J]
11. The ecology of acidophilic microorganisms in the corroding concrete sewer environment[J]10.3389/fmicb.2017.00683 ↗
12. Analysis of concrete from corroded sewer pipe[J]10.1016/S0964-8305(98)00049-3 ↗
13. Surface neutralization and H2S oxidation at early stages of sewer corrosion: Influence of temperature, relative humidity and H2S concentration[J]10.1016/j.watres.2012.05.011 ↗
14. Corrosion by bacteria of concrete in sewerage systems and inhibitory effects of formates on their growth[J]10.1016/S0043-1354(01)00473-0 ↗
15. Interactions of nutrients, moisture and pH on microbial corrosion of concrete sewer pipes[J]10.1016/0043-1354(92)90107-F ↗
16. Current understanding on microbiologically induced corrosion of concrete in sewer structures: A review of the evaluation methods and mitigation measures[J]10.1016/j.conbuildmat.2020.118539 ↗
17. Comparisons of alkali-activated binder concrete (ABC) with OPC concrete-A review[J]10.1016/j.cemconcomp.2022.104851 ↗
18. Corrosion resistance of alkali-activated slag cement[J]10.1680/adcr.2003.15.2.77 ↗
19. Resistance of fly ash based geopolymer mortars in sulfuric acid[J]
20. Performance of alkali-activated slag mortars exposed to acids[J]
21. Characterization and comparison of corrosion layer microstructure between cement mortar and alkali-activated fly ash/slag mortar exposed to sulfuric acid and acetic acid[J]10.3390/ma15041527 ↗
22. Decalcification resistance of alkali-activated slag[J]10.1016/j.jhazmat.2012.06.063 ↗
23. Decalcification of alkali-activated slag pastes. Effect of the chemical composition of the slag[J]10.1617/s11527-014-0422-4 ↗
24. Durability of calcium aluminate and sulphate resistant Portland cement based mortars in aggressive sewer environment and sulphuric acid[J]10.1016/j.cemconres.2019.105852 ↗
25. Influence of different activators on microstructure and strength of alkali-activated nickel slag cementitious materials[J]10.1016/j.conbuildmat.2019.117449 ↗
26. Early hydration and microstructure formation of ultra-rapid hardening alkali-activated slag cement (URHA) at presence of MgO[J]10.1016/j.cemconcomp.2025.106057 ↗
27. Influence of silica fume content on microstructure development and bond to steel fiber in ultra-high strength cement-based materials (UHSC)[J]10.1016/j.cemconcomp.2016.05.005 ↗
28. Study of acidic degradation of alkali-activated materials using synthetic C-(N)-ASH and NASH gels[J]10.1016/j.compositesb.2021.109510 ↗
29. Acid resistance of alkali-activated binders: A review of performance, mechanisms of deterioration and testing procedures[J]10.1016/j.conbuildmat.2022.128057 ↗
30. Degradation process of alkali-activated slag/fly ash and Portland cement-based pastes exposed to phosphoric acid[J]10.1016/j.conbuildmat.2019.117209 ↗
31. Sulphuric acid resistance of cementitious materials: Multiscale approach to assessing the degradation[J]10.1061/(ASCE)MT.1943-5533.0003261 ↗
32. Resistance of alkali-activated blast furnace slag to acids[C]
33. Review of microbially induced corrosion and comments on needs related to testing procedures[J]10.5703/1288284315388 ↗
34. Pore solution composition of alkali-activated slag/fly ash pastes[J]10.1016/j.cemconres.2018.10.010 ↗
35. Evaluation of extent of corrosion degradation and deterioration mechanism of hybrid alkali-activated mortar subjected to sulfuric acid and hydrochloric acid solutions[J]
36. Modification of phase evolution in alkali-activated blast furnace slag by the incorporation of fly ash[J]10.1016/j.cemconcomp.2013.09.006 ↗
37. Proposed structure for calcium silicate hydrate gel[J]10.1111/j.1151-2916.1986.tb07446.x ↗
38. Hydration products and reactivity of blast-furnace slag activated by various alkalis[J]10.1111/j.1151-2916.2003.tb03623.x ↗
39. Expansion behavior and microstructure change of alkali-activated slag grouting material in carbonate environment[J]10.1016/j.conbuildmat.2020.120593 ↗
40. Hydration characteristics and microstructure of alkali-activated slag concrete: a review[J]10.1016/j.eng.2021.07.026 ↗
41. Silica fume and waste glass in cement concrete production: A review[J]
42. Gel nanostructure in alkali-activated binders based on slag and fly ash, and effects of accelerated carbonation[J]10.1016/j.cemconres.2013.06.007 ↗
43. Influence of slag chemistry on the hydration of alkali-activated blast-furnace slag—Part I: Effect of MgO[J]10.1016/j.cemconres.2011.05.002 ↗
44. Synthesis and characterization of the LDH hydrotalcite–pyroaurite solid-solution series[J]10.1016/j.cemconres.2009.08.031 ↗
45. Degradation resistance of different cementitious materials to phosphoric acid attack at early stage[J]10.1016/j.cemconres.2021.106606 ↗
46. Mechanical and microstructural properties of heat cured alkali-activated slag mortars10.1016/j.matdes.2011.10.005 ↗
47. Effect of alkali dosage and silicate modulus on the deterioration of alkali-activated concrete properties subjected to sodium chloride attack and freeze thaw cycles[J]10.1016/j.conbuildmat.2024.138335 ↗
48. Influence of curing schedule on the integrity of geopolymers[J]10.1007/s10853-006-0533-6 ↗
49. Influence of cement type on resistance to attack from two carboxylic acids[J]10.1016/j.cemconcomp.2017.07.004 ↗