Deformation of heated and loaded wooden stick: Towards fire safety design of timber structure
Source abstract
Abstract
Mass timber construction has been emerging in architecture because of exceptional durability, sustainability, and versatility. This work applies the 3-point bending test to a reduced-scale wooden stick with a supporting span of 16.5 cm, under loads up to 560 times its self-weight under raised environmental temperatures up to 300 °C in the oven. The experiments quantify the deformation, critical shear stress of rupture, and degradation mass losses of the heated wood before ignition and combustion, while the numerical model further analyses the detailed thermomechanical responses. Results show that with increasing temperature, the deflection of loaded wooden sticks increases, driven by drying, thermal creep deformation, and thermal degradation. Moreover, the critical shear stress and temperature for wooden sticks rupture decrease, primarily caused by the thermal degradation of wood. The effects of fire-scene temperature on bending strength and modulus of elasticity on the loss of load-bearing capacity for wooden sticks are further quantified with numerical simulation. This work reveals the pre-ignition thermomechanical behaviours of wood under fire scenes, which supports early warnings for ignition and collapse, fire resilience design, and structural-fire stability assessment for wooden structures. • Applying 3-point bending tests on wooden sticks under simulated fire thermal impact. • Determining the critical shear stresses for wood stick rupture at elevated temperatures. • Examining the load-bearing capacity and bending strength as temperature rises to charring. • Numerical simulation of fire load to reveal variation of timber elasticity and rupture stress.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Wood Treatment and Properties · Fire dynamics and safety research · Tree Root and Stability Studies
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (46)
Show source-provided references
1. A review of structural, thermo-physical, acoustical, and environmental properties of wooden materials for building applications10.1016/j.buildenv.2016.12.033 ↗
2. A flame-retardant densified wood as robust and fire-safe structural material10.1007/s00226-022-01415-9 ↗
3. Design of taller timber buildings subjected to accidental loads: a state-of-the-art review
4. The predictive research of ancient wooden building internal defects compressive bearing capacity based on nondestructive testing methods10.1080/15376494.2018.1556826 ↗
5. Influence of natural aging on wood combustion heat release10.1007/s00226-024-01565-y ↗
6. Tall timber buildings: what’s next in fire safety10.1007/s10694-015-0497-7 ↗
7. Structure–property–function relationships of natural and engineered wood10.1038/s41578-020-0195-z ↗
8. Processing bulk natural wood into a high-performance structural material10.1038/nature25476 ↗
9. Efficient nonlinear modeling of strong wood frame shear walls for mid-rise buildings10.1016/j.engstruct.2020.110670 ↗
10. Thickness of zero-strength layer in timber beam exposed to fuel-controlled parametric fires10.1007/s00226-023-01480-8 ↗
11. Zelinka · 2020
12. Fire dynamics in mass timber compartments10.1016/j.firesaf.2020.103098 ↗
13. Review of large-scale CLT compartment fire tests10.1016/j.conbuildmat.2021.126099 ↗
14. Use of pre-charred surfaces to improve fire performance of wood10.1016/j.firesaf.2023.103745 ↗
15. A review of factors affecting the burning behaviour of wood for application to tall timber construction10.1007/s10694-018-0787-y ↗
16. Scale modeling of thermo-structural fire tests of multi-orientation wood laminates10.1007/s00226-024-01568-9 ↗
17. Fire engulfs ethnic village in SW China
18. Honey maps the Pb fallout from the 2019 fire at Notre-Dame Cathedral, Paris: a geochemical perspective10.1021/acs.estlett.0c00485 ↗
19. University of Nottingham laboratory fire probed by safety officers. BBC NEWS 2014.
20. A review of kinetics data for the pyrolysis of wood and related substances10.1016/S0010-2180(70)80037-2 ↗
21. Pyrolysis and spontaneous ignition of wood under transient irradiation: experiments and a-priori predictions10.1016/j.firesaf.2017.03.081 ↗
22. Structural response of cross-laminated timber compression elements exposed to fire10.1016/j.firesaf.2017.05.010 ↗
23. Charring rate of wood as a tool for fire investigations10.1016/j.firesaf.2005.05.006 ↗
24. The effect of chemical composition on the charring of wood across scales10.1016/j.proci.2018.06.080 ↗
25. Effect of oxygen on the burning rate of wood10.1016/j.combustflame.2021.111591 ↗
26. Experimental study and theoretical analysis of fire resistance properties of prestressed glued laminated timber beams10.1016/j.conbuildmat.2024.135967 ↗
27. Fire performance of cultural heritage and contemporary timbers10.1016/j.engstruct.2019.109739 ↗
28. Proposal for a new formula to predict the fire resistance of timber connections10.1016/j.engstruct.2019.110041 ↗
29. Hirashima T., Yamashita H., Ishi S., Igarashi T., Baba S., Someya T. Deformation behaviour and failure time of glued laminated timber columns in fire. The 11th International Conference on Structures in Fire, 2020.10.14264/beec17b ↗
30. Li Y. Factors Affecting the Structural Integrity of Wood-Based Composites: Elevated Temperature and Adhesive Bonding, Virginia Tech, 2021.
31. Smoldering ignition and emission dynamics of wood under low irradiation10.1002/fam.3107 ↗
32. Correlation between charring rate and oxygen permeability for 12 different wood species10.1007/s10086-006-0816-1 ↗
33. Minimum oxygen supply rate for smouldering propagation: effect of fuel bulk density and particle size10.1016/j.combustflame.2024.113292 ↗
34. The effects of timber species and adhesive type on the behavior of finger joints in tension under fire conditions10.1016/j.conbuildmat.2024.138080 ↗
35. Structural performance and charring of loaded wood under fire10.1016/j.engstruct.2020.111491 ↗
36. Flammability behaviour of wood and a review of the methods for its reduction10.1186/2193-0414-2-4 ↗
37. Reaction to fire of the timber structure encapsulated by multilayer mortar coating under uniform thermal loading10.1007/s10694-024-01622-9 ↗
38. Deformation of wood slice in fire: Interactions between heterogeneous chemistry and thermomechanical stress10.1016/j.proci.2020.08.060 ↗
39. Structural fire engineering considerations for cross-laminated timber walls10.1016/j.conbuildmat.2022.126605 ↗
40. Structural response of fire-exposed cross-laminated timber beams under sustained loads10.1016/j.firesaf.2016.08.002 ↗
41. Thermal degradation of bending properties of structural wood and wood-based composites10.1515/hf.2011.001 ↗
42. Shear strengths of wood measured by various short beam shear test methods10.1007/s00226-003-0180-x ↗
43. Effect of heat treatment (ThermoWood) on some surface properties of parquet beech (Fagus orientalis Lipsky.) with different layers of UV system applied10.15376/biores.12.2.3876-3889 ↗
44. Effects of thermal treatment on chemical, mechanical and colour traits in Norway spruce wood10.1016/j.biortech.2013.06.110 ↗
45. Thermal degradation of beech wood with thermogravimetry/Fourier transform infrared analysis10.1016/j.enconman.2016.05.007 ↗
46. Bauchau O.A., Craig J.I. Euler-Bernoulli beam theory, 2009, p. 173–221.10.1007/978-90-481-2516-6_5 ↗