journal article·2024-12Open access

Experimental assessment of FRP repairing in concrete cylinders exposed high temperatures

Yunus Emrahan Akbulut, Safa Nayır, Ahmet Can Altunışık, Volkan Kahya, Muhammet Oğuz Sünnetci, Hakan Ersoy

Abstract

This study presents an experimental evaluation of fiber-reinforced polymer (FRP) strengthening in concrete specimens damaged by exposure to high temperatures. For this purpose, sixty cylindrical concrete specimens were produced. Specimens exposed to temperatures of 200 °C, 400 °C, and 600 °C were strengthened using carbon and glass FRP fabrics in two or three layers. Compression tests were conducted to assess the strength of the specimens. The impact of temperature, fabric type, and the number of fabric layers on the concrete's strength was thoroughly investigated. Digital microscopy was employed to explore the formation of cracks due to temperature changes, followed by Scanning Electron Microscopy (SEM) analyses to examine the microscopic structural changes in the concrete samples. The study highlights the importance of considering changes in both strength and behavior models together when evaluating the strengthening contributions provided by FRP. The results indicate that FRP applications on fire-damaged concrete structures can provide effective strengthening up to 400 °C but may be insufficient at temperatures of 600 °C and above. Although an effective increase in strength was achieved at 600 °C, low levels of ductility were observed, which is undesirable for an engineering structure. Therefore, it has been determined that FRP-strengthening applications may not be effective in reinforced concrete (RC) structural elements exposed to temperatures of 600°C and higher.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Structural Behavior of Reinforced Concrete · Fire effects on concrete materials · Structural Load-Bearing Analysis

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (62)

Show source-provided references
1. Strength and durability recovery of fire-damaged concrete after post-fire-curing10.1016/S0008-8846(01)00582-8 ↗
2. Mechanical properties of high-strength concrete after fire10.1016/j.cemconres.2003.11.007 ↗
3. Effects of elevated temperatures on properties of concrete10.1016/j.firesaf.2007.01.003 ↗
4. Effects of concrete types, elevated temperatures, and different cooling technique on concrete compressive strength
5. Yüksek sıcaklığın ve farklı soğutma koşulunun kalker agregalı betonlar üzerindeki etkilerinin araştırılması, Gazi Üniv
6. Mechanical properties of concrete composites subject to elevated temperature10.1016/j.firesaf.2017.10.010 ↗
7. Effect of elevated temperature on mechanical properties of normal strength concrete: an overview
8. Residual compressive strength of plain and fiber reinforced concrete after exposure to different heating and cooling regimes10.1080/19648189.2021.1960898 ↗
9. Effects of cement dosage and cooling regimes on the compressive strength of concrete after post-fire-curing from 800 °C10.1016/j.conbuildmat.2017.03.053 ↗
10. Post-cooling properties of concrete exposed to fire10.1016/j.firesaf.2017.06.010 ↗
11. Fiber-reinforced polymer-strengthened/reinforced concrete structures exposed to fire: a review10.2749/101686612X13363929517613 ↗
12. Fire behaviour of FRP-strengthened reinforced concrete structural elements: a state-of-the-art review10.1016/j.compositesb.2015.05.045 ↗
13. Performances, challenges and opportunities in strengthening reinforced concrete structures by using FRPs – a state-of-the-art review10.1016/j.engfailanal.2020.104480 ↗
14. Elevated temperature behaviour of carbon fibre-reinforced polymer applied by hand lay-up (M-CFRP) under simultaneous thermal and mechanical loadings: Experimental and analytical investigation10.1016/j.firesaf.2018.07.007 ↗
15. Numerical parametric studies on the fire endurance of fibre-reinforced-polymer-confined concrete columns10.1139/l04-071 ↗
16. Numerical evaluation of the post-earthquake fire resistance of CFRP-strengthened reinforced concrete joints based on experimental observations10.1080/19648189.2015.1018448 ↗
17. Modeling of stiffness of FRP composites under elevated and high temperatures10.1016/j.compscitech.2008.07.005 ↗
18. J. Kumar, R. Bajpai, Performance of FRP Confined Concrete Columns In Fire, 2012.10.47893/IJATCE.2012.1014 ↗
19. Effects of elevated temperatures on the compressive strength capacity of concrete cylinders confined with FRP sheets: an experimental investigation10.1155/2015/549187 ↗
20. Effects of bars slippage on the pre-and post-heating flexural behavior of FRP reinforced concrete beams: experimental and theoretical investigations
21. Behavior of CFRP-reinforced concrete columns at elevated temperatures10.1016/j.conbuildmat.2022.129425 ↗
22. Behavior of FRP-confined concrete after high temperature exposure10.1016/j.conbuildmat.2010.06.103 ↗
23. Failure modes of reinforced concrete beams strengthened with carbon fiber sheet in fire10.1016/j.firesaf.2009.05.006 ↗
24. The performance of near-surface mounted CFRP strengthened RC beam in fire10.1016/j.firesaf.2017.04.031 ↗
25. Structural performance of concrete sandwich panels under fire10.1016/j.firesaf.2021.103293 ↗
26. Experimental study of the effect of different insulation schemes on fire performance of FRP strengthened concrete: FIRECOAT and REALROCK10.1186/s40069-023-00604-5 ↗
27. Evaluating the high-temperature endurance of FRP-strengthened concrete using an innovative insulation system: experimental investigation
28. Investigation of insulated FRP-wrapped reinforced concrete columns in fire10.1016/j.firesaf.2006.10.007 ↗
29. Performance in fire of FRP-strengthened and insulated reinforced concrete columns10.1016/j.firesaf.2012.08.006 ↗
30. Experimental evaluation of the fire behaviour of insulated fibre-reinforced-polymer-strengthened reinforced concrete columns10.1016/j.firesaf.2006.05.004 ↗
31. Strengthening fire-damaged concrete by confinement with fibre-reinforced polymer wraps10.1016/j.engstruct.2011.07.002 ↗
32. Seismic strengthening of shear critical post-heated circular concrete columns wrapped with FRP composite jackets10.1016/j.compstruct.2011.09.004 ↗
33. Compressive strength of concrete damaged by elevated temperature and confined by CFRP fabrics
34. Axial compression behavior of fire-damaged concrete cylinders confined with CFRP sheets10.1061/(ASCE)CC.1943-5614.0000683 ↗
35. Compressive behavior of heat-damaged square concrete prisms confined with basalt fiber-reinforced polymer jackets10.1016/j.engstruct.2021.112504 ↗
36. Restorability of strength and stiffness of fire damaged concrete using various composite confinement techniques10.1016/j.conbuildmat.2020.121984 ↗
37. Repair of thermally damaged concrete cylinders with basalt fiber-reinforced polymer jackets
38. Experimental and numerical study on wrapping concrete cylinders post heating and cooling under preload using CFRP fabrics10.1016/j.istruc.2019.10.005 ↗
39. Experimental and numerical study of strengthening and repairing heat-damaged RC circular column using hybrid system of CFRP
40. Repair of fire damaged circular reinforced concrete columns with FRP composites10.1016/j.conbuildmat.2010.06.017 ↗
41. L.A. Bisby, J.F. Chen, S.Q. Li, T.J. Stratford, N. Cueva, K. Crossling, Strengthening fire damaged circular concrete columns with FRP, in: Advanced Composites in Construction 2011, ACIC 2011 - Proceedings of the 5th International Conference, 2011.
42. Strengthening of heat damaged reinforced concrete short columns10.1260/2040-2317.5.4.381 ↗
43. Experimental and numerical study of the behaviour of heat-damaged RC circular columns confined with CFRP fabric10.1016/j.compstruct.2015.07.116 ↗
44. An experimental investigation of the behaviour of heat-damaged RC columns confined with CFRP fabrics using photogrammetry10.1617/s11527-016-0873-x ↗
45. FRP Confinement of heat-damaged circular RC columns10.1007/s40069-016-0181-4 ↗
46. Experimental and analytical investigation on strengthening of heat damaged concrete by textile reinforced concrete (TRC)10.1016/j.acme.2019.09.008 ↗
47. Behavior of heat damaged circular reinforced concrete columns repaired using carbon fiber reinforced polymer rope
48. Repair of post-heated short rectangular reinforced concrete columns with FRP jackets10.1016/j.istruc.2021.10.038 ↗
49. Flexural strengthening of fire-damaged GFRP-reinforced concrete beams using CFRP sheet: experimental and analytical study10.1016/j.compstruct.2022.115378 ↗
50. Experimental behavior of fire-exposed reinforced concrete slabs without and with FRP retrofitting
51. Repair of fire-damaged RC square columns with CFRP textile-reinforced ECC matrix10.1016/j.engstruct.2023.116530 ↗
52. Analytical model to predict axial stress-strain behavior of heat-damaged unreinforced concrete columns wrapped by FRP jacket10.1016/j.engstruct.2023.116244 ↗
53. Stress–strain model for FRP confined heat-damaged concrete columns10.1016/j.firesaf.2023.103748 ↗
54. Unified strength model for FRP confined heat-damaged circular and square concrete columns10.1016/j.compstruct.2022.116647 ↗
55. Stress-strain models for FRP-confined thermally damaged concrete
56. TS 802, Design of Concrete Mixes, Turkish Standards Institute, Ankara, 2016.
57. TS EN 206, Concrete - Specification, performance, production and conformity, Ankara, Türkiye, 2021.
58. Performance of metakaolin concrete at elevated temperatures10.1016/S0958-9465(01)00061-0 ↗
59. Master Builders Solutions, MasterBrace: Technical Data Sheets, (n.d.). 〈https://www.master-builders-solutions.com/en-au/about-us/news/master-builders-solutions-australia-technical-datasheet〉 (accessed March 9, 2024).
60. EN 12390-3, Testing hardened concrete - Part 3: Compressive strength of test specimens, 2019.
61. Stress-strain behaviour of normal compacting and self compacting concrete under elevated temperatures10.1260/2040-2317.5.1.63 ↗
62. Assessment of damage on geo-mechanical and micro-structural properties of weak calcareous rocks exposed to fires using thermal treatment coefficient10.1016/j.enggeo.2021.106046 ↗