Long-term influence of tailings wastewater on mechanical performance and microstructure of dam concrete: A case study in southeastern China
Source abstract
Abstract
Tailings wastewater contains a large number of harmful ions which damage the hydraulic concrete structures and seriously affect the safety of water conservancy systems. This paper studied the dam concrete of a medium-sized reservoir in southeastern China which was corroded by tailings wastewater. To this end, a long-term follow-up investigation was conducted into the corrosion of the dam concrete during the period from 2013 to 2019. A multiscale analysis was also carried out on the long-term influence of the tailings wastewater on the mechanical performance and microstructure of the dam concrete. The results revealed that the corrosion by the tailings wastewater containing H+ and SO42− caused a significant decline in the mechanical performance of the dam concrete in terms of the increase in the carbonation depth and the reduction of the compressive strength. Compared to the time period from 2006 to 2013, the rate of corrosion slowed down during 2013–2019. Furthermore, the main reason for the deterioration of the dam concrete was that the attack of H+ and SO42− resulted in the dissolution erosion and expansion erosion of the dam concrete. The dissolution erosion of the concrete led to the increase in the average pore diameter, median pore diameter, and porosity of the dam concrete, while the expansion erosion improved the formation of gypsum and ettringite. Moreover, the dam concrete experienced various degrees of corrosion in different zones. Specifically, the dissolution erosion was most serious in the tidal zone, while the expansion erosion was severest in the submerged zone. Finally, this paper can provide a frame of reference for the research on the corrosion mechanism and service safety of hydraulic concrete structures eroded by various types of tailings wastewater.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Tailings Management and Properties · Mine drainage and remediation techniques · Arsenic contamination and mitigation
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (35)
Show source-provided references
1. Mine tailings dams: characteristics, failure, environmental impacts, and remediation10.1016/j.apgeochem.2014.09.010 ↗
2. Aqueous oxidation of pyrite by molecular oxygen10.1021/cr00051a001 ↗
3. Geochemistry of Cd in the secondary environment near abandoned metalliferous mines, Wales10.1016/S0883-2927(09)80006-1 ↗
4. Population Exposure To Trace Elements In The Kilembe Copper Mine Area, Western Uganda: a pilot study
5. Mine-water chemistry: the good, the bad and the ugly10.1007/s002540050204 ↗
6. Biologically produced sulphide for purification of process streams, effluent treatment and recovery of metals in the metal and mining industry10.1016/j.hydromet.2006.03.017 ↗
7. Removal of pollutants from acid mine wastewater using metallurgical by-product slags10.1016/j.seppur.2004.01.003 ↗
8. Cyanide ion concentration in the effluent from two gold mines in Zimbabwe and in a stream receiving effluent from one of the goldmines
9. Sources, distribution and storage of heavy metals in the Rio Pilcomayo, Bolivia10.1016/S0375-6742(01)00164-9 ↗
10. Water contamination with heavy metals and trace elements from Kilembe copper mine and tailing sites in Western Uganda; implications for domestic water quality10.1016/j.chemosphere.2016.11.077 ↗
11. Mercury contamination in the Carson River, Nevada: a preliminary study of the impact of mining wastes10.1007/BF00283569 ↗
12. Effects of acidic water on hydro-mechanical properties of asphalt concrete
13. Interaction of treated industrial wastewater and zeolite on compressive strength of plain concrete in different cement contents and curing ages
14. Sulfate attack of concrete building foundations induced by sewage waters10.1016/S0008-8846(01)00752-9 ↗
15. Physical sulfate attack on concrete lining–A field case analysis
16. The durability of a concrete sewer pipeline under deterioration by sulphate and chloride corrosion10.1016/j.proeng.2016.08.229 ↗
17. Effects of Acid Rain On Deterioration Of Coquina At Castle De San Macros Monument. Materials Degradation Caused by Acid Rain
18. Research on mechanism of concrete corrosion subjected to underground acid liquid10.4028/www.scientific.net/KEM.302-303.91 ↗
19. Investigation of the effects of acid rain on the deterioration of cement concrete using accelerated tests established in laboratory10.1016/j.atmosenv.2004.05.017 ↗
20. Modeling of damage in cement-based materials subjected to external sulfate attack. ii: comparison with experiments10.1061/(ASCE)0899-1561(2003)15:4(314) ↗
21. Sulfate attack expansion mechanisms10.1016/j.cemconres.2013.07.005 ↗
22. Mechanism of expansion associated with ettringite formation10.1016/0008-8846(73)90056-2 ↗
23. Mechanism of expansion of mortars immersed in sodium sulfate solutions10.1016/j.cemconres.2012.10.001 ↗
24. Magnesium sulfate attack on Portland cement paste: I. Microstructural analysis10.1016/0008-8846(92)90147-N ↗
25. Mechanism of sulfate attack: a fresh look: Part 1: summary of experimental results10.1016/S0008-8846(02)00724-X ↗
26. An experimental study of combined acid and sulfate attack of concrete10.1016/S0958-9465(03)00123-9 ↗
27. Physicochemical study on the interface zone of concrete exposed to different sulfate solutions
28. Magnesium sulfate attack on hardened blended cement pastes under different circumstances10.1016/S0008-8846(02)00801-3 ↗
29. Stability and decomposition mechanism of ettringite in presence of ammonium sulfate solution10.1016/j.conbuildmat.2016.07.135 ↗
30. Thaumasite sulfate attack on concrete: mechanisms, influential factors and mitigation10.1016/j.conbuildmat.2014.09.034 ↗
31. Degradation mechanisms of cast-in-situ concrete subjected to internal-external combined sulfate attack
32. Effect of physical and chemical sulfate attack on performance degradation of concrete under different conditions
33. A chemo-transport-damage model for concrete under external sulfate attack10.1016/j.cemconres.2020.106048 ↗
34. Macro-microscopically numerical analysis on expansion response of hardened cement paste under external sulfate attack10.1016/j.conbuildmat.2019.02.159 ↗
35. China National Standards. Standard for test method of mechanical properties on ordinary concrete. GB/T50081–2019.