journal article·2026-02

Sustainable synthesis of porous reaction-formed SiC ceramics through siliconization of waste fabric-derived carbon preforms using reclaimed Si wafers

Dulal Das, Jinha Kim, Heeju Kim, Sungho Lee, Hyeondeok Jeong

Carbon Letters· Volume 36· Issue 1
Publisher page

Abstract

No abstract is available for this record. The assistant can identify its topic from the title, but cannot infer the study’s results.

Source: Not provided · Quality: missing

Research context

OpenAlex topics: Advanced ceramic materials synthesis · Silicon Carbide Semiconductor Technologies · Aerogels and thermal insulation

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (78)

Show source-provided references
1. Ohji T, Fukushima M (2012) Macro-porous ceramics: processing and properties. Int Mater Rev 57:115–131. https://doi.org/10.1179/1743280411Y.000000000610.1179/1743280411Y.0000000006 ↗
2. Colombo P (2008) In praise of pores. Science 322:381–383. https://doi.org/10.1126/science.116296210.1126/science.1162962 ↗
3. Ihle J, Martin HP, Herrmann M et al (2006) The influence of porosity on the electrical properties of liquid-phase sintered silicon carbide. Int J Mater Res 97:649–656. https://doi.org/10.3139/146.10128510.3139/146.101285 ↗
4. Fukushima M, Zhou Y, Miyazaki H et al (2006) Microstructural characterization of porous silicon carbide membrane support with and without alumina additive. J Am Ceram Soc 89:1523–1529. https://doi.org/10.1111/j.1551-2916.2006.00931.x10.1111/j.1551-2916.2006.00931.x ↗
5. Fukushima M, Zhou Y, Yoshizawa YI (2008) Fabrication and microstructural characterization of porous silicon carbide with nano-sized powders. Mater Sci Eng B 148:211–214. https://doi.org/10.1016/j.mseb.2007.09.02610.1016/j.mseb.2007.09.026 ↗
6. Majoulet O, Sandra F, Bechelany MC et al (2013) Silicon–boron–carbon–nitrogen monoliths with high, interconnected and hierarchical porosity. J Mater Chem A 1:10991–11000. https://doi.org/10.1039/C3TA12119D10.1039/C3TA12119D ↗
7. Zhang BX, Zhang Y, Luo Z et al (2019) Monolithic silicon carbide with interconnected and hierarchical pores fabricated by reaction-induced phase separation. J Am Ceram Soc 102:3860–3869. https://doi.org/10.1111/jace.1626310.1111/jace.16263 ↗
8. Durif C, Wynn M, Balestrat M et al (2019) Open-celled silicon carbide foams with high porosity from boron-modified polycarbosilanes. J Eur Ceram Soc 39:5114–5122. https://doi.org/10.1016/j.jeurceramsoc.2019.08.01210.1016/j.jeurceramsoc.2019.08.012 ↗
9. Gomez-Gomez A, Moyano JJ, Roman-Manso B et al (2019) Highly-porous hierarchical SiC structures obtained by filament printing and partial sintering. J Eur Ceram Soc 39:688–695. https://doi.org/10.1016/j.jeurceramsoc.2018.12.03410.1016/j.jeurceramsoc.2018.12.034 ↗
10. Sandra F, Ballestero A, Nguyen VL et al (2016) Silicon carbide-based membranes with high soot particle filtration efficiency, durability and catalytic activity for CO/HC oxidation and soot combustion. J Membr Sci 501:79–92. https://doi.org/10.1016/j.memsci.2015.12.01510.1016/j.memsci.2015.12.015 ↗
11. Zhou Y, Fukushima M, Miyazaki H et al (2011) Preparation and characterization of tubular porous silicon carbide membrane supports. J Membr Sci 369:112–118. https://doi.org/10.1016/j.memsci.2010.11.05510.1016/j.memsci.2010.11.055 ↗
12. Chithra A, Rajeev R, Prabhakaran K (2022) C/SiO2 and C/SiC composite foam monoliths from rice husk for thermal insulation and EMI shielding. Carbon Lett 32(2):639–651. https://doi.org/10.1007/s42823-021-00303-910.1007/s42823-021-00303-9 ↗
13. Das D, Lucio MDS, Oh Y, Kim YW (2024) Tuning the electrical, thermal, and mechanical properties of porous SiC ceramics using metal carbides. J Eur Ceram Soc 44:3020–3030. https://doi.org/10.1016/j.jeurceramsoc.2023.12.01710.1016/j.jeurceramsoc.2023.12.017 ↗
14. Soto C, Garcia-Rosales C, Echeberria J et al (2017) SiC-based sandwich material for flow channel inserts in DCLL blankets: manufacturing, characterization, corrosion tests. Fusion Eng Des 124:958–963. https://doi.org/10.1016/j.fusengdes.2017.05.05910.1016/j.fusengdes.2017.05.059 ↗
15. Lara A, Ortiz AL, Munoz A, Rodriguez AD (2012) Densification of additive-free polycrystalline β-SiC by spark-plasma sintering. Ceram Int 38:45–53. https://doi.org/10.1016/j.ceramint.2011.06.03610.1016/j.ceramint.2011.06.036 ↗
16. Lee EJ, Lee DW, Kim JC, Kim DJ (2014) Densification behavior of high purity SiC by hot pressing. Ceram Int 40:16389–16392. https://doi.org/10.1016/j.ceramint.2014.07.14310.1016/j.ceramint.2014.07.143 ↗
17. Liang H, Yao X, Zhang J et al (2014) The effect of rare earth oxides on the pressureless liquid phase sintering of α-SiC. J Eur Ceram Soc 34:2865–2874. https://doi.org/10.1016/j.jeurceramsoc.2014.03.02910.1016/j.jeurceramsoc.2014.03.029 ↗
18. Eom JH, Seo YK, Kim YW (2016) Mechanical and thermal properties of pressureless sintered silicon carbide ceramics with alumina-yttria-calcia. J Am Ceram Soc 99:1735–1741. https://doi.org/10.1111/jace.1411410.1111/jace.14114 ↗
19. Xue R, Liu P, Zhang Z et al (2021) Improvement of toughness of reaction bonded silicon carbide composites reinforced by surface-modified SiC whiskers. Ceram Int 47:18150–18156. https://doi.org/10.1016/j.ceramint.2021.03.13310.1016/j.ceramint.2021.03.133 ↗
20. Santhosh B, Ionescu E, Andreolli F et al (2021) Effect of pyrolysis temperature on the microstructure and thermal conductivity of polymer-derived monolithic and porous SiC ceramics. J Eur Ceram Soc 41:1151–1162. https://doi.org/10.1016/j.jeurceramsoc.2020.09.02810.1016/j.jeurceramsoc.2020.09.028 ↗
21. Ye Z, Wang Y, Xiong X et al (2024) Microstructure, interfacial and mechanical properties of SiC interphase modified C/C-SiC composites prepared by reactive melt infiltration. J Eur Ceram Soc 44:116785. https://doi.org/10.1016/j.jeurceramsoc.2024.11678510.1016/j.jeurceramsoc.2024.116785 ↗
22. Sun J, Zhang J, Zhang X et al (2024) High strength mullite-bond SiC porous ceramics fabricated by digital light processing. J Adv Ceram 13:53–62. https://doi.org/10.26599/JAC.2024.922083510.26599/JAC.2024.9220835 ↗
23. Lucio MD, Kultayeva S, Kim YW, Song IH (2022) Effects of SiC whisker addition on mechanical, thermal, and permeability properties of porous silica-bonded SiC ceramics. Int J Appl Ceram Technol 19:1439–1452. https://doi.org/10.1111/ijac.1395710.1111/ijac.13957 ↗
24. Chiang YM, Messner RP, Terwilliger CD, Behrendt DR (1991) Reaction-formed silicon carbide. Mater Sci Eng A 144:63–74. https://doi.org/10.1016/0921-5093(91)90210-E10.1016/0921-5093(91)90210-E ↗
25. Xia H, Qiao G, Zhou S, Wang J (2013) Reciprocating friction and wear behavior of reaction-formed SiC ceramic against bearing steel ball. Wear 303:276–285. https://doi.org/10.1016/j.wear.2013.03.03810.1016/j.wear.2013.03.038 ↗
26. Cai N, Ma R, Qiao GJ, Jin ZH (2001) Reaction mechanism of silicon carbide ceramics derived from woods. J Inorg Mater 16:763–768
27. Wang Y, Tan S, Jiang D (2004) The effect of porous carbon preform and the infiltration process on the properties of reaction-formed SiC. Carbon 42:1833–1839. https://doi.org/10.1016/j.carbon.2004.03.01810.1016/j.carbon.2004.03.018 ↗
28. Xu S, Qiao G, Li D et al (2009) Reaction forming of silicon carbide ceramic using phenolic resin derived porous carbon preform. J Eur Ceram Soc 29:2395–402. https://doi.org/10.1016/j.jeurceramsoc.2009.01.02210.1016/j.jeurceramsoc.2009.01.022 ↗
29. Pampuch R, Walasek E, Bialoskorski J (1986) Reaction-mechanism in carbon liquid silicon systems at elevated-temperatures. Ceram Int 12:99–106. https://doi.org/10.1016/0272-8842(86)90023-410.1016/0272-8842(86)90023-4 ↗
30. Kim J, Kim S, Song S, Lee D (2020) Effects of residual Si on the ablation properties of biomorphic C/SiC composites for reusable thermal protection systems. Adv Compos Mater 30:91–102. https://doi.org/10.1080/09243046.2020.179012410.1080/09243046.2020.1790124 ↗
31. Wang Y, Tan S, Jiang D (2004) The fabrication of reaction-formed silicon carbide with controlled microstructure by infiltrating a pure carbon preform with molten Si. Ceram Int 30:435–439. https://doi.org/10.1016/S0272-8842(03)00128-710.1016/S0272-8842(03)00128-7 ↗
32. Zhou XN, Hao X, Xu JQ et al (2024) Light-weight, wood-derived, biomorphic SiC ceramics by carbothermal reduction. Ceram Int 50:23135–23149. https://doi.org/10.1016/j.ceramint.2024.04.03710.1016/j.ceramint.2024.04.037 ↗
33. Cho SY, Jang D, Kim SH et al (2025) Unexpected flame retardancy mechanism of sulfuric acid treated and pyrolyzed waste cotton fabrics. J Anal Appl Pyrolysis 186:106954. https://doi.org/10.1016/j.jaap.2025.10695410.1016/j.jaap.2025.106954 ↗
34. Kim J, Kwon W, Bai BC et al (2022) Recycling of cotton clothing into activated carbon fibers. Carbon Lett 32:1315–1327. https://doi.org/10.1007/s42823-022-00366-210.1007/s42823-022-00366-2 ↗
35. Deng R, Chang N, Lunardi MM et al (2021) Remanufacturing end-of‐life silicon photovoltaics: feasibility and viability analysis. Prog Photovoltaics Res Appl 29:760–774. https://doi.org/10.1002/pip.337610.1002/pip.3376 ↗
36. Tan J, Jia S, Ramakrishna S (2022) End-of-Life photovoltaic modules. Energies 15:5113. https://doi.org/10.3390/en1514511310.3390/en15145113 ↗
37. Liu W, Tian J, Xiang D, Mao R, Wang B (2020) Fabricating superior thermal conductivity SiC–AlN composites from photovoltaic silicon waste. J Clean Prod 274:122799. https://doi.org/10.1016/j.jclepro.2020.122799.X10.1016/j.jclepro.2020.122799.X ↗
38. Ren X, Ma B, Qian F et al (2021) Green synthesis of porous SiC ceramics using silicon kerf waste in different sintering atmospheres and pore structure optimization. Ceram Int 47:26366–26374. https://doi.org/10.1016/j.ceramint.2021.06.04710.1016/j.ceramint.2021.06.047 ↗
39. Messner RP, Chiang YM (1990) Liquid-phase reaction-bonding of silicon carbide using alloyed silicon–molybdenum melts. J Am Ceram Soc 73:1193–1200. https://doi.org/10.1111/j.1151-2916.1990.tb05179.x10.1111/j.1151-2916.1990.tb05179.x ↗
40. Margiotta JC, Zhang D, Nagle DC, Feeser CE (2008) Formation of dense silicon carbide by liquid silicon infiltration of carbon with engineered structure. J Mater Res 23:1237–1248. https://doi.org/10.1557/JMR.2008.016710.1557/JMR.2008.0167 ↗
41. Zhu F, Feng Q, Xu Y et al (2015) Kinetics of pyrolysis of ramie fabric wastes from thermogravimetric data. J Therm Anal Calorim 119:651–657. https://doi.org/10.1007/s10973-014-4179-310.1007/s10973-014-4179-3 ↗
42. Motaung TE, Gqokoma Z, Linganiso LZ, Hato MJ (2016) The effect of acid content on the poly (furfuryl) alcohol/cellulose composites. Polym Compos 37:2434–2441. https://doi.org/10.1002/pc.2342810.1002/pc.23428 ↗
43. Yang Z, He X, Wu M et al (2013) Infiltration mechanism of diamond/SiC composites fabricated by Si-vapor vacuum reactive infiltration process. J Eur Ceram Soc 33:869–878. https://doi.org/10.1016/j.jeurceramsoc.2012.09.01010.1016/j.jeurceramsoc.2012.09.010 ↗
44. Kim JH (2023) Control of the properties of a binder pitch to enhance the density and strength of graphite blocks. Carbon Lett 33:1757–1766. https://doi.org/10.1007/s42823-023-00515-110.1007/s42823-023-00515-1 ↗
45. Chen Y, Zhao Y, Liu D et al (2017) Fabrication and ultra-high-temperature properties of lightweight carbon-bonded carbon fiber composites. Ceram Int 45:22249–22252. https://doi.org/10.1016/j.ceramint.2019.07.25010.1016/j.ceramint.2019.07.250 ↗
46. Zhang Y, Lu Z, Yang Z et al (2017) Compression behaviors of carbon-bonded carbon fiber composites: experimental and numerical investigations. Carbon 116:398–408. https://doi.org/10.1016/j.carbon.2017.02.01210.1016/j.carbon.2017.02.012 ↗
47. Pati SK, Hwang Y, Lee HM, Kim BJ, Park S (2024) Porous activated carbon derived from petroleum coke as a high-performance anodic electrode material for supercapacitors. Carbon Lett 34:153–162. https://doi.org/10.1007/s42823-023-00628-710.1007/s42823-023-00628-7 ↗
48. Murugan N, Thangarasu S, Seo SB et al (2023) Facile synthesis of interconnected layered porous carbon framework for high-performance supercapacitors. Carbon Lett 33:791–802. https://doi.org/10.1007/s42823-023-00460-z10.1007/s42823-023-00460-z ↗
49. Joo JH, Kim SH, Kim JH et al (2025) Recent advances in activated carbon fibers for pollutant removal. Carbon Lett 35:21–44. https://doi.org/10.1007/s42823-024-00803-410.1007/s42823-024-00803-4 ↗
50. Kianfar E, Sayadi H (2022) Recent advances in properties and applications of nanoporous materials and porous carbons. Carbon Lett 32:1645–1669. https://doi.org/10.1007/s42823-022-00395-x10.1007/s42823-022-00395-x ↗
51. Greil P, Lifka T, Kaindl A (1998) Biomorphic cellular silicon carbide ceramics from wood: i. Processing and microstructure. J Eur Ceram Soc 18:1961–1973. https://doi.org/10.1016/S0955-2219(98)00156-310.1016/S0955-2219(98)00156-3 ↗
52. Shang J, Liu Y, Chen J et al (2025) Microstructure and mechanical properties of CfSic composites fabricated by RMI: effect of CfC preform heat treatment. Mater Charact 225:115171. https://doi.org/10.1016/j.matchar.2025.11517110.1016/j.matchar.2025.115171 ↗
53. Calderon NR, Martínez-Escandell M, Narciso J et al (2009) The combined effect of porosity and reactivity of the carbon preforms on the properties of SiC produced by reactive infiltration with liquid Si. Carbon 47:2200–2210. https://doi.org/10.1016/j.carbon.2009.04.00210.1016/j.carbon.2009.04.002 ↗
54. Dezellus O, Jacques S, Hodaj F, Eustathopoulos N (2005) Wetting and infiltration of carbon by liquid silicon. J Mater Sci 40:2307–11. https://doi.org/10.1007/s10853-005-1950-710.1007/s10853-005-1950-7 ↗
55. Whalen TJ, Anderson AT (1975) Wetting of SiC, Si3N4, and carbon by Si and binary Si alloys. J Am Ceram Soc 58:396–399. https://doi.org/10.1111/j.1151-2916.1975.tb19006.x10.1111/j.1151-2916.1975.tb19006.x ↗
56. Kultayeva S, Kim YW, Song IH (2021) Effects of dopants on electrical, thermal, and mechanical properties of porous SiC ceramics. J Eur Ceram Soc 41:4006–4015. https://doi.org/10.1016/j.jeurceramsoc.2021.01.04910.1016/j.jeurceramsoc.2021.01.049 ↗
57. Wan C, Xia P, Hua J et al (2025) Fabrication of SiC composites by selective laser sintering and reactive melt infiltration. Ceram Int 51:14842–14851. https://doi.org/10.1016/j.ceramint.2025.01.32710.1016/j.ceramint.2025.01.327 ↗
58. Shang J, Ma Y, Liu Y et al (2025) Optimizing reactive melt infiltration using compound carbon sources for SiC matrix with low-residual silicon content. J Eur Ceram Soc 8:117648. https://doi.org/10.1016/j.jeurceramsoc.2025.11764810.1016/j.jeurceramsoc.2025.117648 ↗
59. Das D, Lucio MD, Kultayeva S, Kim YW (2024) Effect of pore size on the flexural strength of porous silicon carbide ceramics. Open Ceram 17:100521. https://doi.org/10.1016/j.oceram.2023.10052110.1016/j.oceram.2023.100521 ↗
60. Rajpoot S, Ha JH, Kim YW (2021) Effects of initial particle size on mechanical, thermal, and electrical properties of porous SiC ceramics. Ceram Int 47:8668–8676. https://doi.org/10.1016/j.ceramint.2020.11.23810.1016/j.ceramint.2020.11.238 ↗
61. Kim GD, Kim YW, Song IH, Kim KJ (2020) Effects of carbon and silicon on electrical, thermal, and mechanical properties of porous silicon carbide ceramics. Ceram Int 46:15594–15603. https://doi.org/10.1016/j.ceramint.2020.03.10610.1016/j.ceramint.2020.03.106 ↗
62. Zhang JF, Zhou XN, Zhi Q et al (2020) Microstructure and mechanical properties of porous SiC ceramics by carbothermal reduction and subsequent recrystallization sintering. J Asian Ceram Soc 8:255–264. https://doi.org/10.1080/21870764.2020.172804510.1080/21870764.2020.1728045 ↗
63. Talwar DN, Sherbondy JC (1995) Thermal expansion coefficient of 3 C-SiC. Appl Phys Lett 67:3301–3303. https://doi.org/10.1063/1.11522710.1063/1.115227 ↗
64. Watanabe H, Yamada N, Okaji M (2004) Linear thermal expansion coefficient of silicon from 293 to 1000 K. Int J Thermophys 25:221–236. https://doi.org/10.1023/B:IJOT.0000022336.83719.4310.1023/B:IJOT.0000022336.83719.43 ↗
65. Zhao L, Tang J, Zhou M, Shen K (2022) A review of the coefficient of thermal expansion and thermal conductivity of graphite. New Carbon Mater 37:544–555. https://doi.org/10.1016/S1872-5805(22)60603-610.1016/S1872-5805(22)60603-6 ↗
66. Kim YH, Kim YW, Seo WS (2020) Processing and properties of silica-bonded porous nano-SiC ceramics with extremely low thermal conductivity. J Eur Ceram Soc 40:2623–2633. https://doi.org/10.1016/j.jeurceramsoc.2019.11.07210.1016/j.jeurceramsoc.2019.11.072 ↗
67. Kang ES, Kim YW, Nam WH (2021) Multiple thermal resistance induced extremely low thermal conductivity in porous SiC-SiO2 ceramics with hierarchical porosity. J Eur Ceram Soc 41(2):1171–1180. https://doi.org/10.1016/j.jeurceramsoc.2020.10.00410.1016/j.jeurceramsoc.2020.10.004 ↗
68. Yoshida K, See CC, Gubarevich A, Yano T (2019) Effects of aluminum, boron and carbon additives on microstructure of porous silicon carbide ceramics and their properties. Mater Today Proc 16:65–71. https://doi.org/10.1016/j.matpr.2019.05.30810.1016/j.matpr.2019.05.308 ↗
69. Zhao J, Ban X, Yang Y et al (2023) Fabrication of SiC porous ceramics by foaming method. Materials 16:1342. https://doi.org/10.3390/ma1604134210.3390/ma16041342 ↗
70. Yin Y, Ma B, Hu C et al (2019) Preparation and properties of porous SiC–Al2O3 ceramics using coal ash. Int J Appl Ceram Technol 16:23–31. https://doi.org/10.1111/ijac.1308010.1111/ijac.13080 ↗
71. Yu C, Deng C, Ding J et al (2023) Enhanced mechanical properties of R–SiC honeycomb ceramics with in situ AlN–SiC solid solution. Ceram Int 49:32153–32163. https://doi.org/10.1016/j.ceramint.2023.07.18610.1016/j.ceramint.2023.07.186 ↗
72. Zhong Z, Zhang B, Ye J, Gao Y et al (2022) The thermal, electrical and mechanical properties of porous α-SiC ceramics bonded with Ti3SiC2 and β-SiC via low temperature in-situ reaction sintering. Ceram Int 48:15189–15199. https://doi.org/10.1016/j.ceramint.2022.02.04810.1016/j.ceramint.2022.02.048 ↗
73. Gómez-Martín A, Orihuela MP, Becerra J et al (2016) Permeability and mechanical integrity of porous biomorphic SiC ceramics for application as hot-gas filters. Mater Des 107:450–460. https://doi.org/10.1016/j.matdes.2016.06.06010.1016/j.matdes.2016.06.060 ↗
74. Qian JM, Jin ZH (2006) Preparation and characterization of porous, biomorphic SiC ceramic with hybrid pore structure. J Eur Ceram Soc 26:1311–1316. https://doi.org/10.1016/j.jeurceramsoc.2005.03.22910.1016/j.jeurceramsoc.2005.03.229 ↗
75. Wu H, Li Y, Yan Y et al (2014) Processing, microstructures and mechanical properties of aqueous gelcasted and solid-state-sintered porous SiC ceramics. J Eur Ceram Soc 34:3469–3478. https://doi.org/10.1016/j.jeurceramsoc.2014.05.03110.1016/j.jeurceramsoc.2014.05.031 ↗
76. Eom JH, Kim YW (2008) Effect of template size on microstructure and strength of porous silicon carbide ceramics. J Ceram Soc Jpn 116:1159–1163. https://doi.org/10.2109/jcersj2.116.115910.2109/jcersj2.116.1159 ↗
77. Chun YS, Kim YW (2005) Processing and mechanical properties of porous silica-bonded silicon carbide ceramics. Met Mater Int 11:351–355. https://doi.org/10.1007/BF0302750410.1007/BF03027504 ↗
78. Ge H, Wang G, Yuan B, Dong B, Li H (2014) Fabrication and microstructure of porous SiC ceramics using suspension emulsions as pore-forming agent. Ceram Int 40:11705–11711. https://doi.org/10.1016/j.ceramint.2014.03.18210.1016/j.ceramint.2014.03.182 ↗