journal article·2026-02-01

Effect of annealing temperature on mechanical properties of welds of Ti-6Al-4V titanium alloy

Jiangyun Zheng, Shengjun Peng, Mingjun Zhang, Junzhao Li, Bo Cheng, Yingzhe Zhang, Zhengwei Qi, Jiaying Yan, Guangliang Li, Zihao Qin, Tao Liu

Journal of Laser Applications· Volume 38· Issue 1
Publisher page

Abstract

This study investigates the microstructure and mechanical properties of Ti-6Al-4V welds at different annealing temperatures, aiming to clarify the role of temperature in joining thin-walled titanium alloy pipes for aerospace applications. It is found that (1) with the same annealing temperature, Widmanstätten structures are observed in the welds by laser welding, and no Widmanstätten structure is observed in the welds by TIG welding. (2) The joint performance depends on the average grain size and the dislocation of the weld. When the annealing temperature is set as 650 °C, the tensile strength of the weld by laser is slightly higher (i.e., 0.9%) than that of the weld by TIG, and the microhardness of the weld by laser shows no difference from that of the weld by TIG. The average grain size of the weld by laser is 3.48% higher than that of the weld by TIG. The KAMave of the weld by laser is 14.8% lower than that of the weld by TIG. (3) When the specimens are joined by laser welding and the annealing temperature is increased from 650 to 800 °C, the weld microstructure transforms into a basketweave structure. Both microhardness and tensile strength of the weld are decreased significantly. The average grain size of the weld is increased by 8.73%, and the KAMave of the weld is decreased by 28.3%. In summary, the impact of the annealing temperature on the joint performance of the weld by laser welding is significantly greater than that of the weld by TIG.
Source: crossref · Quality: baseline

Research context

OpenAlex topics: Welding Techniques and Residual Stresses · Titanium Alloys Microstructure and Properties · Advanced Welding Techniques Analysis

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

Hunan Provincial Key Laboratory of Intelligent Manufacturing Technology for High-Performance Mechanical Equipment, Changsha University of Science and Technology 1 , Changsha 410114,

HuNan Xiangtou Goldsky New Materials Co., Ltd. 2 , Yiyang 413000,

School of Mechanical Engineering, Hunan University of Technology 3 , Zhuzhou 412007,

Funding

National Natural Science Foundation of China · Science and Technology Program of Hunan Province · Hunan Provincial Outstanding Youth Science Foundation · Scientific Research Foundation of Hunan Provincial Education Department · Changsha Municipal Natural Science Foundation

References (39)

Show source-provided references
1. A literature review of Ti-6Al-4V linear friction welding10.1016/j.pmatsci.2017.10.003 ↗
2. Grain refinement and anisotropy improvement of arc-directed energy deposited Ti-6Al-4V with oscillating laser10.1016/j.msea.2024.146144 ↗
3. Wear behavior of Ti6Al4V biomedical alloys processed by selective laser melting, hot pressing and conventional casting10.1016/S1003-6326(17)60060-8 ↗
4. Welding materials for TIG welding, surfacing, and WAAM technology of titanium alloys10.1007/s40194-023-01464-z ↗
5. Studies on the weld integrity, formability and microstructural evolution of grade 2 titanium sheets of laser beam welding process10.1088/2053-1591/aafa90 ↗
6. An assessment into mechanical properties and microstructural behavior of TIG welded Ti-6Al-4V titanium alloy10.1108/GS-11-2019-0052 ↗
7. Experimental and numerical assessment of temperature field and analysis of microstructure and mechanical properties of low power laser annealed welded joints10.3390/ma11091514 ↗
8. A comparative study of pulsed Nd:YAG laser welding and TIG welding of thin Ti6Al4V titanium alloy plate10.1016/j.msea.2012.06.016 ↗
9. Microstructure and residual stresses in Ti-6Al-4V alloy pulsed and unpulsed TIG welds10.1016/j.jmatprotec.2016.01.018 ↗
10. Electron beam welding, laser beam welding and gas tungsten arc welding of titanium sheet10.1016/S0921-5093(99)00662-0 ↗
11. Microstructure evolution and mechanical characterization of Nd:YAG laser beam welded titanium tubes10.1016/j.matchar.2017.10.025 ↗
12. Microstructure and mechanical properties of laser welded Ti-22Al-27Nb/TC4 dissimilar alloys10.1016/j.msea.2012.09.057 ↗
13. Effect of cyclic heat treatment on commercially pure titanium part fabricated by electron beam additive manufacturing10.1016/j.jallcom.2019.04.335 ↗
14. Effect of three-stage heat treatment on mechanical properties and micro-deformation mechanism of TC4 titanium alloy welded joint10.1016/j.jmrt.2024.05.060 ↗
15. Heat treatment of Ti6Al4V produced by selective laser melting: Microstructure and mechanical properties10.1016/j.jallcom.2012.07.022 ↗
16. Effect of AC/DC mixed current waveform on surface oxidation, microstructure and mechanical properties of TIG welded TC4 titanium alloy10.1177/02670836241253012 ↗
17. Microstructure and property of TB8 sheets TIG welded seam10.19476/j.ysxb.1004.0609.2019.10.10 ↗
18. Effects of annealing temperature on microstructure and properties of near α titanium alloy sheet10.15980/j.tzzz.Y20240020 ↗
19. Unraveling microstructure characteristics induced mechanical responses in laser welding of titanium alloy subjected to varied inclination angle10.1016/j.optlastec.2024.112091 ↗
20. Influence of heat accumulation on the distribution uniformity of microstructure and mechanical properties of laser additive manufacturing joint of 80 mm thick Ti6Al4V titanium alloy plates10.1016/j.jmatprotec.2022.117774 ↗
21. Grain size and microstructure of TC4 titanium alloy TIG and laser welding joint10.12073/j.hjxb.20211015001 ↗
22. EBSD study of microstructural and textural changes of hot-rolled Ti-6Al-4V sheet after annealing at 800 °C10.1007/s40195-018-0768-7 ↗
23. Influence of the mode of laser welding parameters on microstructural morphology in thin sheet Ti6Al4V alloy10.1016/j.optlastec.2020.106456 ↗
24. Predicting tensile properties of Ti-6Al-4V produced via directed energy deposition10.1016/j.actamat.2017.05.025 ↗
25. Study on microstructure, mechanical and corrosion behavior of Ti-6Al-4V titanium alloy by keyhole gas tungsten arc welding10.1016/j.mtcomm.2024.109530 ↗
26. Microstructure and texture evolution of Ti-6Al-4V alloy T-joint fabricated by dual laser beam bilateral synchronous welding10.1016/j.msea.2021.141426 ↗
27. A comparative study of pulsed laser and pulsed TIG welding of Ti-5Al-2.5Sn titanium alloy sheet10.1016/j.jmatprotec.2016.11.018 ↗
28. Synergistic toughening of welds through adding SiC nanoparticles and modulating oscillating laser10.1016/j.jmrt.2025.01.069 ↗
29. Additive manufacturing of metallic components—process, structure and properties10.1016/j.pmatsci.2017.10.001 ↗
30. Influence of high-temperature annealing on microstructure and properties of welded joints using narrow gap laser welding of TC4 titanium with welding wire10.1007/s11665-023-08629-3 ↗
31. Strength improvement of CoCrNi medium-entropy alloy through introducing lattice defects in refined grains10.1016/j.matchar.2022.112254 ↗
32. Hall–Petch relation and boundary strengthening10.1016/j.scriptamat.2004.06.002 ↗
33. Aifantis, geometrically necessary dislocations and strain gradient plasticity––a dislocation dynamics point of view10.1016/S1359-6462(02)00341-X ↗
34. Multi-regional microstructure control using ultrasonic-assisted directed energy deposition for Al–Cu alloy10.1016/j.jmatprotec.2023.118269 ↗
35. An investigation on the strengthening mechanism based on grain-boundary misorientation of high-strength pipeline steel10.1002/srin.201900317 ↗
36. Deformation behavior and microstructure characteristics of the laser-welded Ti-6Al-4V joint under variable amplitude fatigue10.1016/j.matchar.2022.112606 ↗
37. Effet de l’anisotropie élastique cristalline sur la distribution des facteurs de Schmid à la surface des polycristaux10.1016/j.crme.2006.03.004 ↗
38. Microstructure and mechanical properties of low-carbon high-strength steel fabricated by wire and arc additive manufacturing10.3390/met10020216 ↗
39. Acceleration of grain-boundary diffusion at recrystallization in submicrocrystalline metals produced by the method of equal-channel angular pressing10.1007/s11182-012-9862-x ↗