journal article·2026Open access

Quantitative Investigation of the Creep Resistance of Different SiC Fibers after Annealing at High Temperature

Xue ZHOU, Zhe LIU, Yan REN, Jinshan YU, Tianyue YANG, Zhongqian ZHAO, Honglei WANG, Xingui ZHOU, Yanzi GOU

Journal of Inorganic Materials· Volume 41· Issue 7

Abstract

No abstract is available for this record. The assistant can identify its topic from the title, but cannot infer the study’s results.

Source: Not provided · Quality: missing

Research context

OpenAlex topics: Advanced ceramic materials synthesis · Silicon Carbide Semiconductor Technologies · High-Temperature Coating Behaviors

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (39)

Show source-provided references
1. IVEKOVIĆ A, NOVAK S, DRAŽIĆ G, et al . Current status and prospects of SiC f /SiC for fusion structural applications. Journal of the European Ceramic Society , 2013, 33(10): 1577.10.1016/j.jeurceramsoc.2013.02.013 ↗
2. PADTURE N P. Advanced structural ceramics in aerospace propulsion. Nature Materials , 2016, 15(8): 804.10.1038/nmat4687 ↗
3. WANG P R, LIU F Q, WANG H, et al . A review of third generation SiC fibers and SiC f /SiC composites. Journal of Materials Science & Technology , 2019, 35(12): 2743.10.1016/j.jmst.2019.07.020 ↗
4. KATOH Y, SNEAD L L, HENAGER C H, et al . Current status and recent research achievements in SiC/SiC composites. Journal of Nuclear Materials , 2014, 455(1/2/3): 387.10.1016/j.jnucmat.2014.06.003 ↗
5. SONG J P, JIAO J, LIU H, et al . Effect of surface state of SiC fibers on their interfacial properties. Composites Communications , 2025, 53: 102232.10.1016/j.coco.2024.102232 ↗
6. SANTORO U, NOVITSKAYA E, KARANDIKAR K, et al . Phase stability of SiC/SiC fiber reinforced composites: the effect of processing on the formation of α and β phases. Materials Letters , 2019, 241: 123.10.1016/j.matlet.2019.01.055 ↗
7. SHI X G, LI M Y, MA W G, et al . Experimental study on thermal transport property of KD-Ⅱ SiC fiber. Journal of Inorganic Materials , 2018, 33(7): 756.10.15541/jim20170429 ↗
8. DONG S M, KATOH Y, KOHYAMA A. Processing optimization and mechanical evaluation of hot pressed 2D Tyranno-SA/SiC composites. Journal of the European Ceramic Society , 2003, 23(8): 1223.10.1016/S0955-2219(02)00298-4 ↗
9. BHATT R T, HALBIG M C. Creep properties of melt infiltrated SiC/SiC composites with Sylramic™-iBN and Hi-Nicalon™-S fibers. International Journal of Applied Ceramic Technology , 2022, 19(2): 1074.10.1111/ijac.13996 ↗
10. HUGUET-GARCIA J, JANKOWIAK A, MIRO S, et al . In situ characterization of ion-irradiation enhanced creep of third generation Tyranno SA 3 SiC fibers. Journal of Materials Research , 2015, 30(9): 1572.10.1557/jmr.2014.412 ↗
11. HOLMES J W, PARK Y H, JONES J W. Tensile creep and creep- recovery behavior of a SiC-fiber-Si 3 N 4 -matrix composite. Journal of the American Ceramic Society , 1993, 76(5): 1281.10.1111/j.1151-2916.1993.tb03753.x ↗
12. LAMOUROUX F, VALLÉS J L, STEEN M. Uniaxial tensile and creep behaviour of an alumina fibre-reinforced ceramic matrix composite: Ⅱ. Modelling of tertiary creep. Journal of the European Ceramic Society , 1994, 14(6): 539.10.1016/0955-2219(94)90125-2 ↗
13. ALMANSOUR A S, MORSCHER G N. Tensile creep behavior of SiC f /SiC ceramic matrix minicomposites. Journal of the European Ceramic Society , 2020, 40(15): 5132.10.1016/j.jeurceramsoc.2020.07.012 ↗
14. YAJIMA S, OKAMURA K, HAYASHI J, et al . Synthesis of continuous sic fibers with high tensile strength. Journal of the American Ceramic Society , 1976, 59(7/8): 324.10.1111/j.1151-2916.1976.tb10975.x ↗
15. BODET R, LAMON J, JIA N Y, et al . Microstructural stability and creep behavior of Si-C-O (nicalon) fibers in carbon monoxide and argon environments. Journal of the American Ceramic Society , 1996, 79(10): 2673.10.1111/j.1151-2916.1996.tb09033.x ↗
16. VAHLAS C, MONTHIOUX M. On the thermal degradation of lox-M tyranno® fibres. Journal of the European Ceramic Society , 1995, 15(5): 445.10.1016/0955-2219(95)00004-E ↗
17. WILSON M, OPILA E. A review of SiC fiber oxidation with a new study of Hi-Nicalon SiC fiber oxidation. Advanced Engineering Materials , 2016, 18(10): 1698.10.1002/adem.201600166 ↗
18. YOUNGBLOOD G E, LEWINSOHN C, JONES R H, et al . Tensile strength and fracture surface characterization of Hi-Nicalon™ SiC fibers. Journal of Nuclear Materials , 2001, 289(1/2): 1.10.1016/S0022-3115(00)00675-9 ↗
19. TAKEDA M, SAEKI A, SAKAMOTO J I, et al . Effect of hydrogen atmosphere on pyrolysis of cured polycarbosilane fibers. Journal of the American Ceramic Society , 2000, 83(5): 1063.10.1111/j.1151-2916.2000.tb01331.x ↗
20. TAKEDA M, SAKAMOTO J, IMAI Y, et al . Properties of stoichiometric silicon carbide fiber derived from polycarbosilane// WACHTMAN J B. Proceedings of the 18th annual conference on composites and advanced ceramic materials—A:ceramic engineering and science proceedings. Hoboken: John Wiley & Sons, Inc., 1994.
21. BUNSELL A R, PIANT A. A review of the development of three generations of small diameter silicon carbide fibres. Journal of Materials Science , 2006, 41(3): 823.10.1007/s10853-006-6566-z ↗
22. ISHIKAWA T, KOHTOKU Y, KUMAGAWA K, et al . High-strength alkali-resistant sintered SiC fibre stable to 2200 ℃. Nature , 1998, 391(6669): 773.10.1038/35820 ↗
23. GOU Y Z, WANG H, JIAN K, et al . Preparation and characterization of SiC fibers with diverse electrical resistivity through pyrolysis under reactive atmospheres. Journal of the European Ceramic Society , 2017, 37(2): 517.10.1016/j.jeurceramsoc.2016.09.023 ↗
24. MORSCHER G N, DICARLO J A. A simple test for thermomechanical evaluation of ceramic fibers. Journal of the American Ceramic Society , 1992, 75(1): 136.10.1111/j.1151-2916.1992.tb05455.x ↗
25. SHA J J, PARK J S, HINOKI T, et al . Heat treatment effects on creep behavior of polycrystalline SiC fibers. Materials Characterization , 2006, 57(1): 6.10.1016/j.matchar.2005.11.019 ↗
26. SHA J J, PARK J S, HINOKI T, et al . Bend stress relaxation of advanced SiC-based fibers and its prediction to tensile creep. Mechanics of Materials , 2007, 39(2): 175.10.1016/j.mechmat.2006.04.001 ↗
27. GAN Y. The regulation of microscopic composition and microstructure of KD-S silicon carbide fibers and the research on these high-temperature creep resistance. Changsha: A Master’s dissertation in National University of Defense Technology, 2018.
28. SHA J J, NOZAWA T, PARK J S, et al . Effect of heat treatment on the tensile strength and creep resistance of advanced SiC fibers. Journal of Nuclear Materials , 2004, 329: 592.10.1016/j.jnucmat.2004.04.123 ↗
29. YUAN W, HU J B, ZHOU L, et al . Effect of argon atmosphere heat treatment on mechanical properties and microstructural evolution of Shicolon-II SiC fibers. Journal of Inorganic Materials , 2026, 41(1): 119.10.15541/jim20250052 ↗
30. GOU Y Z, JIAN K, WANG H, et al . Fabrication of nearly stoichiometric polycrystalline SiC fibers with excellent high-temperature stability up to 1900 ℃. Journal of the American Ceramic Society , 2018, 101(5): 2050.10.1111/jace.15366 ↗
31. WU S, GOU Y Z, XIANG Y, et al . Effect of long-time annealing at high temperature on the microstructure and mechanical properties of different types of SiC fibers. Composites Part A: Applied Science and Manufacturing , 2024, 185: 108291.10.1016/j.compositesa.2024.108291 ↗
32. ZHANG Y, CHEN T X, CHEN J H, et al . The effects of annealing atmosphere and intrinsic component on high temperature evolution behaviors of SiC fibers. Materials Science and Engineering: A , 2022, 848: 143363.10.1016/j.msea.2022.143363 ↗
33. WU S, GOU Y Z, WANG Y S, et al . Effect of heat treatment on composition, microstructure and mechanical property of domestic KD-SA SiC fibers. Journal of Inorganic Materials , 2023, 38(5): 569.10.15541/jim20220548 ↗
34. ICHIKAWA H. Polymer-derived ceramic fibers. Annual Review of Materials Research , 2016, 46: 335.10.1146/annurev-matsci-070115-032127 ↗
35. SHA J J, HINOKI T, KOHYAMA A. Microstructural characterization and fracture properties of SiC-based fibers annealed at elevated temperatures. Journal of Materials Science , 2007, 42(13): 5046.10.1007/s10853-006-0579-5 ↗
36. USUKAWA R, ISHIKAWA T. Effect of Al contained in polymer- derived SiC crystals on creating stable crystal grain boundaries. International Journal of Applied Ceramic Technology , 2021, 18(1): 6.10.1111/ijac.13627 ↗
37. ZHANG Y, WU C L, WANG Y D, et al . A detailed study of the microstructure and thermal stability of typical SiC fibers. Materials Characterization , 2018, 146: 91.10.1016/j.matchar.2018.09.041 ↗
38. ZHANG Y, CHEN J H, YAN D X, et al . Conversion of silicon carbide fibers to continuous graphene fibers by vacuum annealing. Carbon , 2021, 182: 435.10.1016/j.carbon.2021.06.043 ↗
39. CHEN J, ZHAO Z Q, WU S, et al . Relationship of defects and mechanical performance of high-crystalline SiC fibers after ultra-high-temperature annealing. Journal of the American Ceramic Society , 2025, 108(12): e20540.10.1111/jace.20540 ↗