Abstract

The methods of atom-force microscopy and measurement of the nanohardness, elasticity modulus, cohesion forces, and friction coefficient with scratch testing (the scratching method) are applied to study the Al2O3 oxide coatings produced by magnetron deposition on Al targets. The morphologies of the coatings are compared when they are produced by the reactive synthesis and magnetron target sputtering and application of oxygen ions in high-frequency plasma. The accomplished study of the tribological and mechanical characteristics demonstrates that the resulting coatings possess stronger hardness and elasticity modulus. Application of the oxide coatings reduces the friction coefficient considerably compared with the substrate; the scratch test reveals higher strength and better adhesion to the substrate. Comparative analysis shows that the Al2O3 coatings applied to the nanostructural TiN film are 1.5 times harder than the coatings deposited on steel.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Metal and Thin Film Mechanics · Diamond and Carbon-based Materials Research · Ion-surface interactions and analysis

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (21)

Show source-provided references
1. Zhang, S., Sun, D., Fu, Y., and Du, H., Recent Advances of Superhard Nanocomposite Coatings: AReview, Surf. Coat. Techn., 2003, vol. 167, nos. 2–3, pp. 113–119.10.1016/S0257-8972(02)00903-9 ↗
2. Arnold, S.M. and Cole, B.E., Ion Beam Sputter Deposition of Low Loss Al2O3 Films for Integrated Optics, Thin Solid Films, 1988, vol. 165, no. 1, pp. 1–9.10.1016/0040-6090(88)90673-6 ↗
3. Teslenko-Ponomarenko, V.V., The Research of Microtopography of Surfaces of Al2O3 Films Obtained by the Method of Magnetron Sputtering under Low Pressures, Vopr. At. Nauki Tekhn., Vacuum, Pure Mater., Supercond., 2003, no. 5, pp. 175–178.
4. Messier, R., and Trolier-McKinstry, S., Thin-Film Processes, in Encyclopedia of Materials: Science and Technology, 2nd ed., Pergamon, 2001, pp. 9306–9313.10.1016/B0-08-043152-6/01678-8 ↗
5. Berg, S. and Nyberg, T., Fundamental Understanding and Modeling of Reactive Sputtering Processes, Thin Solid Films, 2005, vol. 476, pp. 215–230.10.1016/j.tsf.2004.10.051 ↗
6. Pogrebnyak, A.D., Tyurin, Yu.N., Ivanov, Yu.F., et al., Preparation and Investigation of the Structure and Properties of Al2O3 Plasma-Detonation Coatings, Techn. Phys. Lett., 2000, vol. 26, no. 11, pp. 960–963.10.1134/1.1329684 ↗
7. Pogrebnjak, A.D., Il’jashenko, M.V., Kul’ment’eva, O.P., et al., Structure and Properties of Al2O3 and Al2O3 + Cr2O3 Coatings Deposited to Steel 3 (0.3 wt % C) Substrate, Using Pulsed Detonation Technology, Vacuum, 2001, vol. 62, no. 1, pp. 21–26.10.1016/S0042-207X(01)00109-9 ↗
8. Portinha, A., Teixeira, V., and Carneiro, J., Mechanical Properties of ZrO2-Al2O3 Nanostructured PVD Coatings Evaluated by Nanoindentation, Rev. Adv. Mater. Sci., 2003, vol. 5, pp. 311–318.
9. Farenik, V.I., Low-Energy Devices of Ion-Plasma Technologies, Tr. nauch.-tekhn. konf. s mezhd. uchastiem “Komp’yuternoe modelirovanie v naukoemkikh tekhnologiyakh” (Proc. Sci.-Techn. Conf. Int. Part. ‘Computer Modeling in Science Intensive Technologies’ CMST-2010), Kharkov: Khar. Nat. Univ., 2010.
10. Koski, K., Hölsä, J., and Juliet, P., Properties of Aluminum Oxide Thin Films Deposited by Reactive Magnetron Sputtering, Thin Solid Films, 1999, vol. 339, nos. 1–2, pp. 240–248.10.1016/S0040-6090(98)01232-2 ↗
11. Raveh, A., Tsameret, Z.K., and Grossman, E., Surface Characterization of Thin Layers of Aluminum Oxide, Surf. Coat. Techn., 1997, vol. 88, nos. 1–3, pp. 103–111.10.1016/S0257-8972(95)02757-2 ↗
12. Oliver, W.C. and Pharr, G.M., An Improved Technique for Determining Hardness and Elastic Modulus Using Load and Displacement Sensing Indentation Experiments, J. Mater. Res., 1992, vol. 6, pp. 1564–1583.10.1557/JMR.1992.1564 ↗
13. Pogrebnyak, A.D., Kravchenko, Yu.A., Alontseva, D.L., et al., Structure and Properties of Powder Coatings Applied by a High-Velocity Plasma Jet, J. Friction Wear, 2005, vol. 26, no. 5, pp. 52–60.
14. Musil, J., Kunc, F., Zeman, H., and Polakova, H., Relationships between Hardness, Young’s Modulus and Elastic Recovery in Hard Nanocomposite Coatings, Surf. Coat. Techn., 2002, vol. 154, nos. 2–3, pp. 304–313.10.1016/S0257-8972(01)01714-5 ↗
15. Firstov, S.A. and Rogul’, T.G., Theoretical (Ultimate) Strength, Rep. Nat. Acad. Sci. Ukraine, 2007, no. 4, pp. 110–114.
16. Gorban’, V.F., Mameka, N.A., Pechkovskii, E.P., and Firstov, S.A., Identification of Material Structural State by Automatic Identification Method, in Sb. dokl. Khar’kovskoi nanotekhnologicheskoi assamblei (Coll. Papers Kharkov Nanotechn. Assembly), Kharkov, 2006, vol. 1, pp. 52–55.
17. Shtanskii, D.V., Kulinich, S.A., Levashov, E.A., and Moore, J.J., Structure and Physical-Mechanical Properties of Nanostructured Thin Films, Phys. Solid State, 2003, vol. 45, no. 6, pp. 1177–1184.10.1134/1.1583811 ↗
18. Shautsukov, A.G., Contemporary Presentation about Possible Mechanisms of Adhesion of Metal Films to Different Substrates, Prikladnaya Fizika, 2006, no. 5, pp. 16–21.
19. Lavrentiev, I.V. and Pogrebnyak, A.D., Effect of Ion Beam on Iron and Steel, Met. Phys. Adv. Techn., 1997, vol. 16, no. 11, pp. 1233–1265.
20. Carvalho, S., Ribeiro, E., Rebouta, L., et al., Microstructure, Mechanical Properties and Cutting Performance of Superhard (Ti, Si, Al)N Nanocomposite Films Grown by D.C. Reactive Magnetron Sputtering, Surf. Coat. Techn., 2004, vol. 177–178, pp. 459–468.10.1016/j.surfcoat.2003.08.056 ↗
21. Pogrebnyak, A.D., Shpak, A.P., Azarenkov, N.A., et al., Structure and Properties of Hard and Superhard Nanocomposite Coatings, Phys.-Usp., 2009, vol. 52, no. 1, pp. 29–54.10.3367/UFNe.0179.200901b.0035 ↗