Abstract
Dielectric, conductivity and piezoelectric properties have been studied on ((hbox {Ba}0.997hbox {Nd}0.003)hbox {TiO}3) ceramic samples prepared through microwave sintered (MWS) and conventional sintered (CS) routes and the results are presented in this paper. The room temperature dielectric constant at 10 kHz for CS and MWS samples are 1245 and 5250 respectively. Room temperature dielectric constant in MWS sample was almost four times higher than that of the CS sample. The value of (K_{mathrm{t}}) is found to be 0.998 and 0.997; whereas the value of (d33) is (7.72 hbox { nm V}-1) (573 K) and (444.66 hbox { nm V}-1) (573 K) for CS and MWS samples, respectively. In the present study almost 57 times enhancement in piezoelectric charge constant ((d33)) is observed for the MWS (hbox {Ba}0.997hbox {Nd}0.003hbox {TiO}3) ceramic when compared to the CS ceramic.
Source: expertdata · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Ferroelectric and Piezoelectric Materials · Microwave Dielectric Ceramics Synthesis · Acoustic Wave Resonator Technologies
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (16)
Show source-provided references
1. Syed M, Dutta A B, Swaminathan G, Prasad G and Kumar G S 2005 Ferroelectrics 326 7910.1080/00150190500318354 ↗
2. Syed M, Dutta A B, Chandra Prakash, Swaminathan G, Suryanarayana S V, Prasad G et al 2006 Mater. Sci. Eng. B 134 3610.1016/j.mseb.2006.06.050 ↗
3. Horng-Yi C, Syh-Yuh C and Ching-Iuan S 2008 Mater. Lett. 62 362010.1016/j.matlet.2008.04.051 ↗
4. Ying-Chieh L, Yu-Yuan Y and Pei-Rong T 2012 J. Eur. Ceram. Soc. 32 172510.1016/j.jeurceramsoc.2011.12.025 ↗
5. Raghavendra Reddy V, Upadhyay S K, Gupta A, Awasthi Anand M and Hussain S 2014 Ceram. Int. 40 833310.1016/j.ceramint.2014.01.039 ↗
6. Mohammad Reza B, Raziyeh Gharah K and Jae-Shin L 2015 Mater. Chem. Phys. 156 25410.1016/j.matchemphys.2015.03.018 ↗
7. Kumar P, Singh S, Juneja J K, Chandra P and Raina K K 2015 Mater. Lett. 142 8410.1016/j.matlet.2014.11.070 ↗
8. Bindra N S, Kaur D and Kunal P 2015 Ferroelectrics 486 7410.1080/00150193.2015.1100033 ↗
9. Syed M, Rizwana Prasad G and Kumar G S 2015 Ferroelectrics 486 17510.1080/00150193.2015.1100922 ↗
10. Gonçalves Mayra D, Souza Flavio L, Elson Longo, Leite Edson R and Camargo Emerson R 2016 Ceram. Int. 42 1442310.1016/j.ceramint.2016.06.035 ↗
11. Yongping P, Zhang L, Mouteng Y, Wanyin G and Min C 2017 Mater. Lett. 189 23210.1016/j.matlet.2016.12.020 ↗
12. Rani R, Kumar P, Singh S, Juneja J K and Chandra P 2017 J. Alloys Compd. 690 71610.1016/j.jallcom.2016.08.119 ↗
13. Syed M, Rizwana Prasad G and Kumar G S 2017 Ferroelectrics 506 6310.1080/00150193.2017.1282252 ↗
14. Sinclair D C and West A R 1989 Phys. Rev. B 39 1348610.1103/PhysRevB.39.13486 ↗
15. Sinclair D C and West A R 1989 J. Appl. Phys. 56 385010.1063/1.344049 ↗
16. ANSI/IEEE Standards on Piezoelectricity 1987 176 51