Abstract

In the present investigation, stellite-6, Cr3C2-NiCr and WC-Co-Cr coatings were deposited by D-Gun on a hot rolled 21Cr-4Ni-N steel meant for fabrication of hydro turbine underwater parts. The coatings have been characterized for microstructure, porosity, microhardness and crystalline nature. The erosion experiments were carried out using an air jet erosion test rig at a velocity of 120 ms−1 and impingement angles of 30° and 90°. Silicon carbide particles of size ranging between 500 and 700 μm were used as erodent. Scanning electron microscopy (SEM) technique was used to analyse the nature and mechanism of erosion. Erosion behaviour is observed to be influenced largely by the nature and extent of porosity in the surface coatings.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Erosion and Abrasive Machining · High-Temperature Coating Behaviors · Particle Dynamics in Fluid Flows

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (25)

Show source-provided references
1. Barbezat G, Nicoll A and Sickinger A 1993 Wear 162–164 52910.1016/0043-1648(93)90538-W ↗
2. Chauhan A K, Goel D B and Prakash S 2009 J. Alloys Compd 459–464 467
3. Fagoaga I, Viviente J L and Gavin P 1998 J. Thin Solid Films 317 25910.1016/S0040-6090(97)00524-5 ↗
4. Guo D Z, Li F L, Wang J Y and Sun J S 1995 Surf. Coat. Technol. 73 7310.1016/0257-8972(94)02364-6 ↗
5. Hearley J A, Little J A and Sturgeon A J 1999 Wear 233–235 32810.1016/S0043-1648(99)00240-9 ↗
6. Herman H and Sampath S 1996 in Metallurgical and ceramic protective coatings (ed.) K H Stern (London, UK: Chapman and Hall) p. 26110.1007/978-94-009-1501-5_10 ↗
7. Ji G C, Li C J, Wang Y Y and Li W Y 2006 Surf. Coat. Technol. 200 674910.1016/j.surfcoat.2005.10.005 ↗
8. Kosel T H 1992 ASM Handbook 18 199
9. Levy A V 1988 Surf. Coat. Technol. 36 38710.1016/0257-8972(88)90168-5 ↗
10. Mishra S B, Prakash S and Chandra K 2006 Wear 260 42210.1016/j.wear.2005.02.098 ↗
11. Murthy J K N, Rao D S and Venkataraman B 2001 Wear 249 59210.1016/S0043-1648(01)00682-2 ↗
12. Sahraoui T, Fenineche N, Montavon G and Coddet C 2003 Mater. Design 24 30910.1016/S0261-3069(03)00059-1 ↗
13. Semenov S Y and Cetegen B M 2002 Mater. Sci. Eng. A335 6710.1016/S0921-5093(01)01948-7 ↗
14. Shipway P H and Hutchings I M 1994 Wear 174 16910.1016/0043-1648(94)90099-X ↗
15. Shipway P H and Hutchings I M 1995 Surf. Coat. Technol. 71 110.1016/0257-8972(94)02314-G ↗
16. Sidhu H S, Sidhu B S and Prakash S 2007 Surf. Coat. Technol. 202 23210.1016/j.surfcoat.2007.05.035 ↗
17. Singh H, Puri D and Prakash S 2005 Anti-Corros. Meth. Mater. 52 8410.1108/00035590510584799 ↗
18. Takeda K, Ito M, Takeuchi S, Sudo K, Koga M and Kazama K 1993 ISIJ Int. 33 97610.2355/isijinternational.33.976 ↗
19. Wang B and Lee S W 2000 Wear 239 8310.1016/S0043-1648(00)00309-4 ↗
20. Wang J, Zhang L, Sun B and Zhou Y 2000 Surf. Coat. Technol. 130 6910.1016/S0257-8972(00)00677-0 ↗
21. Wang Y 1993 Wear 161 6910.1016/0043-1648(93)90454-T ↗
22. Wood R J K and Wheeler D W 1999 Wear 220 9510.1016/S0043-1648(98)00196-3 ↗
23. Zhang K 2003 Wear 255 54510.1016/S0043-1648(03)00050-4 ↗
24. Zhang P, Jiang J, Ma A, Wang Z, Wu Y and Lin P 2007 Adv. Mater. Res. 15–17 199
25. Zhao L, Zwick J and Lugscheider E 2004 Surf. Coat. Technol. 182 7210.1016/S0257-8972(03)00874-0 ↗