Studies of the Action of Silicone at the Interphase on the Flame Retardant System of EBA Copolymer-chalk
Source abstract
Abstract
Mechanistic study on the system has been performed with the aid of XPS in combination with other appraisal techniques, like TGA/LOI/CONE. It follows that remarkable enhancement of silicon-containing species at the surface region in the course of the combustion appear to play the crucial role for the protective barrier.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Flame retardant materials and properties · Polymer Nanocomposites and Properties · Silicone and Siloxane Chemistry
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
School of Materials and Textile Wuhan University of Science and Engineering College of Textile & Materials, No. 1 Luxiang Textile Road, Hongshan District 430073 Wu Han, Hu Bei Province, China
National Laboratory of Flame Retardant Materials, School of Materials Science & Engineering, Beijing Institute of Technology, Zhongguancun Road Haidian District, 100081 Beijing, China,
References (30)
Show source-provided references
1. 10.1002/app.1051010.1002/app.10510 ↗
2. 10.1002/fam.81710.1002/fam.817 ↗
3. 10.1016/S0141-3910(02)00385-310.1016/S0141-3910(02)00385-3 ↗
4. 10.1002/fam.91010.1002/fam.910 ↗
5. 10.1177/095400830504382210.1177/0954008305043822 ↗
6. Hermansson, A. · Chalk and Silicone Elastomer and its Effect on Flame Retardant Properties, Journal of Applied Polymer Science · 2006 · 100 · 2085
7. Kräer, R.H. · Polymer Degradation and Stability · 2007 · 92 · 189910.1016/j.polymdegradstab.2007.06.014 ↗
8. 10.1177/073490410706811610.1177/0734904107068116 ↗
9. Thermo Avantage 3.22, Software for Surface Chemical Analysis, VG MultiLab · 2000
10. Wang, J. · Degrad. Stab. · 2002 · 77 · 24910.1016/S0141-3910(02)00055-1 ↗
11. 10.1016/0032-3861(75)90157-310.1016/0032-3861(75)90157-3 ↗
12. Kashiwagi, T. and Gilman, J.W. (2000). Fire Retardancy of Polymeric Materials, In: Grand, A.F. and Wilkie, C.A. (eds), Silicon-based Flame Retardants, Ch. 10, pp. 285-324, Marcel Dekker, Inc.
13. 10.1016/j.polymdegradstab.2005.07.02110.1016/j.polymdegradstab.2005.07.021 ↗
14. Wang, J. · National Defence Publishing House · 1992 · 524
15. 10.1016/S0141-3910(98)00106-210.1016/S0141-3910(98)00106-2 ↗
16. 10.1016/S0141-3910(00)00180-410.1016/S0141-3910(00)00180-4 ↗
17. 10.1016/S0141-3910(01)00164-110.1016/S0141-3910(01)00164-1 ↗
18. 10.1016/S0141-3910(02)00055-110.1016/S0141-3910(02)00055-1 ↗
19. 10.1016/S0141-3910(02)00074-510.1016/S0141-3910(02)00074-5 ↗
20. 10.1016/S0141-3910(02)00295-110.1016/S0141-3910(02)00295-1 ↗
21. 10.1016/S0141-3910(03)00198-810.1016/S0141-3910(03)00198-8 ↗
22. 10.1016/j.polymdegradstab.2006.03.02310.1016/j.polymdegradstab.2006.03.023 ↗
23. 23. Huang, N., Zhang, Q., Li, Z. and Wang, J. to be submitted.
24. 10.1016/S0141-3910(01)00098-210.1016/S0141-3910(01)00098-2 ↗
25. 10.1002/pen.76033200810.1002/pen.760332008 ↗
26. 10.1016/0141-3910(95)00146-810.1016/0141-3910(95)00146-8 ↗
27. Wagner, C.D. · 1979
28. 10.1016/S0141-3910(03)00261-110.1016/S0141-3910(03)00261-1 ↗
29. Kashiwagi, T. · 2005
30. Wang, J. and Huang, N. to be submitted.