Abstract
Mechanical properties and water resistance of Pulp/PLA high performance paper for heat molding were investigated in this paper. Especially, the properties of high performance papers before and after heating processes were examined. It is cleared here that the tensile strength can be obtained in the case of 20% content of PLA at heating time 30 min. and temperature 200 ̊C. And the water absorptiveness of presented paper decreases largely after heating process. The strength of paper under the wet condition decreases gradually with the increase of water. However it was shown that the strength was improved by mixing of PLA.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Injection Molding Process and Properties · Additive Manufacturing and 3D Printing Technologies · Manufacturing Process and Optimization
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
Department of Environmental Engineering, Hohhot Minzu College
Kyoto Institute of Technology
References (18)
Show source-provided references
1. [1] X. Xu, E. Sachs and S. Allen, Polymer Engineering and Science, 4(7), 1265(2001).10.1002/pen.10827 ↗
2. [2] T. Matsumori, K. Yamazaki and S. Kitayama, Seikei-kakou, 21(11), 699(2009).10.4325/seikeikakou.21.699 ↗
3. [3] Y. Lam, L. Zhai, K. Tai and S. C. Fok, Journal of Production Research, 42(10), 2047(2004).10.1080/00207540310001622412 ↗
4. [4] A. Takafuji, K. Tamura and A. Yokoyama, Seikeikakou, 15(5), 357(2009).10.4325/seikeikakou.15.357 ↗
5. [5] B. Wendel, D. Rietzel, F. Kühnlein, R. Feulner, G. Hülder and E. Schmachtenberg, Additive Processing of Polymers. MacromolMater Eng. 293 (10), 799(2008).10.1002/mame.200800121 ↗
6. [6] X. Xu, E. Sachs and S. Allen, Polymer Engineering and Science, 4(7), 1265(2001).10.1002/pen.10827 ↗
7. [7] S. N. Ong, Y. H. Koh, Materials and Manufacturing Processes, 20(2), 245(2005).10.1081/AMP-200042004 ↗
8. [8] O. Amano, Plastics, 50(8), 81(1999).
9. [9] M. Tadayoshi, Y. Koetsu, K. Satoshi, Seikei-Kakou, 21(11), 699(2009).10.4325/seikeikakou.21.699 ↗
10. [10] K. Kodama, K. Fujiwara, K. Yamashita, C. Nonomura and A. Yokoyama, Seikei-Kakou, 22(6),312(2010).10.4325/seikeikakou.22.312 ↗
11. [11] Y. Murata, T. Hishida, T. Komatsu, K. Nitta, K. Saitoh and K. Kikumori, Seikei-Kakou, 25(6), 283 (2013).10.4325/seikeikakou.25.283 ↗
12. [12] M. Muraki, K. Fijimura, S. Kataoka, S. Takeuchi and N. Terayama, Journal of the Japan Society of Mechanical Engineers, 76(764), 960(2010).10.1299/kikaic.76.960 ↗
13. [13] A. Nishiguchi, Journal of the Japan Society Tribologists, 54(1), 28(2009).
14. [14] X. Xu, E. Sachs and S. Allen, Polymer Engineering and Science, 4(7), 1265(2001).10.1002/pen.10827 ↗
15. [15] K. Yamashita, C. Nonomura, T.Yamada, Seikei-Kakou,13(6),400(2001).10.4325/seikeikakou.13.400 ↗
16. [18] H. Si, K. Teruo, The Society of Fiber Science and Technology, 73(12), 355(2017).10.2115/fiberst.2017-0047 ↗
17. [20] M. Zhang, C. N. Cui, J. T. Hang, Plastics, 38(4), 85(2009).
18. [21] T. Emae, Y. Mori, O.Isogai, Water absorption and water repellency evaluation of paper by micro size (2009).