Improved interfacial bonding of PVC/wood-flour composites by lignin amine modification
Source abstract
Abstract
An activation process involving chitosan was conducted to prepare electroless nickel plated wood veneers for electromagnetic interference (EMI) shielding. In this process Pd(Ⅱ) ions were ed on wood surface modified with chitosan. Then they were reduced and dipped into a plating bath in which Ni-P co-deposition was successfully initiated. The coatings were characterized by SEM-EDS and XRD. The metal deposition, surface , and electromagnetic shielding effectiveness were measured. The morphology of the coating observed by SEM was uniform, compact, and continuous. EDS results showed that the coating consists of 1.8 wt.% phosphorus and 98.2 wt.% nickel. XRD analysis indicated that the coating was crystalline, which is supposed to be related to the low phosphorus content. The plated birch veneers exhibited electro-conductivity with surface resistivity of 0.24 Ω·cm-2 and good electromagnetic shielding effectiveness of over 50 dB in frequency range from10 MHz to 1.5 GHz.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Electromagnetic wave absorption materials
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
Northeast Forestry University
References
Reference metadata was not supplied for this record.