Strength distribution superiority of compact-Siro spun yarn
Source abstract
Abstract
This study examined the superiority of the strength of compact-Siro spun yarn. First, the strength properties of four types of yarn—ring, compact, Siro, and compact-Siro spun yarn—were compared based on an experiment with 9.7 tex and 14.6 tex polyester yarns. Yarn unevenness and compactness were analyzed in terms of their influence on yarn strength. It was determined that compact spinning enhanced the strength distribution by improving the overall yarn compactness. Siro spinning significantly increased the minimum yarn strength by reducing unevenness. Furthermore, compact-Siro spun yarn, which incorporates the advantages of both compact and Siro, remarkably improved the yarn strength distribution. These results were verified in the first part of the experiment. Finally, the four types of yarn were applied in the same weaving process. The results indicated that the efficiency of weaving with compact-Siro pure polyester yarn was higher than that of other methods by 3%–6%, thereby confirming the superior productivity of the method.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Textile materials and evaluations · Dyeing and Modifying Textile Fibers · Silk-based biomaterials and applications
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
Key Laboratory of Eco-textiles, Ministry of Education, Jiangnan University, Wuxi, China
Jiangsai Textile Technology Co., Ltd, Suzhou, China
School of Textile and Clothing, Jiangnan University, Wuxi, China
Funding
the Enterprise University Research Prospective Program of Jiangsu Province · the National Key R&D Program of China
References (23)
Show source-provided references
1. 10.1080/00405000.2013.83457510.1080/00405000.2013.834575 ↗
2. 10.1007/s12221-014-1752-010.1007/s12221-014-1752-0 ↗
3. Chellamani KP · Indian J Fibre Text · 2004 · 29 · 12
4. 10.1007/BF0287727510.1007/BF02877275 ↗
5. 10.1177/00405175020720030610.1177/004051750207200306 ↗
6. 10.1177/00405175660360110310.1177/004051756603601103 ↗
7. 10.1007/s12221-012-0231-810.1007/s12221-012-0231-8 ↗
8. 10.1177/00405175870570080210.1177/004051758705700802 ↗
9. 10.1177/00405175540240011410.1177/004051755402400114 ↗
10. Rengasamy RS · Indian J Fibre Text · 2005 · 30 · 283
11. 10.5604/12303666.115244710.5604/12303666.1152447 ↗
12. 10.2478/v10304-012-0009-510.2478/v10304-012-0009-5 ↗
13. 10.1177/00405175030730041210.1177/004051750307300412 ↗
14. Nikolic M · Fibres Text East Eur · 2003 · 43 · 30
15. Xu BJ · Fibres Text East Eur · 2010 · 78 · 24
16. 10.1177/00405175980680070910.1177/004051759806800709 ↗
17. 10.1080/00405000.2011.59556710.1080/00405000.2011.595567 ↗
18. 10.1080/00405000.2011.62811710.1080/00405000.2011.628117 ↗
19. 10.1177/00405175020720021210.1177/004051750207200212 ↗
20. 10.1177/004051750606559110.1177/0040517506065591 ↗
21. 10.1007/s12221-012-0110-310.1007/s12221-012-0110-3 ↗
22. GB/ T3916-2013. Measurements on breaking strength and elongation of textiles—curl yarn and single yarn.
23. 10.1177/00405175920620060610.1177/004051759206200606 ↗