journal article·2019-01Open access

The deterioration of Apuan white marble in contemporary architectural context

Francesca Gherardi, Chrysi Kapridaki, Marco Roveri, Davide Gulotta, Pagona Noni Maravelaki, Lucia Toniolo

Abstract

Assessment of the state of conservation of the marble slabs of the Oslo Opera House and investigation of the causes of their discoloration;.• Ongoing phenomenon of calcite grains detachment, with inter- and intra-granular corrosion, due to the atmospheric conditions to which the marble slabs are exposed;.• Presence of siloxanes and oxidized by-products of a mixture of treatments identified by micro-FTIR spectroscopy;.• No migration phenomena from the cementitious bedding mortars used for cladding towards the surface. © 2018 Elsevier Masson SAS The conservation of contemporary buildings is particularly challenging as only few information about their degradation and guidelines for their maintenance are available and at the same time, despite their architectural importance, the attention and caring procedures are nοt adequate to safeguard standards. The Oslo Opera House is a high-standing contemporary architecture (opening 2008) characterized by a large ornamental pavement mainly made of Apuan marble slabs. After a few years, large parts of the marble surface suffered from a marked yellow discoloration and dirt accumulation. In this context, the current research was carried out aiming at assessing the state of conservation of the marble slabs and investigating the causes of their discoloration, to suggest possible remediation and adequate maintenance procedures. Due to the extreme microclimatic conditions, a severe inter- and intra-granular decohesion of the calcite grains can be observed by microscopic analyses, while a surface corrosion phenomenon of the crystals is in progress. The chemical analyses of surface stone material from the slabs allow the detection of deteriorated organic by-products, as a result of the degradation of previous protective treatments, excluding the correlation of iron ions concentration with the discoloration. The state of conservation gathered so far was the starting point for the development of a tailor-made cleaning methodology of the marble cladding and a complete revision of the protective treatments and ordinary maintenance protocol.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Building materials and conservation · Conservation Techniques and Studies · Cultural Heritage Materials Analysis

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (25)

Show source-provided references
1. Sousa Camposinhos · 2014 · 1
2. Service life prediction models for exterior stone cladding10.1080/09613218.2011.617095 ↗
3. Functional and physical service life of natural stone claddings10.1061/(ASCE)MT.1943-5533.0001663 ↗
4. Stones in monuments: natural and anthropogenic deterioration of marble artifacts10.1127/ejm/7/4/0735 ↗
5. Siegesmund · 2011
6. Conservation of stony materials in the built environment10.1007/s10311-015-0526-2 ↗
7. Some considerations on the warping of marble façades: the example of Alvar Aalto's Finland Hall in Helsinki10.1016/S0950-0618(99)00036-7 ↗
8. V.V.A.A. · 2015
9. Alnæs · 2004
10. Doehne · 2011
11. New trends and related problems in stone cleaning and conservation
12. A robust X-ray fluorescence technique for multielemental analysis of solid samples10.1007/s10661-016-5127-4 ↗
13. On the thermal degradation of marble10.1016/S0148-9062(98)00169-7 ↗
14. Physical weathering of marbles caused by anisotropic thermal expansion10.1007/s005310050324 ↗
15. Thermal degradation of marble: indications from finite-element modelling10.1016/S0360-1323(03)00082-9 ↗
16. FT-IR study of the hydrolysis and polymerization of tetraethyl orthosilicate and polydimethyl siloxane in the presence of tetrabutyl orthotitanate10.1081/SL-120028420 ↗
17. TiO2–SiO2–PDMS nano-composite hydrophobic coating with self-cleaning properties for marble protection10.1016/j.porgcoat.2012.10.006 ↗
18. Hydrophobizing coatings for cultural heritage. A detailed study of resin/stone surface interaction10.1007/s00339-013-8127-z ↗
19. Kinetic studies of attachment and re-orientation of octyltriethoxysilane for formation of self-assembled monolayer on a silica substrate
20. An infrared spectroscopic study of the nature of zinc carboxylates in oil paintings10.1039/C5JA00120J ↗
21. FTIR analysis of cellulose treated with sodium hydroxide and carbon dioxide10.1016/j.carres.2004.11.027 ↗
22. Ramachandran · 2002
23. Producing photoactive, transparent and hydrophobic SiO2-crystalline TiO2 nanocomposites at ambient conditions with application as self-cleaning coatings10.1016/j.apcatb.2014.03.042 ↗
24. Modified tetraethoxysilane with nanocalcium oxalate in one-pot synthesis for protection of building materials10.1021/acs.iecr.5b00247 ↗
25. Analyses of the surfaces of concrete by Raman and FT-IR spectroscopies: comparative study of hardened samples after demoulding and after organic post-treatment10.1002/sia.3548 ↗