Long-Term Deflections of Reinforced Concrete Beams Externally Bonded with FRP System
Source abstract
Abstract
External bonding of fiber-reinforced polymer (FRP) composite laminates to the tension soffit of reinforced concrete beams has become a popular method for flexural strengthening. However, the long-term performance of FRP-bonded beams under service loads is still a concern. This study was therefore aimed at investigating, both analytically and experimentally, the long-term deflection characteristics of FRP-bonded beams under sustained loads. Nine reinforced concrete beams, six of which were externally bonded with glass FRP composite laminates, were subjected to sustained loads for 2 years. The test parameters were the FRP ratio and sustained load level. The long-term deflections of the beams were reduced 23 and 33% with a FRP ratio of 0.64 and 1.92%, respectively. The total beam deflections were accurately predicted by the adjusted effective modulus method, and overestimated by about 20% by the effective modulus method.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Structural Behavior of Reinforced Concrete · Concrete Corrosion and Durability · Innovative concrete reinforcement materials
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
Associate Professor, Dept. of Civil Engineering, National Univ. of Singapore, Blk E1A, No. 07-03, 1 Engineering Dr. 2, Singapore 117576. E-mail: cvetankh@nus.edu.sg
Ph.D. Candidate, Dept. of Civil Engineering, National Univ. of Singapore, Blk E1A, No. 07-03, 1 Engineering Dr. 2, Singapore 117576. E-mail: g0203442@nus.edu.sg
References (15)
Show source-provided references
1. American Concrete Institute (ACI). (1992). “Prediction of creep shrinkage and temperature effects in concrete structures.” Manual of concrete practice ACI Committee 209R Detroit.
2. American Concrete Institute (ACI). (1995). “Control of deflection in concrete structures.” ACI Committee 435 Detroit 10 66–71.
3. American Concrete Institute (ACI). (2002). “Building code requirements for reinforced concrete and commentary.” ACI Committee 318 Detroit 353.
4. 10.1061/(ASCE)1090-0268(2001)5:2(102)10.1061/(ASCE)1090-0268(2001)5:2(102) ↗
5. Branson D. E. · 1977 · 167
6. 10.1016/S0950-0618(09)90034-410.1016/S0950-0618(09)90034-4 ↗
7. 10.1061/(ASCE)0733-9445(1995)121:4(727)10.1061/(ASCE)0733-9445(1995)121:4(727) ↗
8. Ghali A. · 1986 · 9
9. Gibson R. F. · 1994 · 69
10. Deflection calculation for reinforced concrete structures—Why we sometimes get it wrong
11. Time-dependent analysis of reinforced and prestressed concrete members
12. Holmes M. · 1983 · 213
13. Phillips L. N. · 1989 · 77
14. Strengthening of reinforced concrete beams with externally bonded composite laminates
15. 10.1061/(ASCE)0899-1561(1994)6:4(474)10.1061/(ASCE)0899-1561(1994)6:4(474) ↗