Stability of partially deacetylated chitin nano-fiber dispersions mediated by protonic acids

Authors not provided

Abstract

Partially deacetylated chitin nano-fiber (DAChN) dispersions were prepared using mechanical treatment of partially deacetylated crab shell α-chitin under acidic conditions mediated by various protonic acids. The representative organic acids had a better efficiency in terms of mediating the nanofibrillation of chitin fibers in comparison to the inorganic acid (HCl). The DAChN dispersed in water at a pH of 3.5 mediated by gluconic acid exhibited the highest yield of nano-fibers (88.6%), followed by succinic, itaconic, and ascorbic acids with a nano-fiber yield of 79.9%, 73.3% and 66.0%, respectively. The pH, conductivity, viscosity, and light transmittance of dispersions were assessed under different storage times. All of the tested DAChN dispersions were stable for at least 15 weeks at 4℃.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Nanocomposite Films for Food Packaging · Advanced Cellulose Research Studies · Electrospun Nanofibers in Biomedical Applications

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References

Reference metadata was not supplied for this record.