Prestress-loading effect on the current–voltage characteristics of a piezoelectric p–n junction together with the corresponding mechanical tuning laws
Source abstract
Abstract
A model is proposed to study the diffusion of non-equilibrium minority carriers under the influence of a piezo potential and to calculate the corresponding current–voltage (I–V) characteristics of a piezoelectric p–n junction exposed to mechanical loading. An effective solution to describe this non-equilibrium process has been put forward including two concepts: the influence of prestress loading on p–n junctions in a quasi-electrostatic thermal equilibrium and the perturbation of small fields superposed on the obtained quasi-electrostatic solutions. A few useful results are obtained through this loaded p–n junction model. Under a forward-bias voltage, a tensile (compressive) loading raises (reduces) the potential barrier of the space charge zone (SCZ), i.e., produces an equivalent reverse- (forward-) electric voltage on the SCZ. When a piezoelectric p–n junction is exposed to a reverse-bias voltage, the current density monotonically decreases with increasing reverse voltage and gradually approaches saturation. A bigger tensile (compressive) loading produces a smaller (larger) saturation current density. The appearance of an equivalent voltage on the SCZ induced by prestress indicates that the performance of a p–n junction with the piezo effect can be effectively tuned and controlled by mechanical loadings. Meanwhile, numerical results show that a loading location closer to the SCZ produces a stronger effect on the I–V characteristics of a piezoelectric p–n junction, implying that the tuning effect of mechanical loadings depends on how much influence of the deformation-induced electric field can reach the SCZ. Furthermore, it is also found that the deformation-induced electric field becomes weak with increasing doping because the higher doping is corresponding to the stronger electric leakage. Thus, the higher mechanical tuning performance on higher doped piezoelectric p–n junctions requires the prestress loadings to be applied closer to the interface of p- and n-zone. This study on a non-equilibrium process of piezoelectric p–n junctions has significance for piezotronics.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Thermal properties of materials · Innovative Energy Harvesting Technologies · Advanced Sensor and Energy Harvesting Materials
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (34)
Show source-provided references
1. 10.1016/j.nantod.2010.10.00810.1016/j.nantod.2010.10.008 ↗
2. 10.1016/s1369-7021(07)70076-710.1016/s1369-7021(07)70076-7 ↗
3. 10.1557/mrs.2018.26310.1557/mrs.2018.263 ↗
4. 10.1016/j.nanoen.2019.01.01210.1016/j.nanoen.2019.01.012 ↗
5. 10.1016/j.actamat.2018.10.00810.1016/j.actamat.2018.10.008 ↗
6. 10.1016/j.mser.2010.06.01510.1016/j.mser.2010.06.015 ↗
7. 10.1038/nnano.2010.4610.1038/nnano.2010.46 ↗
8. 10.1126/science.112400510.1126/science.1124005 ↗
9. 10.1038/nature0660110.1038/nature06601 ↗
10. 10.1038/nnano.2008.31410.1038/nnano.2008.314 ↗
11. 10.1002/adfm.20080054110.1002/adfm.200800541 ↗
12. 10.1021/nl071310j10.1021/nl071310j ↗
13. 10.1002/adma.20110090610.1002/adma.201100906 ↗
14. 10.1063/1.9932510.1063/1.99325 ↗
15. 10.1109/ultsym.1986.19878010.1109/ultsym.1986.198780 ↗
16. Zhu · Acta Mechanica Solida Sinica · 2017 · 3 · 46
17. Pierret · 1988
18. 10.1088/1361-665x/aa542e10.1088/1361-665x/aa542e ↗
19. 10.1007/s10338-019-00109-310.1007/s10338-019-00109-3 ↗
20. 10.1016/j.nanoen.2017.07.04910.1016/j.nanoen.2017.07.049 ↗
21. 10.1007/978-3-319-77504-3_1310.1007/978-3-319-77504-3_13 ↗
22. 10.3762/bjnano.9.18310.3762/bjnano.9.183 ↗
23. 10.1016/j.nanoen.2017.11.00210.1016/j.nanoen.2017.11.002 ↗
24. 10.1088/2053-1591/aaecbb10.1088/2053-1591/aaecbb ↗
25. 10.1063/1.504473910.1063/1.5044739 ↗
26. 10.1016/j.nanoen.2018.10.03710.1016/j.nanoen.2018.10.037 ↗
27. 10.1007/s10338-018-0010-110.1007/s10338-018-0010-1 ↗
28. 10.1016/j.nanoen.2018.08.01710.1016/j.nanoen.2018.08.017 ↗
29. 10.1063/1.499675410.1063/1.4996754 ↗
30. 10.1016/j.commatsci.2018.05.04110.1016/j.commatsci.2018.05.041 ↗
31. 10.1016/s0020-7683(02)00122-110.1016/s0020-7683(02)00122-1 ↗
32. Huang · 2015
33. 10.1109/58.26582010.1109/58.265820 ↗
34. Auld · 1973 · I