The analyses of precipitation processes in the microstructure of S31035 steel after ageing at 750 °C
Source abstract
Abstract
Abstract This paper presents the results of the analysis of the precipitation process in S31035 (22Cr25Ni3W3CuCoNbN) steel after long-term ageing at 750 °C for up to 30,000 h. The identification of precipitates was carried out using selective electron diffraction with FEI TITAN 80–300 transmission electron microscope. In the microstructure of the test steel in the as-received condition, the primary precipitates of Z phase were revealed. Ageing has contributed to the precipitation of secondary phases at the grain boundaries, twin boundaries and inside the grains. At the grain boundaries, M 23 C 6 carbides and Laves phase precipitates were revealed during the initial period of ageing. Longer ageing times resulted in the occurrence of sigma phase and G phase particles at the boundaries. Only M 23 C 6 carbides were observed at the twin boundaries. In turn, inside the grains, the presence of ε_Cu particles, Laves phase and secondary Z phase precipitates was demonstrated. In addition, single complexes of precipitates consisting of the primary Z phase particles and M 23 C 6 carbides nucleating on them as well as the Laves phase precipitates were revealed near the grain boundaries.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: High Temperature Alloys and Creep · Microstructure and Mechanical Properties of Steels · Hydrogen embrittlement and corrosion behaviors in metals
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (37)
Show source-provided references
1. Jurasz J, Mikulik J. Economic and environmental analysis of a hybrid solar, wind and pumped storage hydroelectric energy source: a Polish perspective. Bull Pol Ac Tech. 2017;66(6):859–69. https://doi.org/10.1515/bpasts-2017-0093.10.1515/bpasts-2017-0093 ↗
2. Dak G, Pandey C. A critical review on dissimilar welds joint between martensitic and austenitic steel for power plant application. J Manuf Process. 2020;58:377–406. https://doi.org/10.1016/j.jmapro.2020.08.019.10.1016/j.jmapro.2020.08.019 ↗
3. Golański G. Modern heat-resistant 11%Cr martensitic steel for power industry. Arch Mater Sc Eng. 2022;113:5–12. https://doi.org/10.5604/01.3001.0015.6966.10.5604/01.3001.0015.6966 ↗
4. Chai G, Forsberg U. Sanicro 25: An advanced high-strength, heat-resistant austenitic stainless steel, W: A. Di Gianfrancesco, editor, Materials for Ultra-Supercritical and Advanced Ultra-Supercritical Power Plants. Woodhead Publishing, 2017, pp. 391–421.10.1016/B978-0-08-100552-1.00012-9 ↗
5. Zieliński A, Wersta R, Sroka M. Analysis of the precipitation process of secondary phases after long-term ageing of the S304H steel, Bull. Pol Ac Tech. 2021;69(5):e137520. https://doi.org/10.24425/bpasts.2021.137520.10.24425/bpasts.2021.137520 ↗
6. Yang X, Yu C, Yang X, Yan K, Qian G, Wang B, Yan W, Shi X. Microstructure and mechanical properties of an austenitic heat-resistant steel after service at 570°C and 25.4 MPa for 18 years. JMEPEG. 2021;30:1030–8.10.1007/s11665-020-05420-6 ↗
7. Zurek J, Yang S-M, Lin D-Y, Huttel T, Singheiser L, Quadakkers WJ. Microstructural stability and oxidation behaviour of Sanicro 25 during long-term steam exposure in the temperature range 600–750°C. Mater Corros. 2014;66:315–27. https://doi.org/10.1002/maco.201407901.10.1002/maco.201407901 ↗
8. Petras PR, Skorik V, Polak J. Thermomechanical fatigue and damage mechanisms in Sanicro 25. Mat Sci Eng A Struct. 2016;650:52–62. https://doi.org/10.1016/j.msea.2015.10.030.10.1016/j.msea.2015.10.030 ↗
9. Heczko M, Polak J, Kruml T. Microstructure and dislocation arrangements in Sanicro 25 steel fatigue at ambient and elevated temperatures. Mat Sci Eng A Struct. 2017;680:168–81. https://doi.org/10.1016/j.msea.2016.10.076.10.1016/j.msea.2016.10.076 ↗
10. Zhou R, Zhu L, Liu Y, Lu Z, Chan L, Ma X. Microstructural evolution and the effect on hardness of Sanicro 25 welded joint base metal after creep at 973K. J Mater Sci. 2017;52:6161–72. https://doi.org/10.1007/s10853-017-0758-6.10.1007/s10853-017-0758-6 ↗
11. Suo J, Peng Z, Yang H, Chai G, Yu M. Formation of Laves phase in Sanicro 25 austenitic steel during creep-rupture test at 700°C. Metallogr Microstruct Anal. 2019;8:281–6. https://doi.org/10.1007/s13632-019-00529-0.10.1007/s13632-019-00529-0 ↗
12. Zhou R, Zhu L, Yang Y, Lu Z, Chen L. Microstructural evolution and the effect on hardness and impact toughness of Sanicro 25 welded joints after ageing at 973K, Metall. Mater Trans A. 2018;49:6290–307. https://doi.org/10.1007/s11661-018-4906-7.10.1007/s11661-018-4906-7 ↗
13. Zhou R, Zhu L. Growth behavior and strengthening mechanism of Cu-rich particles in Sanicro 25 austenitic heat-resistant steel after aging at 973K. Mat. Sci. Eng. A Struct. 2020;796:139973. https://doi.org/10.1016/j.msea.2020.139973.10.1016/j.msea.2020.139973 ↗
14. Sun W, Qin X, Guo J, Lou L, Zhou L. Thermal stability of primary MC carbide and its influence on the performance of cast Ni-base superalloys. Mater Des. 2015;69:81–8. https://doi.org/10.1016/j.matdes.2014.12.038.10.1016/j.matdes.2014.12.038 ↗
15. Solenthaler C, Ramesh M, Uggowitzer PJ, Spolenak R. Precipitation strengthening of Nb-stabilised TP347 austenitic steels by a dispersion of secondary Nb(C, N) formed upon a short-term hardening heat treatment. Mat Sci Eng A Struct. 2015;647:294–302. https://doi.org/10.1016/j.msea.2015.09.028.10.1016/j.msea.2015.09.028 ↗
16. Zhou Y, Aust KT, Erb U, Palumbo G. Effects of grain boundary structure on carbide precipitation in 304L stainless steel. Scr Mater. 2001;45:49–54. https://doi.org/10.1016/s1359-6462(01)00990-3.10.1016/s1359-6462(01)00990-3 ↗
17. Lv H, Chen S, Rong L. Evolution of precipitate and its effect on the degradation of impact toughness in a carbon and nitrogen-controlled 316 stainless steel during thermal aging at 650°C. J Mater Resear Technol. 2024;33:3728–37422. https://doi.org/10.1016/j.jmrt.2024.10.043.10.1016/j.jmrt.2024.10.043 ↗
18. Zieliński A, Golański G, Sroka M. Evolution of the microstructure and mechanical properties of HR3C austenitic stainless steel after ageing for up to 30,000 h at 650–750°C. Mat Sci Eng A Struct. 2020;796:139944. https://doi.org/10.1016/j.msea.2020.139944.10.1016/j.msea.2020.139944 ↗
19. Gajjar PK, Khatri BC, Siddhpura AM, Siddhpura MA. Sensitization and desensitisation (healing) in austenitic stainless steel: a critical review. Trans Indian Inst Met. 2022;75:1411–27. https://doi.org/10.1007/s12666-021-02439-8.10.1007/s12666-021-02439-8 ↗
20. Fedoseeva A, Tkachev E, Dudko V, Dudova N, Kaibyshev R. Effect alloying on interfacial energy of precipitation/matrix in high-chromium martensitic steels. J Mater Sci. 2017;52:4197–209. https://doi.org/10.1007/s10853-016-0654-5.10.1007/s10853-016-0654-5 ↗
21. Abe F. Effect of boron on microstructure and creep strength advanced ferritic power plant steel. Eng Proc. 2011;10:94–9. https://doi.org/10.1016/j.proeng.2011.04.018.10.1016/j.proeng.2011.04.018 ↗
22. Chen SW, Zhang C, Xia ZX, Ishikawa H, Yang ZG. Precipitation behavior of Fe2Nb Laves phase on grain boundaries in austenitic heat resistant steels. Mat Sci Eng A Struct. 2014;615:183–8. https://doi.org/10.1016/j.msea.2014.07.104.10.1016/j.msea.2014.07.104 ↗
23. Aghajani A, Richter F, Somsen C, Fries SG, Steinbach I, Eggeler G. On the formation and growth of Mo-rich Laves phase particles during long-term creep of a 12% chromium tempered martensite ferritic steel. Scr Mater. 61(11):1068–71. https://doi.org/10.1016/j.scriptamat.2009.08.03110.1016/j.scriptamat.2009.08.031 ↗
24. Roychowdhury S, Kalin V, Matcheswala A, Bhandakkar A. σ-Phase induced embrittlement in titanium containing austenitic stainless steel tie-bars in a condenser. Eng Fail Anal. 2012;25:123–32. https://doi.org/10.1016/j.engfailanal.2012.05.002.10.1016/j.engfailanal.2012.05.002 ↗
25. Padilha AF, Rios PR. Decomposition of austenite in austenite stainless steel. ISIJ Int. 2002;42:325–37. https://doi.org/10.2355/isijinternational.42.325.10.2355/isijinternational.42.325 ↗
26. Minami Y, Kimura H, Ihara Y. Microstructural changes in austenitic stainless steels during long-term aging. Mater Sci Tech Lond. 1986;2:795–806. https://doi.org/10.1179/mst.1986.2.8.795.10.1179/mst.1986.2.8.795 ↗
27. Purzyńska H, Golański G, Zieliński A, Dobrzański J, Sroka M. Precipitation study in Ti-stabilised austenitic stainless steel after 207,000 h of service. Mater High Temp. 2019;36:296–303. https://doi.org/10.1080/09603409.2018.1546919.10.1080/09603409.2018.1546919 ↗
28. Zieliński A, Wersta R, Sroka M. The study of the evolution of the microstructure and creep properties of Super 304H austenitic stainless steel after aging for up to 50,000 h. Arch Civ Mech Eng. 2022;22(89). https://doi.org/10.1007/s43452-022-00408-6.10.1007/s43452-022-00408-6 ↗
29. Wang JZ, Liu Z-D, Bao H-S, Cheng S-C. Evolution of precipitates of S31042 heat resistant steel during 700°C aging. J Iron Steel Res Int. 2013;20:113–21. https://doi.org/10.1016/s1006-706x(13)60186-7.10.1016/s1006-706x(13)60186-7 ↗
30. Cempura G, Kruk A. Precipitation processes in Sanicro 25 Steel at 700–900°C: experimental study and digital twin simulation. Materials. 2025;18(15):3594. https://doi.org/10.3390/ma1815359410.3390/ma18153594 ↗
31. Li Y, Wang X. Strengthening mechanisms and creep rupture behavior of advanced austenitic heat resistant steel SA-213 S31035 for A-USC power plants. Mat Sci Eng A Struct. 2020;775. https://doi.org/10.1016/j.msea.2020.138991.10.1016/j.msea.2020.138991 ↗
32. Bai JW, Liu PP, Zhu YM, Chi CY, Yu XY, Xie XS, Zhan Q. Coherent precipitation of copper in Super304H austenitic steel. Mat Sci Eng A Struct. 2013;584:57–62. https://doi.org/10.1016/j.msea.2013.06.082.10.1016/j.msea.2013.06.082 ↗
33. Zhang L, Zhu L, Lu Z. Microstructural evolution and the effect on mechanical properties of S30432 heat-resistant steel during aging at 650°C. ISIJ Int. 2010;50:596–600. https://doi.org/10.2355/isijinternational.50.596.10.2355/isijinternational.50.596 ↗
34. Li Y, Liu Y, Liu C, Li C, Li H. Mechanism for the formation of Z-phase in 25Cr-20Ni-Nb-N austenitic stainless steel. Mater Lett. 2018;233:16–9. https://doi.org/10.1016/j.matlet.2018.08.141.10.1016/j.matlet.2018.08.141 ↗
35. Zhou R, Zhu L, Liu Y, Lu Z, Chen L. Precipitates and precipitation strengthening of Sanicro 25 welded joint base metal crept at 973 K. Steel Res Int. 2017;88. https://doi.org/10.1002/srin.201600414.10.1002/srin.201600414 ↗
36. Golański G, Wieczorek P. Precipitation of carbides in Cr-Mo-V caste steel after service and regenerative heat treatment. Arch Found Eng. 2009;9:97–102.
37. Golański G, Zieliński A, Merda A, Urbańczyk P, Słania J, Kierat M. Microstructure and mechanical properties of HR6W alloy dedicated for manufacturing of pressure elements in supercritical and ultra-supercritical power units. In: Proceedings of E3S Web of Conferences ICBT Poland 2018; 2019. p. 01005. https://doi.org/10.1051/e3sconf/20198201005.10.1051/e3sconf/20198201005 ↗