journal article·2026-06-23Open access

The use of granulated copper slag as a raw material component for Portland cement clinker production

Wojciech Wons, Karol Rzepa, Aleksander Glich, Sebastian Komarek

Abstract

Abstract The cement industry is energy-intensive, highly-emissive, and fossil fuels-consuming. The natural direction of its development is the partial substitution of raw materials, e.g. with industrial waste. Such potential, alternative raw material is granulated copper slag (GCS), which has a high Fe 2 O 3 content, making it a potential iron-bearing raw material in the production of Portland clinker. Moreover, GCS contains CaO in a decarbonated form. Therefore, its use can contribute to CO 2 emissions reduction in the production of Portland clinker. However, GCS contains components that are not desirable in excessive amounts, such as heavy metals. As literature indicate, they may have a real impact on the clinkerization and the properties of Portland clinker. The main aim of the article is to assess the effect of GCS on the sinterability of Portland clinker, including the influence of heavy metals introduced. The sinterability tests carried out on batches with different GCS contents allowed us to establish that its substitution for the natural iron-bearing raw material does not cause a decrease in the sinterability, but decreases the grindability of Portland clinker. It was shown that Ti and Mn has location priority in the C 4 AF phase, while the remaining metals are evenly distributed in all phases present in Portland clinker. The higher GCS addition, the greater the share of the M3 alite in the clinker, at the expense of the M1 variety. The decrease in CO 2 emissions associated with the introduction of the calcite-free CaO along with the slag is lower than the expected calculated value.
Source: crossref · Quality: baseline

Research context

OpenAlex topics: Concrete and Cement Materials Research · Recycling and utilization of industrial and municipal waste in materials production · Advanced materials and composites

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (51)

Show source-provided references
1. Phiri TC, Singh P, Nikoloski AN. The potential for copper slag waste as a resource for a circular economy: A review–Part I. Min Eng. 2022;180:107474.10.1016/j.mineng.2022.107474 ↗
2. Klaffenbach E, Montenegro V, Guo M, Blanpain B. Sustainable and Comprehensive Utilization of Copper Slag: A Review and Critical Analysis. J Sustainable Metall. 2023;9:468–96. https://doi.org/10.1007/s40831-023-00683-4.10.1007/s40831-023-00683-4 ↗
3. Phiri TC, Singh P, Nikoloski AN. The potential for copper slag waste as a resource for a circular economy: A review–Part II. Min Eng. 2021;172:107150.10.1016/j.mineng.2021.107150 ↗
4. Wang D, Wang Q, Huang Z. Reuse of copper slag as a supplementary cementitious material: Reactivity and safety. Resour Conserv Recycl. 2020;162:105037. https://doi.org/10.1016/j.resconrec.2020.105037.10.1016/j.resconrec.2020.105037 ↗
5. Alp İ, Deveci H, Süngün H. Utilization of flotation wastes of copper slag as raw material in cement production. J Hazard Mater. 2008;159:390–5. https://doi.org/10.1016/j.jhazmat.2008.02.056.10.1016/j.jhazmat.2008.02.056 ↗
6. Łowińska-Kluge A. Żużel pomiedziowy jako składnik kompozytów cementowych o zwiększonej trwałości. Wydawnictwo Politechniki Poznańskiej, 2008. https://books.google.pl/books?id=PjQyYAAACAAJ
7. Vanguri Suresh P, Suresh P, Gonthi CS, Kumar M, Bibekananda. Feasibility Studies for Use of Copper Slag in Clinker Manufacture. Makara J Sci. 2022;26. https://doi.org/10.7454/mss.v26i4.1306.10.7454/mss.v26i4.1306 ↗
8. Matkarimov S, Berdiyarov B, Nosirkhujayev S, Ochildiyev K, Marjorie B. PROCESSING OF SLAGS OF COPPER MANUFACTURING WITH THE USE OF IDEAL MIXING EQUIPMENT. Tech Sci Innov. 2020;2020:227–34. https://doi.org/10.51346/tstu-01.20.3-77-0088.10.51346/tstu-01.20.3-77-0088 ↗
9. Shen H, Forssberg E. An overview of recovery of metals from slags. Waste Manag. 2003;23:933–49. https://doi.org/10.1016/S0956-053X(02)00164-2.10.1016/S0956-053X(02)00164-2 ↗
10. Habib A, Bhatti HN, Iqbal M. Metallurgical Processing Strategies for Metals Recovery from Industrial Slags. Z für Phys Chem. 2020;234:201–31. https://doi.org/10.1515/zpch-2019-0001.10.1515/zpch-2019-0001 ↗
11. Bellemans I, De Wilde E, Moelans N, Verbeken K. Metal losses in pyrometallurgical operations - A review. Adv Colloid Interface Sci. 2018;255:47–63. https://doi.org/10.1016/j.cis.2017.08.001.10.1016/j.cis.2017.08.001 ↗
12. Barnes CD, Lumsdaine I, O’Hare SM. Copper converter slag treatment at Mount Isa Mines Limited, Mount Isa, Qld, in: AusIMM Proc, 1993: p. 31.
13. Anand S, Rao PK, Jena PK. Recovery of metal values from copper converter and smelter slags by ferric chloride leaching. Hydrometallurgy. 1980;5:355–65.10.1016/0304-386X(80)90025-0 ↗
14. Basir SMA, Rabah MA. Hydrometallurgical recovery of metal values from brass melting slag. Hydrometallurgy. 1999;53:31–44.10.1016/S0304-386X(99)00030-4 ↗
15. Ziyadanogullari B. Recovery of copper and cobalt from concentrate and converter slag. Sep Sci Technol. 2000;35:1963–71.10.1081/SS-100100630 ↗
16. Tümen F, Bailey NT. Recovery of metal values from copper smelter slags by roasting with pyrite. Hydrometallurgy. 1990;25:317–28.10.1016/0304-386X(90)90047-6 ↗
17. Huang X, Wang F. An overview of steel slag processing and utilization. Manganese Ore China. 2001;3:135-139.
18. Murari K, Siddique R, Jain KK. Use of waste copper slag, a sustainable material. J Mater Cycles Waste Manag. 2015;17:13–26. https://doi.org/10.1007/s10163-014-0254-x.10.1007/s10163-014-0254-x ↗
19. Hallet V, De Belie N, Pontikes Y. The impact of slag fineness on the reactivity of blended cements with high-volume non-ferrous metallurgy slag. Constr Build Mater. 2020;257:119400. https://doi.org/10.1016/j.conbuildmat.2020.119400.10.1016/j.conbuildmat.2020.119400 ↗
20. Feng Y, Kero J, Yang Q, Chen Q, Engström F, Samuelsson C, Qi C. Mechanical Activation of Granulated Copper Slag and Its Influence on Hydration Heat and Compressive Strength of Blended Cement. Materials. 2019;12:772. https://doi.org/10.3390/ma12050772.10.3390/ma12050772 ↗
21. Gorai B, Jana RK. Premchand, Characteristics and utilisation of copper slag—a review. Resour Conserv Recycl. 2003;39:299–313. https://doi.org/10.1016/S0921-3449(02)00171-4.10.1016/S0921-3449(02)00171-4 ↗
22. Huang K. Use of copper slag in cement production. Sichuan Cem. 2001;4:25–7.
23. Shi C, Meyer C, Behnood A. Utilization of copper slag in cement and concrete. Resour Conserv Recycl. 2008;52:1115–20. https://doi.org/10.1016/j.resconrec.2008.06.008.10.1016/j.resconrec.2008.06.008 ↗
24. Dhir R, Brito J, Mangabhai R, Lye CQ. Sustainable Construction Materials: Copper Slag, 2016.10.1016/B978-0-08-100986-4.00001-8 ↗
25. Tan Y, Zhou Q, Wei R. The initial study on the use of copper slag as a additional materials for cement production. J Xinjiang Inst Technol. 2000;21:236–9.
26. Guo Y. Investigations on the use of industrial wastes in cement production. Arid Environ Monit. 2003;17:177–9.
27. Cheng Y, Qi R, Hou J, Huang Q. Feasibility study on utilization of copper tailings as raw meal and addition for low carbon Portland cement production. Constr Build Mater. 2023;382:131275. https://doi.org/10.1016/j.conbuildmat.2023.131275.10.1016/j.conbuildmat.2023.131275 ↗
28. Zhao R, Zhang L, Fan G, Chen Y, Huang G, Zhang H, Zhu J, Guan X. Probing the exact form and doping preference of magnesium in ordinary Portland cement clinker phases: A study from experiments and DFT simulations. Cem Concr Res. 2021;144:106420. https://doi.org/10.1016/j.cemconres.2021.106420.10.1016/j.cemconres.2021.106420 ↗
29. Gao T, Dai T, Shen L, Jiang L. Benefits of using steel slag in cement clinker production for environmental conservation and economic revenue generation. J Clean Prod. 2021;282:124538. https://doi.org/10.1016/j.jclepro.2020.124538.10.1016/j.jclepro.2020.124538 ↗
30. Kolovos K, Tsivilis S, Kakali G. The effect of foreign ions on the reactivity of the CaO–SiO 2 –Al 2 O 3 –Fe 2 O 3 system. Cem Concr Res. 2002;32:463–9. https://doi.org/10.1016/S0008-8846(01)00705-0.10.1016/S0008-8846(01)00705-0 ↗
31. Ma X-W, Chen H-X, Wang P-M. Effect of CuO on the formation of clinker minerals and the hydration properties. Cem Concr Res. 2010;40:1681–7. https://doi.org/10.1016/j.cemconres.2010.08.009.10.1016/j.cemconres.2010.08.009 ↗
32. Zhang B, Bogush A, Wei J, Zhang T, Xu W, Yu Q. Influence of sulfur on the fate of heavy metals during clinkerization. Constr Build Mater. 2018;182:144–55. https://doi.org/10.1016/j.conbuildmat.2018.06.084.10.1016/j.conbuildmat.2018.06.084 ↗
33. Al-sallami ZHA, Marshdi QSR, Mukheef RAAH. Effect of cement replacement by fly ash and epoxy on the properties of pervious concrete. Asian J Civil Eng. 2020;21:49–58. https://doi.org/10.1007/s42107-019-00183-5.10.1007/s42107-019-00183-5 ↗
34. Alsalami ZHA. Study the effect of partially replacement sand by waste pistachio shells in cement mortar. Appl Adhes Sci. 2017;5. https://doi.org/10.1186/s40563-017-0099-3.10.1186/s40563-017-0099-3 ↗
35. Lee DJ. Effect of calcite on Pb-doped solidified waste forms in leaching. Chemosphere. 2006;63:1903–11. https://doi.org/10.1016/j.chemosphere.2005.10.018.10.1016/j.chemosphere.2005.10.018 ↗
36. Halim CE, Amal R, Beydoun D, Scott JA, Low GKC. Leachability of lead and cadmium from cementitious wastes, in: Developments in Chemical Engineering and Mineral Processing, Curtin University of Technology, 2004: pp. 355–368. https://doi.org/10.1002/apj.550012041110.1002/apj.5500120411 ↗
37. Hu P, Dai W. Computer modeling of leaching of heavy metal from cementitious waste. Res J Appl Sci Eng Technol. 2013;6:2083–5. https://doi.org/10.19026/rjaset.6.3828.10.19026/rjaset.6.3828 ↗
38. Suzuki K, Ono Y. Leaching characteristics of stabilized/solidified fly ash generated from ash-melting plant. Chemosphere. 2008;71:922–32. https://doi.org/10.1016/j.chemosphere.2007.11.002.10.1016/j.chemosphere.2007.11.002 ↗
39. Gheorghe M, Radu L, Năstac D, Saca N, Caracteristici de mediu ale betonului cu ciment fabricat cu combustibil alternativ ▲. Environmental characteristics of concrete with cement manufactured with alternative fuel, 2013.
40. Blaise R, Musikas N, Tiedrez H. Nouvelle méthode de détermination cinétique de lÕ aptitude ala cuisson dÕ un cru de cimenterie. Rev Mater Constr. 1971;674-675.
41. Javellana MP, Jawed I. Extraction of free lime in portland cement and clinker by ethylene glycol. Cem Concr Res. 1982;12:399–403. https://doi.org/10.1016/0008-8846(82)90088-6.10.1016/0008-8846(82)90088-6 ↗
42. PN-EN 196-6. Metody badania cementu. Oznaczanie stopnia zmielenia; 1997.
43. Taylor HFW. Cement chemistry, Thomas Telford London, 1997.
44. de Matos PR, Andrade Neto JS, Campos CEM, Snellings R, Dinnebier RE, Kirchheim AP. Polymorph and minor phase quantification in Portland clinker by X-ray powder diffraction analysis: Addressing challenges and foreign ion effects. Cem Concr Res. 2025;190:107801. https://doi.org/10.1016/j.cemconres.2025.107801.10.1016/j.cemconres.2025.107801 ↗
45. Kocaba V, Gallucci E, Scrivener KL. Methods for determination of degree of reaction of slag in blended cement pastes. Cem Concr Res. 2012;42:511–25. https://doi.org/10.1016/j.cemconres.2011.11.010.10.1016/j.cemconres.2011.11.010 ↗
46. Jansen D, Goetz-Neunhoeffer F, Lothenbach B, Neubauer J. The early hydration of Ordinary Portland Cement (OPC): An approach comparing measured heat flow with calculated heat flow from QXRD. Cem Concr Res. 2012;42:134–8. https://doi.org/10.1016/j.cemconres.2011.09.001.10.1016/j.cemconres.2011.09.001 ↗
47. Prince W, Espagne M, Aı̈tcin P-C. Ettringite formation. Cem Concr Res. 2003;33:635–41. https://doi.org/10.1016/S0008-8846(02)01042-6.10.1016/S0008-8846(02)01042-6 ↗
48. Szudek W, Szydłowski J, Buchała I, Kapeluszna E. Synthesis and Characterization of Calcium Sulfoaluminate Hydrates—Ettringite (AFt) and Monosulfate (AFm). Materials. 2024;17:5216.10.3390/ma17215216 ↗
49. Zhou H, Yao X, Min H, Huang H, Ma B, Shen X, Liu Y, Lin T. Research on structure modulation of alite and its effect on the mechanical properties of cement clinker. Constr Build Mater. 2021;303:124511. https://doi.org/10.1016/j.conbuildmat.2021.124511.10.1016/j.conbuildmat.2021.124511 ↗
50. Wang Q, Gu X, Zhou H, Chen X, Shen X. Cation substitution induced reactivity variation on the tricalcium silicate polymorphs determined from first-principles calculations. Constr Build Mater. 2019;216:239–48. https://doi.org/10.1016/j.conbuildmat.2019.05.005.10.1016/j.conbuildmat.2019.05.005 ↗
51. Zunino F, Scrivener K. Factors influencing the sulfate balance in pure phase C3S/C3A systems. Cem Concr Res. 2020;133. https://doi.org/10.1016/j.cemconres.2020.106085.10.1016/j.cemconres.2020.106085 ↗