WAAM-based repair cladding for forging tools: a comprehensive study of wear in laboratory and industrial conditions
Source abstract
Abstract
This study explores Wire Arc Additive Manufacturing (WAAM) as a repair method for forging tools, comparing it to conventional H11 tool steel. Laboratory tests were conducted on four samples obtained from different WAAM layers, which are representative of the respective layer positions for hardness and wear tests at room temperature and 500 °C. Chemical composition analysis was performed to verify compliance with tool steel standards, and evaluations included hardness testing at both temperatures, tensile strength assessment, wear resistance measurements (ball-on-disc mode), and hardness mapping to verify layer consistency. The WAAM material exhibited wear factors on the order of 10⁻⁶ mm³/Nm, below typical literature values reported for H11 tool steel, and showed a clear correlation between layer hardness and wear response. Industrial validation through hot forging trials demonstrated that WAAM-repaired tools achieved 3000 cycles compared to 2500 cycles for conventionally repaired tools, with approximately 60% shorter repair time and 21% lower filler material consumption. These results confirm WAAM as a viable and superior method for cladding and repairing forging tools, offering improved durability, higher efficiency, and reduced use of expensive alloying elements in industrial applications.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Additive Manufacturing Materials and Processes · High Entropy Alloys Studies · Metal Alloys Wear and Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (48)
Show source-provided references
1. Widomski P, Gronostajski Z. Comprehensive review of methods for increasing the durability of hot forging tools. Procedia Manuf. 2020;47:349–355. https://doi.org/10.1016/j.promfg.2020.04.280.10.1016/j.promfg.2020.04.280 ↗
2. Ahn D-G. Hardfacing technologies for improvement of wear characteristics of hot working tools: a review. Int J Precis Eng Manuf. 2013;14:1271–83. https://doi.org/10.1007/s12541-013-0174-z.10.1007/s12541-013-0174-z ↗
3. Lange K, Cser L, Geiger M, Kals JAG. Tool life and tool quality in bulk metal forming. CIRP Ann. 1992;41:667–75. https://doi.org/10.1016/S0007-8506(07)63253-3.10.1016/S0007-8506(07)63253-3 ↗
4. Emamverdian AA, Sun Y, Cao C, Pruncu C, Wang Y. Current failure mechanisms and treatment methods of hot forging tools (dies) - a review. Eng Fail Anal. 2021;129:105678. https://doi.org/10.1016/j.engfailanal.2021.105678.10.1016/j.engfailanal.2021.105678 ↗
5. Euroforge IS. 2023-2, https://www.euroforge.org/wp-content/uploads/2023/09/International-Statistics-2023-2.pdf, (n.d.).
6. Singh AK. Factors affecting die wear. Wear. 1973;25:271–9. https://doi.org/10.1016/0043-1648(73)90077-X.10.1016/0043-1648(73)90077-X ↗
7. Wanheim T, Bay N, Petersen AS. A theoretically determined model for friction in metal working processes. Wear. 1974;28:251–8. https://doi.org/10.1016/0043-1648(74)90165-3.10.1016/0043-1648(74)90165-3 ↗
8. Kchaou M, Elleuch R, Desplanques Y, Boidin X, Degallaix G. Failure mechanisms of H13 die on relation to the forging process – a case study of brass gas valves. Eng Fail Anal. 2010;17:403–15. https://doi.org/10.1016/j.engfailanal.2009.08.015.10.1016/j.engfailanal.2009.08.015 ↗
9. Kim DH, Lee HC, Kim BM, Kim KH. Estimation of die service life against plastic deformation and wear during hot forging processes. J Mater Process Technol. 2005;166:372–80. https://doi.org/10.1016/j.jmatprotec.2004.07.103.10.1016/j.jmatprotec.2004.07.103 ↗
10. Kang JH, Park IW, Jae JS, Kang SS. A study on die wear model considering thermal softening (II): application of the suggested wear model. J Mater Process Technol. 1999;94:183–8. https://doi.org/10.1016/S0924-0136(99)00104-1.10.1016/S0924-0136(99)00104-1 ↗
11. Sharma R, Arrowsmith DJ. The wear of forging dies in the first five forging blows. Wear. 1981;74:1–10. https://doi.org/10.1016/0043-1648(81)90190-3.10.1016/0043-1648(81)90190-3 ↗
12. Summerville E, Venkatesan K, Subramanian C. Wear processes in hot forging press tools. Mater Des. 1995;16:289–94. https://doi.org/10.1016/0261-3069(96)00010-6.10.1016/0261-3069(96)00010-6 ↗
13. Gronostajski Z, Kaszuba M, Hawryluk M, Zwierzchowski M. A review of the degradation mechanisms of the hot forging tools. Arch Civ Mech Eng. 2014;14:528–39. https://doi.org/10.1016/j.acme.2014.07.002.10.1016/j.acme.2014.07.002 ↗
14. Lv L, Deng Z, Liu T, Wan L, Huang W, Yin H, Zhao T. A composite evaluation model of sustainable manufacturing in machining process for typical machine tools. Processes. 2019;7:110. https://doi.org/10.3390/pr7020110.10.3390/pr7020110 ↗
15. Ong SK, Fang HC, Nee AYC. A design feature-based approach for product remanufacturability assessment and analysis. Procedia CIRP. 2016;53:15–20. https://doi.org/10.1016/j.procir.2016.07.005.10.1016/j.procir.2016.07.005 ↗
16. Reike D, Vermeulen WJV, Witjes S. The circular economy: new or refurbished as CE 3.0? — exploring controversies in the conceptualization of the circular economy through a focus on history and resource value retention options. Resour Conserv Recycl. 2018;135:246–64. https://doi.org/10.1016/j.resconrec.2017.08.027.10.1016/j.resconrec.2017.08.027 ↗
17. Velte C.J., Scheller K., Steinhilper R. Circular economy through Objectives – Development of a proceeding to understand and shape a circular economy using Value-focused thinking. Procedia CIRP. 2018;69:775–80. https://doi.org/10.1016/j.procir.2017.11.031.10.1016/j.procir.2017.11.031 ↗
18. Rahito D, Wahab A, Azman. Additive manufacturing for repair and restoration in remanufacturing: an overview from object design and systems perspectives. Processes. 2019;7:802. https://doi.org/10.3390/pr7110802.10.3390/pr7110802 ↗
19. Paterson DAP, Ijomah WL, Windmill JFC. End-of-life decision tool with emphasis on remanufacturing. J Clean Prod. 2017;148:653–64. https://doi.org/10.1016/j.jclepro.2017.02.011.10.1016/j.jclepro.2017.02.011 ↗
20. Pytel S, Turek J, Okoński S, Zarębski K. The properties and microstructure of padding welds built up on the surface of forging dies. Arch Foundry Eng. 2010;10:5–10. http://www.afe.polsl.pl/index.php/pl/magazine/show/64/volume-10-special-issue-3-2010.
21. Balu CU, Daijo PO, Faizal KPS, Rinson TO, Salim J, Sigimon T, Mathew. Welding life enhancement of steel forging dies. Int J Adv Eng Glob Technol. 2016;4:1771–9.
22. Farhani M, Amadeh A, Kashani H, Saeed-Akbari A. The study of wear resistance of a hot forging die, hardfaced by a cobalt-base Superalloy. Mater Forum. 2006;30:212–8.
23. Kashani H, Amadeh A, Ghasemi HM. Room and high temperature wear behaviors of nickel and Cobalt base weld overlay coatings on hot forging dies. Wear. 2007;262:800–6. https://doi.org/10.1016/j.wear.2006.08.028.10.1016/j.wear.2006.08.028 ↗
24. Bayramoglu M, Polat H, Geren N. Cost and performance evaluation of different surface treated dies for hot forging process. J Mater Process Technol. 2008;205:394–403. https://doi.org/10.1016/j.jmatprotec.2007.11.256.10.1016/j.jmatprotec.2007.11.256 ↗
25. Ahn D-G, Lee H-J, Cho J-R, Guk D-S. Improvement of the wear resistance of hot forging dies using a locally selective deposition technology with transition layers. CIRP Ann. 2016;65:257–60. https://doi.org/10.1016/j.cirp.2016.04.013.10.1016/j.cirp.2016.04.013 ↗
26. Kim D-I, Jang Y-H, Lee H-J, Ahn D-G, Song H, Seok C-S. Design of overlay coated region with hardfacing, transition and damage diminution layers for the reduction of damages of hot forging tools. J Mech Sci Technol. 2017;31:5639–47. https://doi.org/10.1007/s12206-017-1104-2.10.1007/s12206-017-1104-2 ↗
27. Gao F, Zhou J, Zhou J, Shen L, Zhang J, Tao Y, Li M. Microstructure and properties of surfacing layers of dies manufactured by bimetal-gradient-layer surfacing technology before and after service. Int J Adv Manuf Technol. 2017;88:1289–97. https://doi.org/10.1007/s00170-016-8679-0.10.1007/s00170-016-8679-0 ↗
28. Shen L, Zhou J, Xiong Y-B, Zhang J-S, Meng Y. Analysis of service condition of large hot forging die and refabrication of die by bimetal-layer weld surfacing technology with a cobalt-based Superalloy and a ferrous alloy. J Manuf Process. 2018;31:731–43. https://doi.org/10.1016/j.jmapro.2018.01.005.10.1016/j.jmapro.2018.01.005 ↗
29. Junker D, Hentschel O, Schmidt M, Merklein M. Investigation of heat treatment strategies for additively-manufactured tools of X37CrMoV5-1. Metals. 2018;8:854. https://doi.org/10.3390/met8100854.10.3390/met8100854 ↗
30. Hentschel O, Siegel L, Scheitler C, Huber F, Junker D, Gorunow A, et al. Processing of AISI H11 tool steel powder modified with carbon black nanoparticles for the additive manufacturing of forging tools with tailored mechanical properties by means of laser metal deposition (LMD). Metals. 2018;8:659. https://doi.org/10.3390/met8090659.10.3390/met8090659 ↗
31. Wang S, Lu H, Shu F, Zhang X, Li G. Bonding mechanism between the AlN ceramic matrix and the copper-based metal cladding layer. Mater Sci-Poland. 2025;43:42–50. https://doi.org/10.2478/msp-2025-0004.10.2478/msp-2025-0004 ↗
32. Junker D, Hentschel O, Schramme R, Schmidt M, Merklein M. Performance of hot forging tools built by laser metal deposition of hot work tool steel X37CrMoV5-1. in: Lasers Manuf Conf, 2017: pp. 1–9.
33. Corbin S. Control of Laser Cladding Process. In: Laser Cladding. CRC Press; 2004. https://doi.org/10.1201/9781420039177.ch5.10.1201/9781420039177.ch5 ↗
34. Müller B, Hund R, Malek R, Gerth N. Laser Beam Melting for Tooling Applications – New Perspectives for Resource-Efficient Metal Forming and Die Casting Processes, in: 2013: pp. 124–137. https://doi.org/10.1007/978-3-642-41329-2_1410.1007/978-3-642-41329-2_14 ↗
35. Muller B, Gebauer M, Hund R, Malek R, Gerth N. Metal additive manufacturing for tooling applications - Laser beam melting technology increases efficiency of dies and molds. in: Met Addit Manuf Conf, 2014: pp. 1–14. http://publica.fraunhofer.de/dokumente/N-322053.html
36. Tang Z, Li W, Yang Z, Wang J. Effect of solution and artificial aging heat treatment on the hardness, friction and wear properties of laser cladding and roll-formed 18Ni300 materials. Mater Sci-Poland. 2024;42:26–40. https://doi.org/10.2478/msp-2024-0017.10.2478/msp-2024-0017 ↗
37. Samodurova MN, Chumanov IV, Anikeev AN, Shaburova NA, Pashkeev KY, Nurkenov AK, Zakirov RA, Latfulina YS. Restoration of die equipment by laser cladding using robotic complex FL-CLAD–R-4. Metallurgist. 2021;64:1086–95. https://doi.org/10.1007/s11015-021-01090-4.10.1007/s11015-021-01090-4 ↗
38. Wang J, Zhang B, Tang H, Wei X, Hao W, Wang J. Development of integrated automatic system of laser cladding for repairing of polycrystalline diamond compact bits. Electronics. 2023. https://doi.org/10.3390/electronics12040900.10.3390/electronics12040900 ↗
39. Yeo NCY, Pepin H, Yang SS. Revolutionizing technology adoption for the remanufacturing industry. Procedia CIRP. 2017;61:17–21. https://doi.org/10.1016/j.procir.2016.11.262.10.1016/j.procir.2016.11.262 ↗
40. Buchmayr B. Damage, lifetime, and repair of forging dies. BHM Berg- und Hüttenmänn Monatsch. 2017;162(3):88–93.10.1007/s00501-016-0566-3 ↗
41. Kaszuba MD, Widomski P, Kiełczawa T, Gronostajski Z. The use of a measuring arm with a laser scanner for analysis and support of regenerative surfacing processes of forging dies. Weld Tech Rev. 2020;92(3):23–32. https://doi.org/10.26628/wtr.v92i3.1103.10.26628/wtr.v92i3.1103 ↗
42. Lisiecka-Graca P, Lisiecki Ł, Zyguła K, Wojtaszek M. Evaluation of cracking risk of 80MnSi8-6 nanobainitic steel during hot forging in the range of lower temperature limits. Mater Science-Poland. 2024;42:171–85. https://doi.org/10.2478/msp-2024-0011.10.2478/msp-2024-0011 ↗
43. Kim J-D, Kim JW, Cheon JY, Kim Y-D, Ji C. Effect of shielding gases on the wire arc additive manufacturability of 5 cr–4 mo tool steel for die casting mold making. Korean J Met Mater. 2020;58(12):852–62. https://doi.org/10.3365/KJMM.2020.58.12.852.10.3365/KJMM.2020.58.12.852 ↗
44. Hackenhaar W, Mazzaferro JA, Mazzaferro CC, Grossi N, Campatelli G. Effects of different Waam current deposition modes on the mechanical properties of AISI h13 tool steel. Weld World. 2022;66(11):2259–69. https://doi.org/10.1007/s40194-022-01342-0.10.1007/s40194-022-01342-0 ↗
45. Tanvir ANM, Ahsan MR, Seo G, Bates B, Lee C, Liaw PK, Noakes M, Nycz A, Ji C, Kim DB. Phase stability and mechanical properties of wire + arc additively manufactured h13 tool steel at elevated temperatures. J Mater Sci Technol. 2021;67:80–94.10.1016/j.jmst.2020.04.085 ↗
46. Wang T, Zhang Y, Wu Z, Shi C. Microstructure and properties of die steel fabricated by WAAM using H13 wire. Vacuum. 2018;149:185–9. https://doi.org/10.1016/j.vacuum.2017.12.034.10.1016/j.vacuum.2017.12.034 ↗
47. Baffa F, Venturini G, Campatelli G, Galvanetto E. Effect of stepover and torch tilting angle on a repair process using WAAM. Adv Manuf. 2022;10(4):541–55. https://doi.org/10.1007/s40436-022-00393-2.10.1007/s40436-022-00393-2 ↗
48. Drozd K, Walczak M, Szala M, Gancarczyk K. Tribological behavior of AlCrSiN-coated tool steel K340 versus popular tool steel grades. Materials. 2020;13:4895. https://doi.org/10.3390/ma13214895.10.3390/ma13214895 ↗