journal article·2026-01-14

Influence of hot isostatic pressing on the microstructural and mechanical properties of Ti6Al4V produced via additive methods: laser powder bed fusion and cold spraying

Bartosz Bucholc, Anna Dobkowska, Barbara Romelczyk-Baishya, Monika Wieczorek-Czarnocka, Szymon Nosewicz, Kamil Kaszyca, Bogusława Adamczyk-Cieślak, Wojciech Żórawski, Zbigniew Pakieła, Rafał Zybała

Publisher page

Abstract

No abstract is available for this record. The assistant can identify its topic from the title, but cannot infer the study’s results.

Source: Not provided · Quality: missing

Research context

OpenAlex topics: Additive Manufacturing Materials and Processes · High-Temperature Coating Behaviors · Titanium Alloys Microstructure and Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (70)

Show source-provided references
1. J. C. Withers, “Fusion and/or solid state additive manufacturing for aerospace applications,” in Additive Manufacturing for the Aerospace Industry, Elsevier, 2019, pp. 187–211. https://doi.org/10.1016/B978-0-12-814062-8.00010-8.10.1016/B978-0-12-814062-8.00010-8 ↗
2. Yin S, Cavaliere P, Aldwell B, Jenkins R, Liao H, Li W, Lupoi R (2018) Cold spray additive manufacturing and repair: fundamentals and applications. Addit Manuf 21:628–650. https://doi.org/10.1016/j.addma.2018.04.01710.1016/j.addma.2018.04.017 ↗
3. Yap CY, Chua CK, Dong ZL, Liu ZH, Zhang DQ, Loh LE, Sing SL (2015) Review of selective laser melting: materials and applications. Appl Phys Rev 2(4):041101. https://doi.org/10.1063/1.493592610.1063/1.4935926 ↗
4. Zopp C, Blümer S, Schubert F, Kroll L (2017) Processing of a metastable titanium alloy (Ti-5553) by selective laser melting. Ain Shams Eng J 8(3):475–479. https://doi.org/10.1016/j.asej.2016.11.00410.1016/j.asej.2016.11.004 ↗
5. Fiocchi J, Tuissi A, Biffi CA (2021) Heat treatment of aluminium alloys produced by laser powder bed fusion: a review. Mater Des 204:109651. https://doi.org/10.1016/j.matdes.2021.10965110.1016/j.matdes.2021.109651 ↗
6. Huang J, Li M, Wang J, Pei Z, Mclntyre P, Ma C (2021) Selective laser melting of tungsten: effects of hatch distance and point distance on pore formation. J Manuf Process 61:296–302. https://doi.org/10.1016/j.jmapro.2020.11.03410.1016/j.jmapro.2020.11.034 ↗
7. Jadhav SD, Goossens LR, Kinds Y, Hooreweder BV, Vanmeensel K (2021) Laser-based powder bed fusion additive manufacturing of pure copper. Addit Manuf 42:101990. https://doi.org/10.1016/j.addma.2021.10199010.1016/j.addma.2021.101990 ↗
8. Grujicic M, Zhao CL, DeRosset WS, Helfritch D (2004) Adiabatic shear instability based mechanism for particles/substrate bonding in the cold-gas dynamic-spray process. Mater Des 25(8):681–688. https://doi.org/10.1016/j.matdes.2004.03.00810.1016/j.matdes.2004.03.008 ↗
9. Assadi H, Kreye H, Gärtner F, Klassen T (2016) Cold spraying – a materials perspective. Acta Mater 116:382–407. https://doi.org/10.1016/j.actamat.2016.06.03410.1016/j.actamat.2016.06.034 ↗
10. Jandaghi MR, Moverare J (2024) Exploring the efficiency of powder reusing as a sustainable approach for powder bed additive manufacturing of 316L stainless steel. Mater Des 244:113222. https://doi.org/10.1016/j.matdes.2024.11322210.1016/j.matdes.2024.113222 ↗
11. Jandaghi MR, Pouraliakbar H, Fallah V, Ghassemali E, Saboori A, Pavese M (2022) Additive manufacturing of nano-oxide decorated AlSi10Mg composites: a comparative study on Gd2O3 and Er2O3 additions. Mater Charact 192:112206. https://doi.org/10.1016/j.matchar.2022.11220610.1016/j.matchar.2022.112206 ↗
12. Yadroitsava I, Grewar S, Hattingh D, Yadroitsev I (2015) Residual stress in SLM Ti6Al4V alloy specimens. Mater Sci Forum 828–829:305–310. https://doi.org/10.4028/www.scientific.net/MSF.828-829.30510.4028/www.scientific.net/MSF.828-829.305 ↗
13. Leuders S, Thöne M, Riemer A, Niendorf T, Tröster T, Richard HA, Maier HJ (2013) On the mechanical behaviour of titanium alloy TiAl6V4 manufactured by selective laser melting: fatigue resistance and crack growth performance. Int J Fatigue 48:300–307. https://doi.org/10.1016/j.ijfatigue.2012.11.01110.1016/j.ijfatigue.2012.11.011 ↗
14. Alegre JM, Díaz A, García R, Peral LB, Cuesta II (2022) Effect of HIP post-processing at 850 °C/200 MPa in the fatigue behavior of Ti-6Al-4V alloy fabricated by selective laser melting. Int J Fatigue 163:107097. https://doi.org/10.1016/j.ijfatigue.2022.10709710.1016/j.ijfatigue.2022.107097 ↗
15. Qiu C, Adkins NJE, Attallah MM (2013) Microstructure and tensile properties of selectively laser-melted and of HIPed laser-melted Ti–6Al–4V. Mater Sci Eng A 578:230–239. https://doi.org/10.1016/j.msea.2013.04.09910.1016/j.msea.2013.04.099 ↗
16. Nosewicz S, Rojek J, Chmielewski M (2020) Discrete element framework for determination of sintering and postsintering residual stresses of particle reinforced composites. Materials 13(18):4015. https://doi.org/10.3390/ma1318401510.3390/ma13184015 ↗
17. Lee J, Ha H, Seol JB, Kim JG, Seo EH, Moon SK, Jung ID, Sung H (2021) Reverse effect of hot isostatic pressing on high-speed selective laser melted Ti–6Al–4V alloy. Mater Sci Eng A 807:140880. https://doi.org/10.1016/j.msea.2021.14088010.1016/j.msea.2021.140880 ↗
18. Eshawish N, Malinov S, Sha W, Walls P (2021) Microstructure and mechanical properties of Ti-6Al-4V manufactured by selective laser melting after stress relieving, hot isostatic pressing treatment, and post-heat treatment. J Materi Eng Perform 30(7):5290–5296. https://doi.org/10.1007/s11665-021-05753-w10.1007/s11665-021-05753-w ↗
19. Callister WD Jr (2020) Materials Science and Engineering: an introduction. Wiley
20. Bocanegra-Bernal MH (2004) Hot isostatic pressing (HIP) technology and its applications to metals and ceramics. J Mater Sci 39(21):6399–6420. https://doi.org/10.1023/B:JMSC.0000044878.11441.9010.1023/B:JMSC.0000044878.11441.90 ↗
21. F42 Committee, Standard for Additive Manufacturing Post Processing Methods Standard Specification for Thermal Post-Processing Metal Parts Made Via Powder Bed Fusion. https://doi.org/10.1520/F3301-18A.10.1520/F3301-18A ↗
22. Li W-Y, Zhang C, Guo X, Xu J, Li C-J, Liao H, Coddet C, Khor KA (2007) Ti and Ti‐6Al‐4V coatings by cold spraying and microstructure modification by heat treatment. Adv Eng Mater 9(5):418–423. https://doi.org/10.1002/adem.20070002210.1002/adem.200700022 ↗
23. Bhowmik A, Wei-Yee Tan A, Sun W, Wei Z, Marinescu I, Liu E (2020) On the heat-treatment induced evolution of residual stress and remarkable enhancement of adhesion strength of cold sprayed Ti–6Al–4V coatings. Results Mater 7:100119. https://doi.org/10.1016/j.rinma.2020.10011910.1016/j.rinma.2020.100119 ↗
24. Khun NW, Tan AWY, Sun W, Liu E (2017) Effect of heat treatment temperature on microstructure and mechanical and tribological properties of cold sprayed Ti-6Al-4V coatings. Tribol Trans 60(6):1033–1042. https://doi.org/10.1080/10402004.2016.124458410.1080/10402004.2016.1244584 ↗
25. Chen C, Xie Y, Yan X, Yin S, Fukanuma H, Huang R, Zhao R, Wang J, Ren Z, Liu M, Liao H (2019) Effect of hot isostatic pressing (HIP) on microstructure and mechanical properties of Ti6Al4V alloy fabricated by cold spray additive manufacturing. Addit Manuf 27:595–605. https://doi.org/10.1016/j.addma.2019.03.02810.1016/j.addma.2019.03.028 ↗
26. Petrovskiy P, Travyanov A, Cheverikin VV, Chereshneva AA, Sova A, Smurov I (2020) Effect of encapsulated hot isostatic pressing on properties of Ti6Al4V deposits produced by cold spray. Int J Adv Manuf Technol 107(1–2):437–449. https://doi.org/10.1007/s00170-020-05080-910.1007/s00170-020-05080-9 ↗
27. Boruah D, Zhang X, McNutt P, Khan R, Begg H (2022) Effect of post-deposition thermal treatments on tensile properties of cold sprayed Ti6Al4V. Metals 12(11):1908. https://doi.org/10.3390/met1211190810.3390/met12111908 ↗
28. Pantawane MV, Yang T, Jin Y, Joshi SS, Dasari S, Sharma A, Krokhin A, Srinivasan SG, Banerjee R, Neogi A, Dahotre NB (2021) Crystallographic texture dependent bulk anisotropic elastic response of additively manufactured Ti6Al4V. Sci Rep 11(1):633. https://doi.org/10.1038/s41598-020-80710-610.1038/s41598-020-80710-6 ↗
29. Chang K, Wang X, Liang E, Zhang R (2020) On the texture and mechanical property anisotropy of Ti6Al4V alloy fabricated by powder-bed based laser additive manufacturing. Vacuum 181:109732. https://doi.org/10.1016/j.vacuum.2020.10973210.1016/j.vacuum.2020.109732 ↗
30. Nosewicz S, Jurczak G, Chrominski W, Rojek J, Kaszyca K, Chmielewski M (2022) Combined EBSD and computer-assisted quantitative analysis of the impact of spark plasma sintering parameters on the structure of porous materials. Metall Mater Trans A 53(11):4101–4125. https://doi.org/10.1007/s11661-022-06821-z10.1007/s11661-022-06821-z ↗
31. Mishurova T, Evsevleev S, Piault P, King A, Henry L, Bruno G (2023) Understanding the hot isostatic pressing effectiveness of laser powder bed fusion Ti-6Al-4V by in-situ X-ray imaging and diffraction experiments. Sci Rep 13(1):18433. https://doi.org/10.1038/s41598-023-45258-110.1038/s41598-023-45258-1 ↗
32. Majchrowicz K, Pakieła Z, Brynk T, Romelczyk-Baishya B, Płocińska M, Kurzynowski T, Chlebus E (2019) Microstructure and mechanical properties of Ti–Re alloys manufactured by selective laser melting. Mater Sci Eng, A 765:138290. https://doi.org/10.1016/j.msea.2019.13829010.1016/j.msea.2019.138290 ↗
33. Peters WH, Ranson WF (1982) Digital imaging techniques in experimental stress analysis. Opt Eng. https://doi.org/10.1117/12.797292510.1117/12.7972925 ↗
34. Swift HW (1952) Plastic instability under plane stress. J Mech Phys Solids 1(1):1–18. https://doi.org/10.1016/0022-5096(52)90002-110.1016/0022-5096(52)90002-1 ↗
35. Fernandes J (1998) A modified swift law for prestrained materials. Int J Plast 14(6):537–550. https://doi.org/10.1016/S0749-6419(98)00027-810.1016/S0749-6419(98)00027-8 ↗
36. Virtanen P et al (2020) SciPy 1.0: fundamental algorithms for scientific computing in Python. Nat Methods 17(3):261–272. https://doi.org/10.1038/s41592-019-0686-210.1038/s41592-019-0686-2 ↗
37. Lakroune Y, Connétable D, Hugues J, Hermantier P, Barriobero-Vila P, Dehmas M (2023) Microstructural evolution during post heat treatment of the Ti–6Al–4V alloy manufactured by laser powder bed fusion. J Market Res 23:1980–1994. https://doi.org/10.1016/j.jmrt.2023.01.12310.1016/j.jmrt.2023.01.123 ↗
38. Rautio T, Hamada A, Mäkikangas J, Jaskari M, Järvenpää A (2020) Laser welding of selective laser melted Ti6Al4V: Microstructure and mechanical properties. Mater Today: Proc 28:907–911. https://doi.org/10.1016/j.matpr.2019.12.32210.1016/j.matpr.2019.12.322 ↗
39. Pathania A, Subramaniyan AK, Nagesha BK (2022) Influence of post-heat treatments on microstructural and mechanical properties of LPBF-processed Ti6Al4V alloy. Prog Addit Manuf 7(6):1323–1343. https://doi.org/10.1007/s40964-022-00306-610.1007/s40964-022-00306-6 ↗
40. Lu H, Deng W, Luo K, Chen Y, Wang J, Lu J (2023) Tailoring microstructure of additively manufactured Ti6Al4V titanium alloy using hybrid additive manufacturing technology. Addit Manuf 63:103416. https://doi.org/10.1016/j.addma.2023.10341610.1016/j.addma.2023.103416 ↗
41. Cao S, Chu R, Zhou X, Yang K, Jia Q, Lim CVS, Huang A, Wu X (2018) Role of martensite decomposition in tensile properties of selective laser melted Ti-6Al-4V. J Alloy Compd 744:357–363. https://doi.org/10.1016/j.jallcom.2018.02.11110.1016/j.jallcom.2018.02.111 ↗
42. Tsai M-T, Chen Y-W, Chao C-Y, Jang JSC, Tsai C-C, Su Y-L, Kuo C-N (2020) Heat-treatment effects on mechanical properties and microstructure evolution of Ti-6Al-4V alloy fabricated by laser powder bed fusion. J Alloy Compd 816:152615. https://doi.org/10.1016/j.jallcom.2019.15261510.1016/j.jallcom.2019.152615 ↗
43. Kaschel FR, Vijayaraghavan RK, Shmeliov A, McCarthy EK, Canavan M, McNally PJ, Dowling DP, Nicolosi V, Celikin M (2020) Mechanism of stress relaxation and phase transformation in additively manufactured Ti-6Al-4V via in situ high temperature XRD and TEM analyses. Acta Mater 188:720–732. https://doi.org/10.1016/j.actamat.2020.02.05610.1016/j.actamat.2020.02.056 ↗
44. Kenel C, Grolimund D, Li X, Panepucci E, Samson VA, Sanchez DF, Marone F, Leinenbach C (2017) In situ investigation of phase transformations in Ti-6Al-4V under additive manufacturing conditions combining laser melting and high-speed micro-X-ray diffraction. Sci Rep 7(1):16358. https://doi.org/10.1038/s41598-017-16760-010.1038/s41598-017-16760-0 ↗
45. Buhairi MA, Foudzi FM, Jamhari FI, Sulong AB, Radzuan NAM, Muhamad N, Mohamed IF, Azman AH, Harun WSW, Al-Furjan MSH (2023) Review on volumetric energy density: influence on morphology and mechanical properties of Ti6Al4V manufactured via laser powder bed fusion. Prog Addit Manuf 8(2):265–283. https://doi.org/10.1007/s40964-022-00328-010.1007/s40964-022-00328-0 ↗
46. Wang H, Chao Q, Yang L, Cabral M, Song ZZ, Wang BY, Primig S, Xu W, Chen ZB, Ringer SP, Liao XZ (2021) Introducing transformation twins in titanium alloys: an evolution of α-variants during additive manufacturing. Mater Res Lett 9(3):119–126. https://doi.org/10.1080/21663831.2020.185053610.1080/21663831.2020.1850536 ↗
47. Zhao X, Li S, Zhang M, Liu Y, Sercombe TB, Wang S, Hao Y, Yang R, Murr LE (2016) Comparison of the microstructures and mechanical properties of Ti–6Al–4V fabricated by selective laser melting and electron beam melting. Mater Des 95:21–31. https://doi.org/10.1016/j.matdes.2015.12.13510.1016/j.matdes.2015.12.135 ↗
48. Nudelis N, Mayr P (2023) Pore tracing in additive manufactured and hot isostatic pressed components. J Mater Sci 58(35):14245–14253. https://doi.org/10.1007/s10853-023-08907-410.1007/s10853-023-08907-4 ↗
49. Louvis E, Fox P, Sutcliffe CJ (2011) Selective laser melting of aluminium components. J Mater Process Technol 211(2):275–284. https://doi.org/10.1016/j.jmatprotec.2010.09.01910.1016/j.jmatprotec.2010.09.019 ↗
50. Yan X, Yue S, Ge J, Chen C, Lupoi R, Yin S (2022) Microstructural and mechanical optimization of selective laser melted Ti6Al4V lattices: effect of hot isostatic pressing. J Manuf Process 77:151–162. https://doi.org/10.1016/j.jmapro.2022.02.02410.1016/j.jmapro.2022.02.024 ↗
51. Nosewicz S, Rojek J, Chmielewski M, Pietrzak K (2017) Discrete element modeling and experimental investigation of hot pressing of intermetallic NiAl powder. Adv Powder Technol 28(7):1745–1759. https://doi.org/10.1016/j.apt.2017.04.01210.1016/j.apt.2017.04.012 ↗
52. Nosewicz S, Rojek J, Wawrzyk K, Kowalczyk P, Maciejewski G, Maździarz M (2019) Multiscale modeling of pressure-assisted sintering. Comput Mater Sci 156:385–395. https://doi.org/10.1016/j.commatsci.2018.10.00110.1016/j.commatsci.2018.10.001 ↗
53. Porter DA (2009) Phase transformations in metals and alloys, 3rd edn. CRC Press, Boca Raton, FL
54. R. M. German, Sintering theory and practice. in A Wiley interscience publication. New York Chichester: Wiley, 1996.
55. R. M. German, “Microstructure Coarsening,” in Sintering: from Empirical Observations to Scientific Principles, Elsevier, 2014, pp. 227–246. https://doi.org/10.1016/B978-0-12-401682-8.00008-2.10.1016/B978-0-12-401682-8.00008-2 ↗
56. Gloaguen D, Girault B, Courant B, Dubos P-A, Moya M-J, Edy F, Rebelo Kornmeier J (2020) Study of residual stresses in additively manufactured Ti-6Al-4V by neutron diffraction measurements. Metall Mater Trans A 51(2):951–961. https://doi.org/10.1007/s11661-019-05538-w10.1007/s11661-019-05538-w ↗
57. Kaoushik VM, Nichul U, Chavan V, Hiwarkar V (2023) Development of microstructure and high hardness of Ti6Al4V alloy fabricated using laser beam powder bed fusion: a novel sub-transus heat treatment approach. J Alloy Compd 937:168387. https://doi.org/10.1016/j.jallcom.2022.16838710.1016/j.jallcom.2022.168387 ↗
58. Strantza M, Ganeriwala RK, Clausen B, Phan TQ, Levine LE, Pagan D, King WE, Hodge NE, Brown DW (2018) Coupled experimental and computational study of residual stresses in additively manufactured Ti-6Al-4V components. Mater Lett 231:221–224. https://doi.org/10.1016/j.matlet.2018.07.14110.1016/j.matlet.2018.07.141 ↗
59. Kasperovich G, Hausmann J (2015) Improvement of fatigue resistance and ductility of TiAl6V4 processed by selective laser melting. J Mater Process Technol 220:202–214. https://doi.org/10.1016/j.jmatprotec.2015.01.02510.1016/j.jmatprotec.2015.01.025 ↗
60. Benedetti M, Torresani E, Leoni M, Fontanari V, Bandini M, Pederzolli C, Potrich C (2017) The effect of post-sintering treatments on the fatigue and biological behavior of Ti-6Al-4V ELI parts made by selective laser melting. J Mech Behav Biomed Mater 71:295–306. https://doi.org/10.1016/j.jmbbm.2017.03.02410.1016/j.jmbbm.2017.03.024 ↗
61. A. Cutolo, C. Elangeswaran, C. De Formanoir, G. K. Muralidharan, and B. Van Hooreweder, “Effect of Heat Treatments on Fatigue Properties of Ti–6Al–4V and 316L Produced by Laser Powder Bed Fusion in As-Built Surface Condition,” in TMS 2019 148th Annual Meeting & Exhibition Supplemental Proceedings, The Minerals, Metals & Materials Series, Ed., in The Minerals, Metals & Materials Series. , Cham: Springer International Publishing, 2019, pp. 395–405. https://doi.org/10.1007/978-3-030-05861-6_36.10.1007/978-3-030-05861-6_36 ↗
62. Roudnicka M, Mertova K, Vojtech D (2019) Influence of hot isostatic pressing on mechanical response of as-built SLM titanium alloy. IOP Conf Ser: Mater Sci Eng 629(1):012034. https://doi.org/10.1088/1757-899X/629/1/01203410.1088/1757-899X/629/1/012034 ↗
63. Rosenthal I, Stern A, Frage N (2017) Strain rate sensitivity and fracture mechanism of AlSi10Mg parts produced by Selective Laser Melting. Mater Sci Eng A 682:509–517. https://doi.org/10.1016/j.msea.2016.11.07010.1016/j.msea.2016.11.070 ↗
64. Shifeng W, Shuai L, Qingsong W, Yan C, Sheng Z, Yusheng S (2014) Effect of molten pool boundaries on the mechanical properties of selective laser melting parts. J Mater Process Technol 214(11):2660–2667. https://doi.org/10.1016/j.jmatprotec.2014.06.00210.1016/j.jmatprotec.2014.06.002 ↗
65. Ghelichi R, Bagherifard S, MacDonald D, Fernandez-Pariente I, Jodoin B, Guagliano M (2014) Experimental and numerical study of residual stress evolution in cold spray coating. Appl Surf Sci 288:26–33. https://doi.org/10.1016/j.apsusc.2013.09.07410.1016/j.apsusc.2013.09.074 ↗
66. Zhou H, Li Z, Wei X, Li X (2024) Effect of particle deposition location on interface bonding during cold spraying. Powder Technol 448:120355. https://doi.org/10.1016/j.powtec.2024.12035510.1016/j.powtec.2024.120355 ↗
67. Vandadi M, Bond T, Asumadu TK, Klenam D, Rahbar N, Soboyejo W (2025) Effect of nanoscale surface oxide layers on the cold spray of commercially pure titanium and Ti–6Al–4V powders. Comput Mater Sci 246:113454. https://doi.org/10.1016/j.commatsci.2024.11345410.1016/j.commatsci.2024.113454 ↗
68. Stoltenhoff T, Borchers C, Gärtner F, Kreye H (2006) Microstructures and key properties of cold-sprayed and thermally sprayed copper coatings. Surf Coat Technol 200(16–17):4947–4960. https://doi.org/10.1016/j.surfcoat.2005.05.01110.1016/j.surfcoat.2005.05.011 ↗
69. Li W-Y, Zhang C, Wang H-T, Guo XP, Liao HL, Li C-J, Coddet C (2007) Significant influences of metal reactivity and oxide films at particle surfaces on coating microstructure in cold spraying. Appl Surf Sci 253(7):3557–3562. https://doi.org/10.1016/j.apsusc.2006.07.06310.1016/j.apsusc.2006.07.063 ↗
70. Wysocki B, Maj P, Sitek R, Buhagiar J, Kurzydłowski K, Święszkowski W (2017) Laser and electron beam additive manufacturing methods of fabricating titanium bone implants. Appl Sci 7(7):657. https://doi.org/10.3390/app707065710.3390/app7070657 ↗