Specimen size effect on fracture toughness of Pyrowear 53 steel for planetary gears
Source abstract
Abstract
Abstract A fracture toughness is one of the critical parameters for Pyrowear 53 steel which is widely used in planetary gears of aircraft vehicles. Due to a limited volume of planetary gears, it is impossible to directly assess their plain strain fracture toughness K Ic . Therefore, the main aim of this study was to determine a formula correlating the plain strain fracture toughness K Ic obtained for laboratory compact tension (CT) specimens having a thickness of B = 50 mm with smaller specimens (B = 10 mm) which can be prepared directly from planetary gears. For this reason, different force-based approaches were utilized considering conditional fracture toughness (K Q ), size-insensitive conditional fracture toughness (K Qsi ) and specimen strength ratio (R sc ) values calculated according to ASTM E399 standard. Four different sizes of CT specimens were analyzed, i.e. B = 50, 25, 16 and 10 mm. The K IC value obtained for the B = 50 mm specimen was 101.7 ± 4.5 MPa m 1/2 , while for the smaller specimen sizes, the K Q value gradually decreased from 125.4 ± 10.0 MPa m 1/2 for B = 25 mm to 101.1 ± 3.0 and 86.6 ± 1.3 MPa m 1/2 for B = 16 and 10 mm, respectively. This trend was opposite to the commonly observed relation that the fracture toughness value increases for smaller specimen size with a higher plain stress region. The specimen size effect observed in the current work resulted from the methodology of determining the K Q value based on a force P Q defined at a point of 5% deviation from linearity of load-displacement curve. It has been shown that the fracture toughness of the Pyrowear 53 steel specimens exhibiting a rising R curve was more dependent on a ligament size.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Fatigue and fracture mechanics · Metal Forming Simulation Techniques · Engineering and Material Science Research
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (37)
Show source-provided references
1. Ferguson BL, Freborg AM, Li Z. Residual stress and bending fatigue strength in carburized and quench hardened Pyrowear 53 steel gears. Proc 23rd Int Fed Heat Treat Surf Eng Congr. 2016;2016:374-81.
2. Korecki M, Wolowiec-Korecka E, Bazel M, Slut M, Kreuzaler TD. Outstanding hardening of Pyrowear® alloy 53 with low pressure carburizing, Tech. Contrib. to 70° Congr. Brazil: Anu. Da ABM, Rio Janeiro; 2015. pp. 17–21.
3. Peng T, Cao J-C, Zhao J-Q, Yang G. Cu precipitation strengthening in AMS 6308 steel. Cailiao Rechuli Xuebao / Trans Mater Heat Treat. 2016;37:126–30.
4. Wojtyczka A, Iżowski B. Microstructure and hardness of Pyrowear 53 steel after low-pressure vacuum carburizing at 921°C. Adv Manuf Sci Technol. 2020;44:109–12. https://doi.org/10.2478/amst-2019-0020.10.2478/amst-2019-0020 ↗
5. ASTM E399 - Standard Test Method for Linear-Elastic. Plane-Strain Fracture Toughness of Metallic Materials, 2020.
6. Wallin K. The size effect in KIC results. Eng Fract Mech. 1985;22:149–63.10.1016/0013-7944(85)90167-5 ↗
7. Jones MH, Brown WF. The influence of crack length and thickness in plane strain fracture toughness testing. ASTM STP. 1970;463:63–101.
8. Rolfe ST, Novak SR. Slow-bend testing of medium-strength high-toughness steels, ASTM STP. 463 (1970) 124–59.10.1520/STP33665S ↗
9. Anderson TL. Fracture mechanics - fundamentals and applications. Third Edit, Taylor & Francis; 2005.10.1201/9781420058215 ↗
10. Mourad AHI, El-Domiaty A, Chao YJ. Fracture toughness prediction of low alloy steel as a function of specimen Notch root radius and size constraints. Eng Fract Mech. 2013;103:79–93. https://doi.org/10.1016/j.engfracmech.2012.05.010.10.1016/j.engfracmech.2012.05.010 ↗
11. Alcaraz-Caracheo LA, Terán-Guillén J, Carrión-Viramontes FJ, Martínez-Madrid M. Correlation between specimen size and fracture toughness of 1Cr-½Ni cast steel used in the anchorage of a Cable-Stayed Bridge. Cientifica. 2012;16:135–43.
12. Ono H, Kasada R, Kimura A. Specimen size effects on fracture toughness of JLF-1 reduced-activation ferritic steel. 2004;329–33. https://doi.org/10.1016/j.jnucmat.2004.04.034.10.1016/j.jnucmat.2004.04.034 ↗
13. Kaufman JG. F.G. <>Nelson 1973 More on specimen size effects in fracture toughness testing. ASTM STP 559 74–98.
14. Wallin K. Critical Assessment of the Standard E399, ASTM STP. 1461 (2004) 433–453.10.1520/STP11510S ↗
15. Wells DN, James MA, Allen PA, Wallin KRW. A review of the proposed KIsi Offset-Secant method for Size-Independent Linear-Elastic toughness evaluation. Mater Perform Charact. 2018;7:1–14.10.1520/MPC20170151 ↗
16. Tilson WG. ASTM E399 Standard Development - KIsi Analysis Method, (2019).
17. Munz D, Galda KH, Link F. Effect of specimen size on fracture toughness of a titanium alloy. ASTM STP. 1976;590:219–34.
18. ASTM E1820. - Standard Test Method for Measurement of Fracture Toughness, 2020.
19. AMS6308G - Steel. Bars and Forgings and Forging Stock 0.90Si – 1.0Cr – 2.0Ni – 3.2Mo – 2.0Cu – 0.10V (0.07–0.13 C). Vacuum Arc of Electroslag Remelted; 2023.
20. Filip R, Ochał K, Gancarczyk K, Nowak WJ, Kościelniak B, Wierzba B. Characteristics of impulse carburization LPC process. Mater (Basel). 2021;14:4269. https://doi.org/10.3390/ma14154269.10.3390/ma14154269 ↗
21. ISO 6892-1 - Metallic materials - Tensile testing - Part 1: Method of test at room temperature, 2019.
22. Majchrowicz K, Romelczyk-Baishya B, Wieczorek-Czarnocka M, Dobkowska A, Raga K, Filip R, Pakieła Z. Determination of the fracture toughness of carburized Pyrowear 53 steel for planetary gears by the small punch test method. Arch Civ Mech Eng. 2024;24:177. https://doi.org/10.1007/s43452-024-00992-9.10.1007/s43452-024-00992-9 ↗
23. ASTM E561. - Standard Test Method for KR Curve Determination, 2020.
24. ASTM E399 - Standard Test Method for Linear-Elastic. Plane-Strain Fracture Toughness of Metallic Materials, 1997.
25. Server WL, Wullaert RA. The use of small specimen strength ratio for measuring fracture toughness. Eng Fract Mech. 1979;11:477–86.10.1016/0013-7944(79)90072-9 ↗
26. Asi O. Fatigue failure of a helical gear in a gearbox. Eng Fail Anal. 2006;13:1116–25. https://doi.org/10.1016/j.engfailanal.2005.07.020.10.1016/j.engfailanal.2005.07.020 ↗
27. SAE J1619. - Single Tooth Gear Bending Fatigue Test, 2017.
28. Chen Z, Shao Y. Dynamic simulation of planetary gear with tooth root crack in ring gear. Eng Fail Anal. 2013;31:8–18. https://doi.org/10.1016/j.engfailanal.2013.01.012.10.1016/j.engfailanal.2013.01.012 ↗
29. Stringer DB, Dykas BD, LaBerge KE, Zakrajsek AJ, Handschuh RF. A new high-speed, high-cycle, gear-tooth bending fatigue test capability, in: 67th annu. Forum Technol Disp, 2011;217039.
30. Chen Z, Shao Y. Dynamic simulation of spur gear with tooth root crack propagating along tooth width and crack depth. Eng Fail Anal. 2011;18:2149–64. https://doi.org/10.1016/j.engfailanal.2011.07.006.10.1016/j.engfailanal.2011.07.006 ↗
31. Morrison WB. Influence of testing direction on the mechanical properties of wrought steel. Met Technol. 1975;2:33–41.10.1179/030716975803277636 ↗
32. Das A, Viehrig HW, Bergner F, Heintze C, Altstadt E, Hoffmann J. Effect of microstructural anisotropy on fracture toughness of hot rolled 13Cr ODS steel – The role of primary and secondary cracking. J Nucl Mater. 2017;491:83–93. https://doi.org/10.1016/j.jnucmat.2017.04.059.10.1016/j.jnucmat.2017.04.059 ↗
33. Zhang XZ, Knott JF. Cleavage fracture in bainitic and martensitic microstructures. Acta Mater. 1999;47:3483–95.10.1016/S1359-6454(99)00200-1 ↗
34. Tomita Y. Effect of microstructure on plane-strain fracture toughness of AISI 4340 steel. Metall Trans Phys Metall Mater Sci. 1988;19 A:2513–21.10.1007/BF02645479 ↗
35. Iżowski B, Wojtyczka A, Motyka M. Numerical simulation of low-pressure carburizing and gas quenching for Pyrowear 53 steel. Met (Basel). 2023;13:371. https://doi.org/10.3390/met13020371.10.3390/met13020371 ↗
36. Freborg AM. Investigating and understanding the role of transformation induced residual stress to increase fatigue life of high strength steel used in transmission gears, PhD Thesis, University of Akron, OH, USA, 2013.
37. Takahashi M, Bhadeshia HKDH. Model for transition from upper to lower bainite. Mater Sci Technol. 1990;6:592–603. https://doi.org/10.1179/mst.1990.6.7.592.10.1179/mst.1990.6.7.592 ↗