journal article·2025-11-05Open access

Antipathogenic electroless copper–titania composite coatings: tailoring the plating process toward better corrosion resistance

Monika Bugajska, Izabella Kwiecien, Marta Janusz-Skuza, Agnieszka Bigos, Maciej Szczerba, Anna Wierzbicka-Miernik, Andrzej Misztela, Aneta Dyner, Marcin Dyner, Deyan Veselinov, Hristo Skulev, Joanna Wojewoda-Budka

Abstract

Abstract Copper coatings production increases due to the society awareness of their great anti-pathogenic properties. However, such coatings must show a set of requirements among which the corrosion resistance plays a key role. This study focused on determining the corrosion resistance of newly designed copper-titania composite coatings enriched with TiO 2 nanoparticles. The series of Cu-TiO 2 coatings have been produced using electroless plating process and different NiSO 4 ·7H 2 O concentration in the bath solution. Composite and copper coatings were examined by Scanning Electron Microscopy and tested using potentiodynamic measurements and Electrochemical Impedance Spectroscopy. Scanning Electron Microscopy observations revealed that both Cu and Cu-TiO 2 coatings exhibit globular morphology without porosity. Electron microscopy analyses confirmed that titania nanoparticles has been incorporated into the copper matrix of composite coatings and also that the grain size of copper coatings and composite, produced under the same plating conditions, is identical. X-ray diffraction showed the highest nickel intensity at the lowest NiSO 4 concentration, indicating its impact on coating thickness. Corrosion studies confirmed that copper-titania coatings also may offer the corrosion protection.
Source: crossref · Quality: baseline

Research context

OpenAlex topics: Electrodeposition and Electroless Coatings · Corrosion Behavior and Inhibition · Hydrogen embrittlement and corrosion behaviors in metals

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (41)

Show source-provided references
1. Makhlouf ASH. Current and advanced coating technologies for industrial applications. Nanocoatings Ultra-Thin Films. 2011;3–23. https://doi.org/10.1533/9780857094902.1.3.10.1533/9780857094902.1.3 ↗
2. Emamverdian AA, Sun Y, Cao C, Pruncu C, Wang Y. Current failure mechanisms and treatment methods of hot forging tools (dies) - a review. Eng Fail Anal. 2021;129:105678.10.1016/j.engfailanal.2021.105678 ↗
3. Dini JW, Snyder DD. Electrodeposition of copper. Mod Electroplating. 2011;33–78. https://doi.org/10.1002/9780470602638.ch2.10.1002/9780470602638.ch2 ↗
4. Ghosh S. Electroless copper deposition: A critical review. Thin Solid Films. 2019;669:641–58. https://doi.org/10.1016/j.tsf.2018.11.016.10.1016/j.tsf.2018.11.016 ↗
5. Bigos A, Bugajska M, Kwiecien I, et al. Antipathogenic copper coatings: electrodeposition process and microstructure analysis. Archiv Civ Mech Eng. 2023;23:233. https://doi.org/10.1007/s43452-023-00772-x.10.1007/s43452-023-00772-x ↗
6. Paunovic M. Electroless deposition of copper. Mod Electroplating. 2011;433–46. https://doi.org/10.1002/9780470602638.ch17.10.1002/9780470602638.ch17 ↗
7. Kwiecien I, Bigos A, Janusz-Skuza M, Szczerba M, Bugajska M, Wierzbicka-Miernik A, Dyner M, Misztela A, Veselinov D, Skulev H, Wojewoda-Budka J. Electroless plating process optimization for successful copper coatings deposition on surgical tools. Arch Metall Mater. 2025;3/25:70. https://doi.org/10.24425/amm.2025.154488.10.24425/amm.2025.154488 ↗
8. Ferreira E, Giacomelli C, Giacomelli F, Spinelli A. Evaluation of the inhibitor effect of l-ascorbic acid on the corrosion of mild steel. Mater Chem Phys. 2004;83(1):129–34. https://doi.org/10.1016/j.matchemphys.2003.09.10.1016/j.matchemphys.2003.09 ↗
9. Monticelli C. Corrosion Inhibitors. In book: Reference Module in Chemistry, Molecular Sciences and Chemical Engineering. 2017. https://doi.org/10.1016/b978-0-12-409547-2.13443-210.1016/b978-0-12-409547-2.13443-2 ↗
10. Abbas M, Dardeir A, Mohamed AMA, Ahmed. Essam. Corrosion Inhibition of AISI 1020 steel in 3% NaCl solution using some environmentally friendly inhibitors. Shanghai Ligong Daxue Xuebao/Journal Univ Shanghai Sci Technol. 2022;23:867–77. https://doi.org/10.51201/jusst/2110846.10.51201/jusst/2110846 ↗
11. Kannan K, Radhika D, Sadasivuni KK, Reddy KR, Raghu AV. Nanostructured metal oxides and its hybrids for photocatalytic and biomedical applications. Adv Colloid Interface Sci. 2020;281:102178.10.1016/j.cis.2020.102178 ↗
12. Ziental D, Czarczynska-Goslinska B, Mlynarczyk DT, Glowacka-Sobotta A, Stanisz B, Goslinski T, Sobotta L. Titanium dioxide nanoparticles: prospects and applications in medicine. Nanomaterials (Basel Switzerland). 2020;10(2):387. https://doi.org/10.3390/nano10020387.10.3390/nano10020387 ↗
13. Wang Y, Lu X, Yuan N, Ding J. A novel nickel-copper alternating-deposition coating with excellent tribological and antibacterial property. J Alloys Compd. 2020;849:156222.10.1016/j.jallcom.2020.156222 ↗
14. Erdural BK, Yurum A, Bakir U, Karakas G. Antimicrobial properties of titanium nanoparticles. Functionalized Nanoscale Mater Devices Syst. 2008;409–14. https://doi.org/10.1007/978-1-4020-8903-9_40.10.1007/978-1-4020-8903-9_40 ↗
15. Shirai R, Miura T, Yoshida A, Yoshino F, Ito T, Yoshinari M, Yajima Y. Antimicrobial effect of titanium dioxide after ultraviolet irradiation against periodontal pathogen. Dent Mater J. 2016;35(3):511–6. https://doi.org/10.4012/dmj.2015-406.10.4012/dmj.2015-406 ↗
16. Ahmed B, El-Sherbini E-S, El-sayed G, Eladl M, Taniguchi A. Akiyoshi. Applications of titanium dioxide nanoparticles in nanomedicine. Mansoura Veterinary Medical Journal. 2020; Vol. 22: Iss. 3, Article 3. https://doi.org/10.21608/mvmj.2021.19603610.21608/mvmj.2021.196036 ↗
17. Tajik S, Beitollahi H, Dourandish Z, Jahani PM, Sheikhshoaie I, Askari MB, Salarizadeh P, Nejad FG, Kim D, Kim SY, Varma RS, Shokouhimehr M. Applications of Non- precious transition metal oxide nanoparticles in electrochemistry. Electroanalysis. 2022;34(7):1065–91. https://doi.org/10.1021/acsanm.4c02000.10.1021/acsanm.4c02000 ↗
18. Shao W, et al. Mechanical and corrosion resistance properties of TiO2 nanoparticles reinforced Ni coating by electrodeposition. IOP Conf Ser : Mater Sci Eng. 2012;40:012043.10.1088/1757-899X/40/1/012043 ↗
19. Veselinov D, Skulev H, Yankova R, Ivanov S, Moriarty TF, Gueorguiev B. Enhancing antibacterial performance: Structure, phase Composition, and microroughness of selective plated copper coatings on Medical-Grade stainless steel 1.4021 and nickel alloy Ni200. Appl Sci. 2023;13:9840. https://doi.org/10.3390/app13179840.10.3390/app13179840 ↗
20. Jafari S, Mahyad B, Hashemzadeh H, Janfaza S, Gholikhani T, Tayebi L. Biomedical applications of TiO2 nanostructures: recent advances. Int J Nanomed. 2020;15:3447–70. https://doi.org/10.2147/IJN.S249441.10.2147/IJN.S249441 ↗
21. Ma Y, Liu BFH, Hao GFH. Enhanced corrosion Inhibition of aniline derivatives electropolymerized coatings on copper: Preparation, characterization and mechanism modeling. Appl Surf Sci. 2020;514:146086.10.1016/j.apsusc.2020.146086 ↗
22. Yashwardhan Deo S, Guha K, Sarkar P, Mohanta. Debabrata Pradhan. Electrodeposited Ni-Cu alloy coatings on mild steel for enhanced corrosion properties. Appl Surf Sci. 2020;515:146078.10.1016/j.apsusc.2020.146078 ↗
23. da Silva FS, Cinca N, Dosta S, Cano IG, Guilemany JM, Caires CSA, Lima AR, Silva CM, Oliveira SL, Caires ARL. Benedetti A.V. Corrosion resistance and antibacterial properties of copper coating deposited by cold gas spray. Surf Coat Technol. 2019;361:292–301.10.1016/j.surfcoat.2019.01.029 ↗
24. Buchtík M, Doskočil L, Brescher R, Doležal P, Másilko J, Wasserbauer J. The effect of crystallization and phase transformation on the mechanical and electrochemical corrosion properties of Ni-P coatings. Coatings. 2021;11:447. https://doi.org/10.3390/COATINGS11040447.10.3390/COATINGS11040447 ↗
25. Ashassi-Sorkhabi H, Rafizadeh SH. Effect of coating time and heat treatment on structures and corrosion characteristics of electroless Ni–P alloy deposits. Surf Coat Technol. 2004;176:318–26. https://doi.org/10.1016/S0257-8972(03)00746-1.10.1016/S0257-8972(03)00746-1 ↗
26. Lu G, Zangari G. Corrosion resistance of ternary Ni-P based alloys in sulfuric acid solutions. Electrochim Acta. 2002;47:2969–79. https://doi.org/10.1016/S0013-4686(02)00198-6.10.1016/S0013-4686(02)00198-6 ↗
27. Wang J, Lin Z. Anodic formation of ordered TiO2 nanotube arrays: effects of electrolyte temperature and anodization potential. Phys Chem C. 2009;113:4026–30.10.1021/jp811201x ↗
28. Macak JM, Tsuchiya H, Ghicov A, Yasuda K, Hahn R, Bauer S, Schmuki P. TiO2 nanotubes: self-organized electrochemical formation, properties and applications. Curr Opin Solid State Mater Sci. 2007;11:3–18.10.1016/j.cossms.2007.08.004 ↗
29. Papavinasam S. Electrochemical polarization techniques for corrosion monitoring. Techniques Corros Monit. 2008;49–85. https://doi.org/10.1533/9781845694050.1.4.10.1533/9781845694050.1.4 ↗
30. Nady H, El-Rabiei MM, Samy M. Corrosion behavior and electrochemical properties of carbon steel, commercial pure titanium, copper and copper–aluminum–nickel alloy in 3.5% sodium chloride containing sulfide ions. Egyptian J Petroleum. 2017;26(1):79–94. https://doi.org/10.1016/j.ejpe.2016.02.008.10.1016/j.ejpe.2016.02.008 ↗
31. Lethabane ML, Olubambi PA, Chikwanda HK. Corrosion behaviour of sintered Ti–Ni–Cu–Nb in 0.9% NaCl environment. J Mater Res Technol. 2015;4(4):367–76. https://doi.org/10.1016/j.jmrt.2015.04.006.10.1016/j.jmrt.2015.04.006 ↗
32. Guo M, Daub K, Dong Q, Long F, Binns WJ, Daymond MR, Shoesmith DV, Noël JJ, Persaud SY. The Early-Stage corrosion of copper materials in chloride and sulfide solutions: nanoscale characterization and the effect of microstructure. J Electrochem Soc. 2022;169(3):031509. https://doi.org/10.1149/1945-7111/ac4bf4.10.1149/1945-7111/ac4bf4 ↗
33. Benzarti Z, Arrousse N, Serra R, Cruz S, Bastos AC, Tedim J, Salgueiro R, Cavaleiro A, Carvalho S. Copper corrosion mechanisms, influencing factors, and mitigation strategies for water circuits of heat exchangers: critical review and current advances. Corros Rev. 2024. https://doi.org/10.1515/corrrev-2024-0001.10.1515/corrrev-2024-0001 ↗
34. Anderson R, Kinee W, Policastro S. Corrosion of Copper-Nickel alloys in Seawater-Based electrolytes. ECS Meeting Abstracts. 2024;MA2024–01:1243–1243. https://doi.org/10.1149/MA2024-01181243mtgabs.10.1149/MA2024-01181243mtgabs ↗
35. Kear G, Barker BD, Walsh FC. Electrochemical corrosion of unalloyed copper in chloride media––a critical review. Corros Sci. 2004;46(1):109–35. https://doi.org/10.1016/s0010-938x(02)00257-3.10.1016/s0010-938x(02)00257-3 ↗
36. Faita G, Fiori G, Salvadore D. Copper behaviour in acid and alkaline brines—I kinetics of anodic dissolution in 0.5 M NaCl and free-corrosion rates in the presence of oxygen. Corros Sci. 1975;15(6–12):383–92. https://doi.org/10.1016/0010-938x(75)90005-0.10.1016/0010-938x(75)90005-0 ↗
37. Bianchi G, Fiori G, Longhi P, Mazza F. Horse shoe corrosion of copper alloys in flowing sea water: Mechanism, and possibility of cathodic protection of condenser tubes in power stations. CORROSION. 1978;34(11):396–406. https://doi.org/10.5006/0010-9312-34.11.396.10.5006/0010-9312-34.11.396 ↗
38. Lee HP. Kinetics and mechanisms of Cu electrodissolution in chloride media. J Electrochem Soc. 1986;133(10):2035. https://doi.org/10.1149/1.2108335.10.1149/1.2108335 ↗
39. Marcus P, editor. Corrosion mechanisms in theory and practice. 2nd ed. CRC; 2002. https://doi.org/10.1201/9780203909188.10.1201/9780203909188 ↗
40. Aydın H, Kaya E, Tokat-Birgin PÇ, et al. Wear and corrosion behaviour of TiO2/Graphite hybrid reinforced Copper-Based composites. Met Mater Int. 2025. https://doi.org/10.1007/s12540-025-02001-x.10.1007/s12540-025-02001-x ↗
41. Kasach AA, Kharytonau DS, Paspelau AV, Ryl J, Sergievich DS, Zharskii IM, Kurilo II. Effect of TiO2 concentration on microstructure and properties of composite Cu–Sn–TiO2 coatings obtained by electrodeposition. Materials. 2021;14:6179. https://doi.org/10.3390/ma14206179.10.3390/ma14206179 ↗