journal article·2025-10-15Open access

Correlating multi-pass hydrostatic extrusion characteristics with microstructure and mechanical properties of titanium grade 4

Łukasz Maj, Anna Jarzębska, Anna Trelka, Magdalena Bieda, Magdalena Gieleciak, Sonia Boczkal, Jacek Skiba, Mariusz Kulczyk

Abstract

Abstract In this work, influence of the variant of the Ti grade 4 plastic deformation with multi-pass hydrostatic extrusion (HE) on its microstructure and mechanical properties was studied. The emphasis was placed on the correlation between the extrusion pressure curves and the microstructure of produced rods after subsequent extrusion passes. The qualitative and quantitative microstructure characterization was performed with SEM/EBSD and orientation imaging in TEM. The mechanical properties were assessed in static tensile test. The results revealed that dynamic recrystallization during three-pass HE allowed to obtain bimodal microstructure consisting of elongated grains and a fraction of ultrafine defect-free equiaxed grains facilitating the plastic deformation. Adding a fourth extrusion pass produced highly deformed microstructure, as the temperature was insufficient to activate recrystallization processes. In this way, the highest mechanical strengthening was obtained inhibiting the extrusion process represented by nonuniform pressure curves. Application of recrystallization annealing to sustain uniform and stable plastic deformation represented by smooth extrusion curves, enabling to obtain relatively high plasticity of the final product. It has been demonstrated that optimization of extrusion path by selection of cross-sectional reduction or application of recrystallization annealing leads to obtaining either large mechanical strengthening or increased plasticity, depending of intended application.
Source: crossref · Quality: baseline

Research context

OpenAlex topics: Metallurgy and Material Forming · Microstructure and mechanical properties · Titanium Alloys Microstructure and Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (37)

Show source-provided references
1. El-Bassyouni GT, Mouneir SM, El-Shamy AM. Advances in surface modifications of titanium and its alloys: implications for biomedical and pharmaceutical applications. Multiscale Multidisciplin Model Exper Design. 2025;8:265.10.1007/s41939-025-00823-1 ↗
2. Chao Q, Sabirov I, Guo T, Hodgson PD, Beladi H. Tailoring the deformation characteristics of commercial purity titanium through hot deformation of a martensitic microstructure. Mater Sci Eng, A. 2021;827:142075.10.1016/j.msea.2021.142075 ↗
3. Zhong C, Liu J, Backes G, Zhao T, Schopphoven T, Gasser A. 3D printing of large-scale components of titanium alloys under open atmosphere. Mater Today Commun. 2021;28:102688.10.1016/j.mtcomm.2021.102688 ↗
4. Costa BC, Tokuhara CK, Rocha LA, Oliveira RC, Lisboa-Filho PN, Pessoa JC. Vanadium ionic species from degradation of Ti-6Al-4V metallic implants: In vitro cytotoxicity and speciation evaluation. Mater Sci Eng C. 2019;96:730–9.10.1016/j.msec.2018.11.090 ↗
5. Li Y, Wong C, Xiong J, Hodgson P, Wen C. Cytotoxicity of titanium and titanium alloying elements. J Dent Res. 2010;89(5):493–7.10.1177/0022034510363675 ↗
6. Sarraf M, Ghomi ER, Alipour S, Ramakrishna S, Sukiman NL. A state-of-the-art review of the fabrication and characteristics of titanium and its alloys for biomedical applications. Bio-Design Manufactur. 2022;5:371–95.10.1007/s42242-021-00170-3 ↗
7. Marin E, Lanzutti A. Biomedical applications of titanium alloys: a comprehensive review. Materials. 2024;17:114.10.3390/ma17010114 ↗
8. Zhu B, Wu X, Wan M, Cui X, Li H, Li X, et al. Effect of cold deformation on microstructure and mechanical behavior of commercially pure grade 4 titanium strip. Metals. 2022;12:1166.10.3390/met12071166 ↗
9. Park C-J, Lee M-R, Cho L-R, Yi Y-J, Jung H-N. Stability changes of dental implants according to the simulated peri-implant bone defects. Key Eng Mater. 2007;342–343:57–60.10.4028/www.scientific.net/KEM.342-343.57 ↗
10. Fang Y, Liu C, Jin K, Wei X, Zhao X, Bei H, et al. Additive manufacturing of titanium alloys with enhanced strength and uniform ductility via multi-element alloying. J Market Res. 2023;24:6854–60.
11. Edelati K, et al. Nanomaterials by severe plastic deformation: review of historical developments and recent advances. Mater Res Lett. 2022;10:163–256.10.1080/21663831.2022.2029779 ↗
12. Raab GI, Kodirov IS, Aksenov DA, Valiev RZ. The formation of a high-strength state in martensitic Ti Grade 4 by ECAP. J Alloy Compd. 2022;922:166205.10.1016/j.jallcom.2022.166205 ↗
13. Edalati K, et al. Severe plastic deformation for producing superfunctional ultrafine-grained and heterostructured materials: An interdisciplinary review. J Alloy Compd. 2024;1002:174667.10.1016/j.jallcom.2024.174667 ↗
14. Lowe TC, Valiev RZ. The use of severe plastic deformation techniques in grain refinement. Metals Mater Soc. 2024;56:64–8.10.1007/s11837-004-0295-z ↗
15. Miura H, Kobayashi M, Aoba T, Aoyama H, Benjanarasuth T. An approach for room-temperature multi-directional forging of pure titanium for strengthening. Mater Sci Eng, A. 2018;713:603–8.10.1016/j.msea.2018.06.060 ↗
16. Sotniczuk A, Garbacz H. Nanostructured bulk titanium with enhanced properties-strategies and prospects for dental applications. Adv Eng Mater. 2021;23:2000909.10.1002/adem.202000909 ↗
17. Garbacz H, Semenova IP, Zherebtsov S, Motyka M Nanocrystalline Titanium, Elsevier 2019;103–121
18. Pachla W, Kulczyk M, Przybysz S, Skiba J, Wojciechowski K, Przybysz M, et al. Effect of severe plastic deformation realized by hydrostatic extrusion and rotary swaging on the properties of CP Ti grade 2. J Mater Process Technol. 2015;221:255–68.10.1016/j.jmatprotec.2015.02.027 ↗
19. Chojnacka A, Kawalko J, Koscielny H, Guspiel J, Drewienkiewicz A, Bieda M, et al. Corrosion anisotropy of titanium deformed by the hydrostatic extrusion. Appl Surf Sci. 2018;426:987–94.10.1016/j.apsusc.2017.07.231 ↗
20. Bieda M, Jarzębska A, Koprowski P, Kawałko J, Kudłacz K, Boczkal S, et al. Microstructural investigations of materials after severe plastic deformation by means of orientations mapping in TEM and SEM. IOP Conference Series. 2018;375:012037.10.1088/1757-899X/375/1/012037 ↗
21. Pachla W, Kulczyk M, Sus-Ryszkowska M, Mazur A, Kurzydlowski KJ. Nanocrystalline titanium produced by hydrostatic extrusion. J Mater Process Technol. 2008;205:173–82.10.1016/j.jmatprotec.2007.11.103 ↗
22. Wojtas D, Wierzbanowski K, Chulist R, Pachla W, Bieda-Niemiec M, Jarzębska A, et al. Microstructure-strength relationship of ultrafine-grained titanium manufactured by unconventional severe plastic deformation process. J Alloy Compd. 2020;837:155576.10.1016/j.jallcom.2020.155576 ↗
23. Skiba J, Kulczyk M, Przybysz-Gloc S, Skorupska M, Niczyporuk K. The impact of severe plastic deformations obtained by hydrostatic extrusion on the machinability of ultrafine-grained Ti grade 2 intended for fasteners. Sci Rep. 2022;12:16240.10.1038/s41598-022-20339-9 ↗
24. Moreno-Valle EC, Pachla W, Kulczyk M, Sabirov I, Hohenwarter A. Anisotropy of tensile and fracture behavior of pure titanium after hydrostatic extrusion. Mater Trans. 2019;60:2160–7.10.2320/matertrans.MF201928 ↗
25. Topolski K, Jaroszewicz J, Garbacz H. Structural aspects and characterization of structure in the processing of titanium grade 4 different chips. Metals. 2021;11:101.10.3390/met11010101 ↗
26. Dubicki A, Kulczyk M, Szlązak K, Łojkowski M, Kurzydłowski KJ. The effect of high-pressure hydrostatic extrusion on mechanical properties of printed with fused deposition modeling PLA and PLA-diatomaceous earth composites. Materials. 2025;18:683.10.3390/ma18030683 ↗
27. Maj Ł, Trelka A, Muhaffel F, Góral A, Wierzbicka-Miernik A, Petrzak P, et al. Phase transformation of coatings produced with micro-arc oxidation on plastically deformed titanium through hydrothermal treatment. Mater Chem Phys. 2025;343:131001.10.1016/j.matchemphys.2025.131001 ↗
28. Wojtas D, Maj Ł, Jarzębska A, Wierzbanowski K, Chulist R, Kawałko J, et al. Influence of low-temperature heat treatment on microstructure and mechanical properties of hydrostatically extruded titanium. Mater Lett. 2022;325:132831.10.1016/j.matlet.2022.132831 ↗
29. Skorupska M, Kulczyk M, Przybysz S, Skiba J, Mizeracki J, Ryszkowska J. Mechanical reinforcement of Polyamide 6 by cold hydrostatic extrusion. Materials. 2021;14:6045.10.3390/ma14206045 ↗
30. http://www.crystorient.com/kikspot-software
31. Kar A, Suwas S, Kailas SV. Multi-length scale characterization of microstructure evolution and its consequence on mechanical properties in dissimilar friction stir welding of titanium to aluminum. Metall and Mater Trans A. 2019;51:5153–73.10.1007/s11661-019-05409-4 ↗
32. Sillekens WH, Bohlen J. Advances in wrought magnesium alloys: hydrostatic extrusion of magnesium alloys, Woodhead Publishing Limited 2012;323–345.10.1533/9780857093844.2.323 ↗
33. Dyakonov G, Zemtsova E, Mironov S, Semenova I, Valiev R, Semiatin S. An EBSD investigation of ultrafine-grain titanium for biomedical applications. Mater Sci Eng, A. 2015;648:305–10.10.1016/j.msea.2015.09.080 ↗
34. Dyakonov G, Mironov S, Yakovleva T, Semenova I. Thermal stability and recrystallization of titanium grade 4 with ultrafine-grained structure. MATEC Web of Conferences. 2020;321:11060.10.1051/matecconf/202032111060 ↗
35. Wojtas D, Maj Ł, Wierzbanowski K, Jarzębska A, Chulist R, Kawałko J, et al. Microstructure evolution of pure titanium during hydrostatic extrusion. Arch Civil Mech Eng. 2023;23:9.10.1007/s43452-022-00549-8 ↗
36. Kawałko J, Wroński M, Bieda M, Sztwiertnia K, Wierzbanowski K, Wojtas D, et al. Microstructure of titanium on complex deformation paths: comparison of ECAP, KOBO and HE techniques. Mater Charact. 2018;141:19–31.10.1016/j.matchar.2018.04.037 ↗
37. Luo P, McDonald DT, Xu W, Palanisamy S, Dargusch MS, Xia K. A modified Hall-Petch relationship in ultrafine-grained titanium recycled from chips by equal channel angular pressing. Scripta Mater. 2012;66(10):785–8.10.1016/j.scriptamat.2012.02.008 ↗