Mechanical characterization of Ti(C,N)-based cermets fabricated through different colloidal processing routes
Source abstract
Abstract
In this work the influence of different colloidal processing routes on the mechanical behavior of several Ti(C,N)-based cermets has been studied. The materials were designed with a Ti(C,N) content ranging between 80 and 85 vol %, in a Fe-Ni alloy matrix (with and without carbon addition). Three processing techniques were investigated: (i) Slip Casting (SC), (ii) Slip Casting + Cold Isostatic Pressing (SC+CIP), and (iii) Spray-Dry + Uniaxial Pressing (SDP). Biaxial strength distributions were determined in all samples using the ball-on-three-balls (B3B) method on disc-shaped specimens. Results were interpreted in the framework of Weibull theory. The characteristic strength ranged between 1090 MPa and 1870 MPa. A fractographic analysis performed on selected specimens showed different critical flaws, depending on the processing route, related to the composition and porosity level in each case. Single Edge V-Notched Beam (SEVNB) specimens fabricated with SDP were tested under 4-point-bending, in order to identify the effect of Fe-Ni content and carbon addition on their fracture resistance. Detailed fractographic analyses revealed slightly different mechanisms of fracture associated with the Fe-Ni and carbon content. Fracture toughness values ranging between ∼12 and ∼14 MPa m were measured. Based upon these findings the SDP route is proposed to improve both the strength and toughness of Ti(C,N) cermets, which can be enhanced by the addition of carbon during the colloidal processing.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advanced materials and composites · Powder Metallurgy Techniques and Materials · Aluminum Alloys Composites Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (51)
Show source-provided references
1. Development of TiCN-based cermets: mechanical properties and wear mechanism10.1016/j.ijrmhm.2012.07.001 ↗
2. Development and application of tool wear: a review of the characterization of TiC-based cermets with different binders10.1016/j.cej.2014.06.078 ↗
3. Microstructure and tribo-mechanical properties of ultrafine Ti(CN) cermets10.1016/S0263-4368(02)00004-5 ↗
4. Effect of nanocrystalline binder on the microstructure and mechanical properties of ultrafine Ti(CN) cermets10.1016/S0921-5093(03)00506-9 ↗
5. Toughened ultra-fine (Ti,W)(CN)–Ni cermets10.1016/j.scriptamat.2004.09.017 ↗
6. Microstructure and mechanical properties of TiC-TiN based cermets for tools application10.1016/j.ijrmhm.2008.10.006 ↗
7. Influence of tantalum on the microstructure and properties of Ti(C,N)-Ni cermets10.1016/j.ijrmhm.2013.08.008 ↗
8. Microstructure and mechanical properties of Mo-free Ti(C,N)-based cermets with Ni–xCr binders10.1016/j.jallcom.2014.11.236 ↗
9. Spark plasma sintering of TixTa1−xC0.5N0.5-based cermets: effects of processing conditions on chemistry, microstructure and mechanical properties10.1016/j.cej.2013.06.104 ↗
10. Hot-pressing of (Ti, Mt)(C, N)–Co–Mo 2 C (Mt = Ta, Nb) powdered cermets synthesized by a mechanically induced self-sustaining reaction10.1016/j.cej.2016.02.007 ↗
11. Effects of metal binder on the microstructure and mechanical properties of Ti(C,N)-based cermets10.1016/j.jallcom.2015.05.059 ↗
12. Comparison of Ti(C,N)-based cermets processed by hot-pressing sintering and conventional pressureless sintering10.1016/j.jallcom.2014.08.261 ↗
13. Interactions in iron-based cermet systems10.1016/S0925-8388(97)00360-5 ↗
14. Influence of milling parameters on the manufacturing of Fe-TiCN composite powders10.1016/j.jmatprotec.2005.02.154 ↗
15. Influence of milling time on the processing of Fe-TiCN composites10.1016/j.msea.2006.05.051 ↗
16. Improvement in microstructure and mechanical properties of Ti(C,N)-Fe cermets with the carbon additions10.1016/j.jallcom.2017.01.119 ↗
17. Microstructure and properties of Ti(C,N)–Mo2C–Fe cermets10.1016/j.ijrmhm.2009.01.003 ↗
18. The effect of WC, Mo2C, TaC content on the microstructure and properties of ultra-fine TiC0.7N0.3 cermet10.1016/j.matdes.2006.03.005 ↗
19. Effect of VC and nano-TiC addition on the microstructure and properties of micrometer grade Ti(CN)-based cermets10.1016/j.matdes.2008.08.017 ↗
20. Effect of secondary carbides addition on the microstructure and mechanical properties of (Ti, W, Mo, V)(C, N)-based cermets10.1016/j.ijrmhm.2011.03.013 ↗
21. Toughening of complete solid solution cermets by graphite addition10.1016/j.cej.2015.01.022 ↗
22. Characterization of interfaces between TiCN and iron-base binders10.1016/j.ijrmhm.2016.08.010 ↗
23. Influence of nickel boride addition on sintering behaviour and mechanical properties of TiC–Ni based cermets10.1016/j.jallcom.2016.06.122 ↗
24. Combustion synthesis of refractory and hard materials: a review10.1016/j.ijrmhm.2012.09.002 ↗
25. One-step preparation of dense TiC1−xNx–Ni3Ti cermet by combustion synthesis10.1016/j.matdes.2015.07.179 ↗
26. Self-propagating high-temperature synthesis of advanced materials and coatings10.1080/09506608.2016.1243291 ↗
27. Preparation of ultra-fine TiC0.7N0.3-based cermet10.1016/j.ijrmhm.2007.05.001 ↗
28. FGM stainless steel-Ti(C,N) cermets through colloidal processing10.1016/j.ijrmhm.2014.05.008 ↗
29. Chemical precipitation of nickel nanoparticles on Ti(C,N) suspensions focused on cermet processing10.1016/j.ijrmhm.2016.08.009 ↗
30. Novel colloidal approach for the microstructural improvement in Ti(C,N)/FeNi cermets10.1016/j.jallcom.2017.07.034 ↗
31. Role of stabilisers in the design of Ti aqueous suspensions for pressure slip casting10.1016/j.powtec.2014.04.093 ↗
32. Forming of nickel compacts by a colloidal filtration route10.1016/j.actamat.2004.10.038 ↗
33. Dispersion of nano-TiN powder in aqueous media10.1016/j.jallcom.2009.12.103 ↗
34. Novel colloidal approach for the microstructural improvement in Ti(C,N)/FeNi cermets10.1016/j.jallcom.2017.07.034 ↗
35. Deformation and fracture processes and the physical metallurgy of WC–Co hardmetals10.1179/imr.1988.33.1.90 ↗
36. Quantitative fractography of WC-Co cermets by Auger spectroscopy10.1007/BF00542749 ↗
37. Torres · 2002
38. Coureaux · 2012
39. The ball on three balls test for strength testing of brittle discs: stress distribution in the disc10.1016/S0955-2219(01)00458-7 ↗
40. The ball on three balls test for strength testing of brittle discs: Part II: analysis of possible errors in the strength determination10.1016/j.jeurceramsoc.2003.10.035 ↗
41. The ball on three balls test—strength and failure analysis of different materials10.1016/j.jeurceramsoc.2006.05.034 ↗
42. Analysis on the mechanical strength of WC-Co cemented carbides under uniaxial and biaxial bending10.1016/j.matdes.2013.10.051 ↗
43. 2.09 – mechanical characterization of ceramics: designing with brittle materials10.1016/B978-0-08-096527-7.00028-3 ↗
44. Influence of measurement uncertainties on the determination of the Weibull distribution10.1016/j.jeurceramsoc.2011.09.008 ↗
45. Strength and fracture analysis of silicon-based components for embedding10.1016/j.jeurceramsoc.2010.10.029 ↗
46. Critical notch-root radius effect in SENB-S fracture toughness testing10.1016/0955-2219(95)00197-2 ↗
47. 1995
48. 2007
49. The work of fracture and its measurement in metals, ceramics and other materials10.1007/BF00550177 ↗
50. Effect of sintering time on the microstructure and mechanical properties of (Ti,Ta)(C,N)-based cermets10.1016/j.ijrmhm.2013.01.001 ↗
51. Influence of carbon content on the sinterability of an FeCr matrix cermet reinforced with TiCN10.1016/j.ijrmhm.2012.10.007 ↗