Friction and wear properties of nano-Si3N4/nano-SiC composite under nanolubricated conditions
Source abstract
Abstract
Friction and wear properties of nano-Si3N4/nano-SiC composite were studied under nanolubricated conditions. Mineral oil mixed with nanoparticles of diamond was used as lubricant. A friction coefficient of 0.043 and a wear coefficient of 4.2×10-7 were obtained for nano-Si3N4/nano-SiC composite under normal load of 600 N with mineral oil + 0.5 wt% nanodiamond, whereas a friction coefficient of 0.077 and a wear coefficient of 10.3×10-7 were obtained for nano-Si3N4/nano-SiC composite under normal load of 600 N with mineral oil. 3D surface profilometer was used to study the surface morphology of wear scars. Scanning electron microscopy (SEM) and X-ray diffraction (XRD) studies were conducted to illustrate reduction in friction and wear.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Diamond and Carbon-based Materials Research · Tribology and Wear Analysis · Lubricants and Their Additives
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (27)
Show source-provided references
1. Segent JE. Chapter 7. Ceramic and ceramic composites. In Handbook of Materials for Product Design. Harper CA, Ed. New York: McGraw Hill, 2003: 7.1–6.
2. Wani MF. Mechanical and tribological properties of a nano-Si3N4/nano-BN composite. Int J Appl Ceram Tec 2010, 7: 512–517.10.1111/j.1744-7402.2009.02362.x ↗
3. Sun Y, Meng Q, Jia D, et al. Effect of hexagonal BN on the microstructure and mechanical properties of Si3N4 ceramics. J Mater Process Tech 2007, 182: 134–138.10.1016/j.jmatprotec.2006.07.020 ↗
4. Qiao Y-L, Sun X-F, Xu B-S, et al. High temperature tribological behaviors of nano-diamond as oil additive. J Cent South Univ T 2005, 12: 181–185.10.1007/s11771-005-0036-7 ↗
5. Chou CC, Lee SH. Rheological behavior and tribological performance of nanodiamond-dispersed lubricant. J Mater Process Tech 2008, 201: 542–547.10.1016/j.jmatprotec.2007.11.169 ↗
6. Šajgalík P, Hnatko M, Lencéš Z, et al. In situ preparation of Si3N4 /SiC nanocomposites for cutting tools application. Int J Appl Ceram Tec 2006, 3: 41–46.10.1111/j.1744-7402.2006.02061.x ↗
7. Rapoport L, Feldman Y, Homyonfer M, et al. Inorganic fullerene-like material as additives to lubricants: Structure–function relationship. Wear 1999, 225–229: 975–982.10.1016/S0043-1648(99)00040-X ↗
8. Wu YY, Tsui WC, Liu TC. Experimental analysis of tribological properties of lubricating oils with nanoparticle additives. Wear 2007, 262: 819–825.10.1016/j.wear.2006.08.021 ↗
9. Marko M, Kyle J, Branson B, et al. Tribological improvements of dispersed nanodiamond additives in lubricating mineral oil. J Tribol 2014, 137: 011802.10.1115/1.4028554 ↗
10. Zhao W, Basnet B, Kim IJ. Carbon nanotube formation using zeolite template and applications. J Adv Ceram 2012, 1: 179–193.10.1007/s40145-012-0018-9 ↗
11. Tarasov S, Kolubaev A, Belyaev S, et al. Study of friction reduction by nanocopper additives to motor oil. Wear 2002, 252: 63–69.10.1016/S0043-1648(01)00860-2 ↗
12. Rapoport L, Leshchinsky V, Lapsker I, et al. Tribological properties of WS2 nanoparticles under mixed lubrication. Wear 2003, 255: 785–793.10.1016/S0043-1648(03)00044-9 ↗
13. Liu G, Li X, Lu N, et al. Enhancing AW/EP property of lubricant oil by adding nano Al/Sn particles. Tribol Lett 2005, 18: 85–90.10.1007/s11249-004-1760-0 ↗
14. Radice R, Mischler S. Effect of electrochemical and mechanical parameters on the lubrication behaviour of Al2O3 nanoparticles in aqueous suspensions. Wear 2006, 261: 1032–1041.10.1016/j.wear.2006.03.034 ↗
15. Chou C-C, Lee S-H. Tribological behavior of nanodiamond-dispersed lubricants on carbon steels and aluminium alloy. Wear 2010, 269: 757–762.10.1016/j.wear.2010.08.001 ↗
16. Joly-Pottuz L, Matsumoto N, Kinoshita H, et al. Diamond-derived onions as lubricant additives. Tribol Int 2008, 41: 69–78.10.1016/j.triboint.2007.05.001 ↗
17. Chang L, Zhang Z, Breidt C, et al. Tribological properties of epoxy nanocomposites: I. Enhancement of the wear resistance by nano-TiO2 particles. Wear 2005, 258: 141–148.
18. Mochalin V, Shenderova O, Ho D, et al. The properties and applications of nanodiamonds. Nat Nanotechnol 2012, 7: 11–23.10.1038/nnano.2011.209 ↗
19. Lee J, Cho S, Hwang Y, et al. Application of fullerene-added nano-oil for lubrication enhancement in friction surfaces. Tribol Int 2009, 42: 440–447.10.1016/j.triboint.2008.08.003 ↗
20. Chang Y, Wang H, Zhu Q, et al. Theoretical calculation and analysis of ZrO2 spherical nanometer powders. J Adv Ceram 2013, 2: 21–25.10.1007/s40145-013-0036-2 ↗
21. Gu C, Li Q, Gu Z, et al. Study on application of CeO2 and CaCO3 nanoparticles in lubricating oils. J Rare Earth 2008, 26: 163–167.10.1016/S1002-0721(08)60058-7 ↗
22. Song H-J, Zhang Z-Z, Men X-H. The tribological behaviors of the polyurethane coating filled with nano-SiO2 under different lubrication conditions. Composites Part A 2008, 39: 188–194.10.1016/j.compositesa.2007.11.003 ↗
23. Battez AH, González R, Viesca JL, et al. CuO, ZrO2 and ZnO nanoparticles as antiwear additive in oil lubricants. Wear 2008, 265: 422–428.10.1016/j.wear.2007.11.013 ↗
24. Yu H-L, Xu Y, Shi P-J, et al. Tribological properties of lubricating mechanisms of Cu nanoparticles in lubricant. T Nonferr Metal Soc 2008, 18: 636–641.10.1016/S1003-6326(08)60111-9 ↗
25. Hnatko M, Šajgalík P, Lencéš Z, et al. Low cost SiC/Si3N4 nanocomposites. Key Eng Mat 2002, 206–213: 1061–1064.10.4028/www.scientific.net/KEM.206-213.1061 ↗
26. Wu J-M, Zhang X-Y, Xu J, et al. Preparation of porous Si3N4 ceramics via tailoring solid loading of Si3N4 slurry and Si3N4 poly-hollow microsphere content. J Adv Ceram 2015, 4: 260–266.10.1007/s40145-015-0158-9 ↗
27. Stachowiak GW, Batchelor AW. Engineering Tribology, 3rd edn. Elsevier Butterworth-Heinemann, 2010: 7.26–7.27.