journal article·2020-08Open access

Fabrication of SiCw/Ti3SiC2 composites with improved thermal conductivity and mechanical properties using spark plasma sintering

Xiaobing Zhou, Lei Jing, Yong Duk Kwon, Jin-Young Kim, Zhengren Huang, Dang-Hyok Yoon, Jaehyung Lee, Qing Huang

Journal of Advanced Ceramics· Volume 9· Issue 4

Abstract

Abstract High strength SiC whisker-reinforced Ti3SiC2 composites (SiCw/Ti3SiC2) with an improved thermal conductivity and mechanical properties were fabricated by spark plasma sintering. The bending strength of 10 wt% SiCw/Ti3SiC2 was 635 MPa, which was approximately 50% higher than that of the monolithic Ti3SiC2 (428 MPa). The Vickers hardness and thermal conductivity (k) also increased by 36% and 25%, respectively, from the monolithic Ti3SiC2 by the incorporation of 10 wt% SiCw. This remarkable improvement both in mechanical and thermal properties was attributed to the fine-grained uniform composite microstructure along with the effects of incorporated SiCw. The SiCw/Ti3SiC2 can be a feasible candidate for the in-core structural application in nuclear reactors due to the excellent mechanical and thermal properties.
Source: crossref · Quality: baseline

Research context

OpenAlex topics: MXene and MAX Phase Materials · Advanced ceramic materials synthesis · Aluminum Alloys Composites Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (42)

Show source-provided references
1. Jeitschko W, Nowotny H. Die kristallstruktur von Ti3SiC2—ein neuer komplexcarbid-typ. Monatshefte Für Chemie 1967, 98: 329–337.10.1007/BF00899949 ↗
2. Barsoum MW. The MN+1AXN phases: A new class of solids. Prog Solid State Chem 2000, 28: 201–281.10.1016/S0079-6786(00)00006-6 ↗
3. Tallman DJ, Hoffman EN, Caspi EN, et al. Effect of neutron irradiation on select MAX phases. Acta Mater 2015, 85: 132–143.10.1016/j.actamat.2014.10.068 ↗
4. Barsoum MW. MAX Phases: Properties of Machinable Ternary Carbides and Nitrides. Weinheim, Germany: Wiley-VCH Verlag GmbH & Co. KGaA, 2013.10.1002/9783527654581 ↗
5. Jovic VD, Jovic BM, Gupta S, et al. Corrosion behavior of select MAX phases in NaOH, HCl and H2SO4. Corros Sci 2006, 48: 4274–4282.10.1016/j.corsci.2006.04.005 ↗
6. Zhu M, Wang R, Chen C, et al. Comparison of corrosion Behaviour of Ti3SiC2 and Ti3AlC2 in NaCl solutions with Ti. Ceram Int 2017, 43: 5708–5714.10.1016/j.ceramint.2017.01.111 ↗
7. Hoffman EN, Vinson DW, Sindelar RL, et al. MAX phase carbides and nitrides: Properties for future nuclear power plant in-core applications and neutron transmutation analysis. Nucl Eng Des 2012, 244: 17–24.10.1016/j.nucengdes.2011.12.009 ↗
8. Liu JW, Zhou XB, Tatarko P, et al. Fabrication, microstructure, and properties of SiC/Al4SiC4 multiphase ceramics via an in situ formed liquid phase sintering. J Adv Ceram 2020, 9: 193–203.10.1007/s40145-020-0359-8 ↗
9. Du Y, Schuster JC, Seifert HJ, et al. Experimental investigation and thermodynamic calculation of the titanium-silicon-carbon system. J Am Ceram Soc 2000, 83: 197–203.10.1111/j.1151-2916.2000.tb01170.x ↗
10. Zhu GX, Feng Q, Yang JS, et al. Effect of BNNTs/matrix interface tailoring on toughness and fracture morphology of hierarchical SiCf/SiC composites. J Adv Ceram 2019, 8: 555–563.10.1007/s40145-019-0338-0 ↗
11. Zhang ZF, Sha JJ, Zu YF, et al. Fabrication and mechanical properties of self-toughening ZrB2-SiC composites from in situ reaction. J Adv Ceram 2019, 8: 527–536.10.1007/s40145-019-0334-4 ↗
12. Wang HL, Gao ST, Peng SM, et al. KD-S SiCj/SiC composites with BN interface fabricated by polymer infiltration and pyrolysis process. J Adv Ceram 2018, 7: 169–177.10.1007/s40145-018-0268-2 ↗
13. Liu GW, Zhang XZ, Yang J, et al. Recent advances in joining of SiC-based materials (monolithic SiC and SiCf/SiC composites): Joining processes, joint strength, and interfacial behavior. J Adv Ceram 2019, 8: 19–38.10.1007/s40145-018-0297-x ↗
14. Zhang JF, Wu T, Wang LJ, et al. Microstructure and properties of Ti3SiC2/SiC nanocomposites fabricated by spark plasma sintering. Compos Sci Technol 2008, 68: 499–505.10.1016/j.compscitech.2007.06.006 ↗
15. Zhou YC, Wan DT, Bao YW, et al. In situ processing and high-temperature properties of Ti3Si(Al)C2/SiC composites. Int J Appl Ceram Technol 2006, 3: 47–54.10.1111/j.1744-7402.2006.02057.x ↗
16. Wan DT, Zhou YC, Bao YW, et al. In situ reaction synthesis and characterization of Ti3Si(Al)C2/SiC composites. Ceram Int 2006, 32: 883–890.10.1016/j.ceramint.2005.07.004 ↗
17. Li SB, Song GM, Zhou Y. A dense and fine-grained SiC/Ti3Si(Al)C2 composite and its high-temperature oxidation behavior. J Eur Ceram Soc 2012, 32: 3435–3444.10.1016/j.jeurceramsoc.2012.04.029 ↗
18. Li SB, Xie JX, Zhang LT, et al. In situ synthesis of Ti3SiC2/SiC composite by displacement reaction of Si and TiC. Mater Sci Eng: A 2004, 381: 51–56.10.1016/j.msea.2004.03.046 ↗
19. Wan DT, Zhou YC, Hu CF, et al. Improved strength-impairing contact damage resistance of Ti3Si(Al)C2/SiC composites. J Eur Ceram Soe 2007, 27: 2069–2076.10.1016/j.jeurceramsoc.2006.07.018 ↗
20. Barsoum M, Ho-Duc LH, Radovic M, et al. Long time oxidation study of Ti3SiC2, Ti3SiC2/SiC and Ti3SiC2/TiC composites in air. J Electrochem Soe 2003, 150: B166–B175.10.1149/1.1556035 ↗
21. Zhang JF, Wang LJ, Jiang W, et al. High temperature oxidation behavior and mechanism of Ti3SiC2-SiC nanocomposites in air. Compos Sci Teehnol 2008, 68: 1531–1538.10.1016/j.compscitech.2007.10.029 ↗
22. Zhang JF, Wang LJ, Shi L, et al. Rapid fabrication of Ti3SiC2-SiC nanocomposite using the spark plasma sintering-reactive synthesis (SPS-RS) method. Seripta Mater 2007, 56: 241–244.10.1016/j.scriptamat.2006.09.029 ↗
23. Becher PF, Hsueh CH, Angelini P, et al. Toughening behavior in whisker-reinforced ceramic matrix composites. J Am Ceram Soc 1988, 71: 1050–1061.10.1111/j.1151-2916.1988.tb05791.x ↗
24. Zan QF, Dong LM, Wang C, et al. Improvement of mechanical properties of Al2O3/Ti3SiC2 multilayer ceramics by adding SiC whiskers into Al2O3 layers. Ceram Int 2007, 33: 385–388.10.1016/j.ceramint.2005.10.007 ↗
25. Hashimoto H, Sun ZM, Tada S, et al. Strengthening of titanium silicon carbide by grain orientation control and silicon carbide whisker dispersion. Mater Trans 2007, 48: 2427–2431.10.2320/matertrans.MAW200718 ↗
26. Sun Z, Zhou Y, Li M. High temperature oxidation behavior of Ti3SiC2-based material in air. Aeta Mater 2001, 49: 4347–4353.
27. Barsoum M, ElRaghy T, Ogbuji LUJT. Oxidation of Ti3SiC2 in air. J Electrochem Soc 1997, 144: 2508–2516.10.1149/1.1837846 ↗
28. Yang SL, Sun ZM, Hashimoto H, et al. Oxidation of Ti3SiC2 at 1000 C in air. Oxid Met 2003, 59: 155–156.10.1023/A:1023026201209 ↗
29. Yang H, Zhou XB, Shi W, et al. Thickness-dependent phase evolution and bonding strength of SiC ceramics joints with active Ti interlayer. J Eur Ceram Soc 2017, 37: 1233–1241.10.1016/j.jeurceramsoc.2016.12.009 ↗
30. Sun J, Gao L. Dispersing SiC powder and improving its rheological behaviour. J Eur Ceram Soc 2001, 21: 2447–2451.10.1016/S0955-2219(01)00196-0 ↗
31. Kwon H, Zhou XB, Yoon DH. Fabrication of SiCj/Ti3SiC2 by the electrophoresis of highly dispersed Ti3SiC2 powder. Ceram Int 2020, 46: 18168–18174.10.1016/j.ceramint.2020.04.138 ↗
32. Midgley PA, Weyland M, Thomas JM, et al. Z-Contrast tomography: A technique in three-dimensional nanostructural analysis based on Rutherford scattering. Chem Commun 2001: 907–908.10.1039/b101819c ↗
33. Sato K, Mishra M, Hirano H, et al. Pressureless sintering and reaction mechanisms of Ti3SiC2 ceramics. J Am Ceram Soc 2014, 97: 1407–1412.10.1111/jace.12903 ↗
34. Sun Z, Zou Y, Tada S, et al. Effect of Al addition on pressureless reactive sintering of Ti3SiC2. Scripta Mater 2006, 55: 1011–1014.10.1016/j.scriptamat.2006.08.019 ↗
35. Spencer CB, Córdoba JM, Obando NH, et al. The reactivity of Ti2AlC and Ti3SiC2 with SiC fibers and powders up to temperatures of 1550 °C. J Am Ceram Scripta 2011, 94: 1737–1743.10.1111/j.1551-2916.2010.04332.x ↗
36. Zhang RS, Wang H, Tian M, et al. Pressureless reaction sintering and hot isostatic pressing of transparent MgAlON ceramic with high strength. Ceram Int 2018, 44: 17383–17390.10.1016/j.ceramint.2018.06.203 ↗
37. Bjork L, Hermansson LAG. Hot isostatically pressed alumina-silicon carbide-whisker composites. J Am Ceram Soc 1989, 72: 1436–1438.10.1111/j.1151-2916.1989.tb07668.x ↗
38. Mai YW, Lawn BR. Crack-interface grain bridging as a fracture resistance mechanism in ceramics: II, theoretical fracture mechanics model. J Am Ceram Soc 1987, 70: 289–294.10.1111/j.1151-2916.1987.tb04983.x ↗
39. Zhou YC, Sun ZM. Electronic structure and bonding properties in layered ternary carbide Ti3SiC2. J Phys: Condens Matter 2000, 12: 457–462.
40. Wang JY, Zhou YC. Polymorphism of Ti3SiC2 ceramic: First-principles investigations. Phys Rev B 2004, 69: 144108.10.1103/PhysRevB.69.144108 ↗
41. Mata-Osoro G, Moya JS, Pecharroman C. Transparent alumina by vacuum sintering. J Eur Ceram Soc 2012, 32: 2925–2933.10.1016/j.jeurceramsoc.2012.02.039 ↗
42. Snead LL, Nozawa T, Katoh Y, et al. Handbook of SiC properties for fuel performance modeling. J Nucl Mater 2007, 371: 329–377.10.1016/j.jnucmat.2007.05.016 ↗