Predictive process diagram for parameters selection in laser powder bed fusion to achieve high-density and low-cracking built parts
Source abstract
Abstract
The laser powder bed fusion process (LPBF) has been widely used in many industrial sectors, including automotive, aerospace, and biomedical devices. With the fast development of new materials designed for critical applications, the conventional design of experiments for determining an optimal LPBF process window is a time and material-consuming activity. This can impose difficulties on small-to-medium industrial businesses where investing resources are limited. To address these challenges, this study draws inspiration from a reliable diagram used in laser welding to construct a similar diagram for the LPBF process. The objective is to enable the "right-first-time" selection of parameters that achieve a minimum of 99% density, regardless of the metallic materials and machine platforms. The diagram is established based on dimensionless beam power and velocity, derived from multiple LPBF process parameters (e.g., laser power, scan speed, hatch spacing) and the thermophysical properties of materials (e.g., melting point, density, thermal diffusivity). Furthermore, hot cracking susceptibility is considered by a strain-rate approach incorporated with the dimensionless thermal strain factor, which benefits when processing hard-to-weld alloys. The diagram shows high reliability in determining parameters corresponding to lack of fusion, keyhole porosity and 99% dense parts when plotting against literature data of LPBF for several metallic materials. Similar results were observed when applying to a novel material ABD-900AM Ni-based alloy, for which no previously published data were available. Moreover, the diagram proved effective in selecting parameters to process the high-cracking susceptible CM247LC Ni-based alloy, resulting in significant mitigation of hot cracking in the as-fabricated parts.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Additive Manufacturing Materials and Processes · Additive Manufacturing and 3D Printing Technologies · Welding Techniques and Residual Stresses
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (73)
Show source-provided references
1. Experimental approach towards parameter evaluation in laser powder bed fusion of metals10.1080/0951192X.2021.1901313 ↗
2. Additive manufacturing in production: a study case applying technical requirements10.1016/j.phpro.2015.11.050 ↗
3. Optimising the process parameters of selective laser melting for the fabrication of Ti6Al4V alloy10.1108/RPJ-03-2016-0045 ↗
4. Process optimization of complex geometries using feed forward control for laser powder bed fusion additive manufacturing
5. Part geometry and conduction-based laser power control for powder bed fusion additive manufacturing
6. The transformation hardening of steel surfaces by laser beams—I. Hypo-eutectoid steels10.1016/0001-6160(84)90175-5 ↗
7. A second report on diagrams of microstructure and hardness for heat-affected zones in welds10.1016/0001-6160(84)90176-7 ↗
8. Diagrams for laser materials processing10.1016/0956-7151(92)90097-X ↗
9. A simple methodology for predicting laser-weld properties from material and laser parameters10.1088/0022-3727/44/44/445401 ↗
10. Observation of keyhole-mode laser melting in laser powder-bed fusion additive manufacturing10.1016/j.jmatprotec.2014.06.005 ↗
11. Scaling laws for the additive manufacturing10.1016/j.jmatprotec.2018.02.034 ↗
12. Validated dimensionless scaling law for melt pool width in laser powder bed fusion10.1016/j.jmatprotec.2021.117316 ↗
13. Application of dimensional analysis to selective laser melting10.1108/13552540810841526 ↗
14. Dimensionless numbers in additive manufacturing10.1063/1.4976006 ↗
15. Normalised model-based processing diagrams for additive layer manufacture of engineering alloys10.1016/j.actamat.2016.02.025 ↗
16. Printability of alloys for additive manufacturing10.1038/srep19717 ↗
17. Energy coupling mechanisms and scaling behavior associated with laser powder bed fusion additive manufacturing10.1002/adem.201900185 ↗
18. Keyhole-induced porosities in Laser-based Powder Bed Fusion (L-PBF) of Ti6Al4V: High-fidelity modelling and experimental validation
19. Laser-based powder bed fusion additive manufacturing of pure copper
20. Laser additive manufacturing of pure molybdenum using freeze-dry pulsated orifice ejection method-produced powders10.1016/j.jmrt.2021.12.084 ↗
21. The prediction of case depth in laser transformation hardening10.1007/BF02665012 ↗
22. Chapter 14 - General Physical Properties
23. Mathematical theory of heat distribution during welding and cutting
24. The theory of moving sources of heat and its application to metal treatments10.1115/1.4018624 ↗
25. The problem of the strength of metals while solidifying during welding
26. Hot cracking tests—an overview of present technologies and applications10.1007/s40194-014-0126-y ↗
27. Initiation and growth mechanisms for weld solidification cracking10.1179/1743280413Y.0000000020 ↗
28. Microstructure characterization and mechanical properties of crack-free Al-Cu-Mg-Y alloy fabricated by laser powder bed fusion
29. Varestraint Testing of Selective Laser Additive Manufactured Alloy 718—Influence of Grain Orientation10.3390/met9101113 ↗
30. Understanding Crack Formation Mechanisms of Ti–48Al–2Cr–2Nb Single Tracks During Laser Powder Bed Fusion10.1007/s12540-020-00770-1 ↗
31. T. Huynh, Parametric Investigation and Optimization for Inconel 718 Nickel-Based Superalloy in Laser Powder Bed Fusion, 2020.
32. Using JMatPro to model materials properties and behavior10.1007/s11837-003-0013-2 ↗
33. The influence of pulsed laser powder bed fusion process parameters on Inconel 718 material properties10.1016/j.msea.2019.138527 ↗
34. Aubert&Duval. (2020, 10/10/2023). Stellar ABD-900AM Datasheet. Available: 〈https://www.aubertduval.com/wp-media/uploads/sites/2/2019/09/ABD-900AM_Stellar_AM_V0_GB.pdf〉.
35. Influence of Laser Powder Bed Fusion Process Parameters on Voids, Cracks, and Microhardness of Nickel-Based Superalloy Alloy 247LC
36. Measurement of thermophysical properties of Ni based super alloys
37. Process Optimization and Microstructure Analysis to Understand Laser Powder Bed Fusion of 316L Stainless Steel10.3390/met11050832 ↗
38. Influence of processing parameters on the density of 316L stainless steel parts manufactured through laser powder bed fusion10.1177/0954405420911768 ↗
39. Effect of process parameters on the microstructure, tensile strength and productivity of 316L parts produced by laser powder bed fusion10.1016/j.matchar.2019.110016 ↗
40. Material-specific phenomena and developing higher yield process parameters in laser powder bed fusion of 17-4 PH stainless steel10.1007/s40430-022-03946-5 ↗
41. Matweb. (31/07/2023). 17-4PH Thermophysical properties. Available: 〈https://www.matweb.com/search/datasheet.aspx?matguid=ef0844b850954281a438dc76c1e0b49e&ckck=1〉.
42. Experimental and numerical investigation of 17–4PH stainless steel fabricated by laser powder bed fusion and hot isostatic pressing10.1088/2053-1591/ac2b55 ↗
43. Experimental investigation on selective laser melting of 17-4PH stainless steel10.1016/j.optlastec.2016.07.012 ↗
44. Quantification and prediction of lack-of-fusion porosity in the high porosity regime during laser powder bed fusion of Ti-6Al-4V10.1016/j.jmatprotec.2021.117426 ↗
45. Influence of processing parameters on the evolution of melt pool, porosity, and microstructures in Ti-6Al-4V alloy parts fabricated by selective laser melting10.1007/s40964-017-0030-2 ↗
46. The influence of porosity on Ti-6Al-4V parts fabricated by laser powder bed fusion in the pursuit of process efficiency10.1007/s00170-021-08374-8 ↗
47. H. Gong, K. Rafi, T. Starr, and B. Stucker, The Effects of Processing Parameters on Defect Regularity in Ti-6Al-4V Parts Fabricated By Selective Laser Melting and Electron Beam Melting, in 24th Annual International Solid Freeform Fabrication Symposium—An Additive Manufacturing Conference, Austin, TX, Aug, 2013, pp. 12-14.
48. Limits and solutions in processing pure Cu via selective laser melting using a high-power single-mode fiber laser10.1007/s00170-019-04015-3 ↗
49. Matweb. (2023). Copper thermophysical properties. Available: 〈https://www.matweb.com/search/datasheet_print.aspx?matguid=9aebe83845c04c1db5126fada6f76f7e〉.
50. Process–Structure–Property Relationships of Copper Parts Manufactured by Laser Powder Bed Fusion10.3390/ma14112945 ↗
51. Effect of Particle Size Distribution on Laser Powder Bed Fusion Manufacturability of Copper10.1007/s00501-021-01107-0 ↗
52. Pure molybdenum manufactured by Laser Powder Bed Fusion: Thermal and mechanical characterization at room and high temperature
53. Plansee. Mo Thermo-physical properties. Available: 〈https://www.plansee.com/en/materials/molybdenum.html〉.
54. Selective laser melting of pure molybdenum: Evolution of defect and crystallographic texture with process parameters10.1016/j.matdes.2020.108588 ↗
55. Gibson · 2018
56. Disertation, The University of Sheffield
57. A systematic analysis of performance measures for classification tasks10.1016/j.ipm.2009.03.002 ↗
58. General Performance Score for classification problems10.1007/s10489-021-03041-7 ↗
59. The impact of class imbalance in classification performance metrics based on the binary confusion matrix10.1016/j.patcog.2019.02.023 ↗
60. Suppression of liquation cracking susceptibility via pre-weld heat treatment for manufacturing of CM247LC superalloy turbine blade welds
61. The effect of absorption ratio on meltpool features in laser-based powder bed fusion of IN71810.1016/j.optlastec.2022.108263 ↗
62. Metal vaporization and its influence during laser powder bed fusion process10.1016/j.matdes.2022.110505 ↗
63. Effects of scan speed on vapor plume behavior and spatter generation in laser powder bed fusion additive manufacturing10.1016/j.jmapro.2018.09.011 ↗
64. The interplay between vapour, liquid, and solid phases in laser powder bed fusion10.1038/s41467-022-30667-z ↗
65. Vapor–plasma plume investigation during high-power fiber laser welding10.1088/1054-660X/23/1/016001 ↗
66. Visualization of refraction and attenuation of near-infrared laser beam due to laser-induced plume10.2351/1.3110058 ↗
67. Solidification crack propagation and morphology dependence on processing parameters in AA6061 from ultra-high-speed x-ray visualization
68. In situ X-ray imaging of hot cracking and porosity during LPBF of Al-2139 with TiB2 additions and varied process parameters10.1016/j.matdes.2023.112031 ↗
69. Carter · 2013
70. Determining the BTR by conducting a Trans-Varestraint test using a high-speed camera and two-color pyrometry10.1007/s40194-018-0608-4 ↗
71. Getting the Strain Under Control: Trans-Varestraint Tests for Hot Cracking Susceptibility10.1007/s11661-019-05140-0 ↗
72. Assessment of the Solidification Cracking Susceptibility of Welding Consumables in the Varestraint Test by Means of an Extended Evaluation Methodology10.1002/adem.202101650 ↗
73. Lippold · 2015