Heat treatment possibilities for an in situ βTi-TiC composite made by laser powder bed fusion
Source abstract
Abstract
After laser powder bed fusion (LPBF) of an ultra-strong in situ TiC whisker reinforced β-Ti composite, this paper investigates the evolution of microstructure and mechanical properties in response to heat treatment at different temperatures. Using in depth nano-SEM and TEM analyses, it is shown that ageing at 400 °C rounds the whiskers, annihilates the strain fields and grows Mo segregated nano-cells, but without improving the ductility. In contrast, ageing at 600 °C enables the transformation of metastable β to a lamellar β + α, leading to a dual phase matrix embedding TiC particles. This is in such a manner that extra ageing at 600 °C coalesces the nano-lamellar α + β microstructure to form a coarser micro-lamellar α + β matrix. This microstructure achieves 66 % of the compressive deformation of Cp-Ti, and over 1400 MPa compressive strength after 1 h of ageing at 600 °C. Despite this success under compression, hard and stiff TiC particles may still cause large spherical fractured voids, severely limiting the plastic deformation under tension.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Titanium Alloys Microstructure and Properties · Additive Manufacturing Materials and Processes · Advanced materials and composites
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (37)
Show source-provided references
1. Preface
2. Particulate reinforced metal matrix composites - a review10.1007/BF00544448 ↗
3. Microstructural and mechanical characteristics of in situ metal matrix composites10.1016/S0927-796X(00)00024-3 ↗
4. Selective laser melting to manufacture “In situ” metal matrix composites: a review10.1002/adem.201801244 ↗
5. Experimental investigation on selective laser melting behaviour and processing windows of in situ reacted Al/Fe2O3 powder mixture10.1016/j.powtec.2012.07.061 ↗
6. Effect of Al alloys on selective laser melting behaviour and microstructure of in situ formed particle reinforced composites10.1016/j.jallcom.2012.06.097 ↗
7. Selective laser melting of in-situ Al4SiC4+SiC hybrid reinforced Al matrix composites: influence of starting SiC particle size10.1016/j.surfcoat.2015.04.029 ↗
8. In situ alloying and reinforcing of Al6061 during selective laser melting10.1016/j.procir.2018.08.009 ↗
9. Densification, microstructure, and wear property of in situ titanium nitride-reinforced titanium silicide matrix composites prepared by a novel selective laser melting process10.1007/s11661-011-0876-8 ↗
10. Preparation of TiN–Ti5Si3 in-situ composites by selective laser melting10.1016/j.matlet.2009.04.010 ↗
11. Comparative study of microstructures and mechanical properties of in situ Ti–TiB composites produced by selective laser melting, powder metallurgy, and casting technologies10.1557/jmr.2014.122 ↗
12. Selective laser melting of in situ titanium–titanium boride composites: processing, microstructure and mechanical properties10.1016/j.actamat.2014.05.022 ↗
13. Effect of powder particle shape on the properties of in situ Ti–TiB composite materials produced by selective laser melting10.1016/j.jmst.2015.08.007 ↗
14. Selective Laser Melting process optimization of Ti–Mo–TiC metal matrix composites10.1016/j.cirp.2019.04.120 ↗
15. In situ transformations during SLM of an ultra-strong TiC reinforced Ti composite10.1038/s41598-020-67434-3 ↗
16. A perspective on molybdenum biocompatibility and antimicrobial activity for applications in implants10.1007/s10853-015-9664-y ↗
17. Effect of titanium carbide coating on the osseointegration response in vitro and in vivo10.1016/j.biomaterials.2006.08.018 ↗
18. Improving osteoblast response in vitro by a nanostructured thin film with titanium carbide and titanium oxides clustered around graphitic carbon10.1371/journal.pone.0152566 ↗
19. Laser deposition of compositionally graded titanium–vanadium and titanium–molybdenum alloys10.1016/S0921-5093(02)00909-7 ↗
20. Laser-assisted synthesis of Ti–Mo alloys for biomedical applications10.1016/j.msec.2012.03.007 ↗
21. Microstructure and mechanical properties of a novel β titanium metallic composite by selective laser melting10.1016/j.actamat.2014.01.018 ↗
22. Crossover from ω-phase to α-phase precipitation in bcc Ti-Mo10.1103/PhysRevB.49.11759 ↗
23. Rhea Trinkle · 2003
24. Comparative study of commercially pure titanium produced by laser engineered net shaping, selective laser melting and casting processes10.1016/j.msea.2017.08.103 ↗
25. Microstructure and mechanical properties investigation of CP titanium processed by selective laser melting (SLM)10.1016/j.jmatprotec.2016.10.022 ↗
26. Role of alloying elements in microstructures of beta titanium alloys with carbon additions10.1179/026708303225005999 ↗
27. Influence of trace boron on the morphology of titanium carbide in an Al–Ti–C–B master alloy10.1016/j.jallcom.2009.10.148 ↗
28. Growth morphologies and mechanisms of TiC grains during selective laser melting of Ti–Al–C composite powder10.1016/j.matlet.2009.08.043 ↗
29. Effect of Mo on the phase stability and elastic mechanical properties of Ti–Mo random alloys from ab initio calculations10.1088/1361-648X/aa87d3 ↗
30. Origin of shear induced β to ω transition in Ti–Nb-based alloys10.1016/j.actamat.2015.03.040 ↗
31. Thermal analysis of the ω nanophase transformation from the metastable β Ti–12Mo alloy10.1007/s10973-010-0713-0 ↗
32. Mo segregation and distribution in Ti–Mo alloy investigated using nanoindentation10.1016/j.msea.2018.01.098 ↗
33. Effect of omega phase on mechanical properties of Ti-Mo alloys for biomedical applications
34. Omega-phase formation in Beta III titanium alloy10.1016/0026-0800(72)90051-1 ↗
35. Effect of carbon on the mechanical properties and structure of titanium alloys10.1007/BF00679223 ↗
36. The effect of carbon on the behavior of the Beta-titanium alloys
37. Effect of boron and carbon addition on microstructure and mechanical properties of metastable beta titanium alloys10.1016/j.matdes.2014.11.004 ↗