Oscillating laser directed energy deposition for manufacturing high-performance titanium alloy
Bibliographic record
Abstract
No abstract is available for this record. The assistant can identify its topic from the title, but cannot infer the study’s results.
Source: Not provided · Quality: missing
Research context
OpenAlex topics: Additive Manufacturing Materials and Processes · Solidification and crystal growth phenomena · Surface Treatment and Residual Stress
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (62)
Show source-provided references
1. Progress and perspectives in laser additive manufacturing of key aeroengine materials10.1016/j.ijmachtools.2021.103804 ↗
2. High-performance functional coatings manufactured by integrated extremely high-speed-rate laser directed energy deposition with interlayer remelting10.1016/j.ijmachtools.2024.104174 ↗
3. Deterministic modeling of solidification microstructure formation in directed energy deposition fabricated Ti6Al4V
4. Microstructure and properties nonuniformity of Ti6Al4V component fabricated by high-power laser melting deposition10.1016/j.msea.2024.146604 ↗
5. Performance-control-orientated hybrid metal additive manufacturing technologies: state of the art, challenges, and future trends10.1088/2631-7990/ad3315 ↗
6. Effects of laser oscillation on metal mixing, microstructure, and mechanical property of Aluminum–Copper welds10.1016/j.ijmachtools.2023.104020 ↗
7. Effect of beam oscillating amplitude on formation characteristics and mechanical properties of laser-arc hybrid welded 8-mm-thick aluminum alloy T-joints10.1016/j.optlastec.2025.112676 ↗
8. Wear and corrosion resistance of TiAlSi-Nix (x = 0, 5, 11, 17, 23 at%) multi-principal component alloy coating prepared by ∞ oscillating laser cladding10.1016/j.jallcom.2024.175677 ↗
9. Microstructural characteristics and mechanical properties of Al-Cu alloys fabricated via 8-shaped oscillating laser wire additive manufacturing10.1016/j.msea.2024.147101 ↗
10. Mechanical properties improvement of nickel-based alloy 625 fabricated by powder-fed laser additive manufacturing based on linear beam oscillation10.1016/j.msea.2022.143054 ↗
11. Reduction of pores by means of laser beam oscillation during remote welding of AlMgSi10.1016/j.optlaseng.2018.04.012 ↗
12. Analysis of copper sheets welded by fiber laser with beam oscillation10.1016/j.optlastec.2020.106563 ↗
13. Optimization of the solidification conditions by means of beam oscillation during laser beam welding of aluminum10.1016/j.matdes.2018.11.009 ↗
14. TiC reinforced Ti6Al4V fabricated by circular oscillating laser directed energy deposition: microstructure and wear resistance10.1016/j.optlastec.2024.112011 ↗
15. Laser-arc hybrid additive manufacturing of stainless steel with beam oscillation
16. Laser spheroidization combined with coaxial powder feeding: A novel strategy for preparing spherical powders for additive manufacturing10.1016/j.jmapro.2025.01.062 ↗
17. Machine learning applications in welding processes: Progresses and opportunities10.1016/j.ijmachtools.2025.104344 ↗
18. Numerical study of keyhole dynamics and porosity formation during high-power oscillating laser welding of medium-thick aluminum alloy plates10.1016/j.ijheatmasstransfer.2022.123084 ↗
19. Numerical and experimental investigation of heat transfer and flow in oscillating laser dual-wire deposition10.1016/j.ijthermalsci.2025.109741 ↗
20. A Simplified model for numerical simulation of laser metal deposition process with beam oscillation10.1088/1742-6596/1109/1/012006 ↗
21. Laser metal deposition of Ti-6Al-4V alloy with beam oscillation10.1016/j.procir.2018.08.090 ↗
22. Determination of beam oscillating pattern for tailoring melt flow and microstructural characteristics of laser welded Ti–6Al–4V alloy10.1016/j.ijthermalsci.2024.109156 ↗
23. Microstructural evolution and performance improvement mechanism of Ti–6Al–4V fabricated by oscillating-wire laser additive manufacturing10.1016/j.jmrt.2023.04.261 ↗
24. Grain refinement and laser energy distribution during laser oscillating welding of Invar alloy10.1016/j.matdes.2019.108195 ↗
25. Influence of laser-wire interaction on heat and metal transfer in directed energy deposition10.1016/j.ijheatmasstransfer.2023.123894 ↗
26. Enhancing TC4/CFRTP joint strength through oscillating laser joining: An investigation into interfacial heat and mass transfer behaviors
27. Predicting tensile properties of Ti-6Al-4V produced via directed energy deposition10.1016/j.actamat.2017.05.025 ↗
28. Microstructural optimization through heat treatment for enhancing the fracture toughness and fatigue crack growth resistance of selective laser melted Ti6Al4V alloy10.1016/j.actamat.2019.03.003 ↗
29. Superior strength-ductility synergy in laser-additive manufactured Ti60 alloy via carbon-driven α₂ phase refinement and pyramidal 〈c + a〉 dislocation activity10.1016/j.actamat.2026.122338 ↗
30. Examination of the twinning activity in additively manufactured Ti-6Al-4V10.1016/j.matdes.2018.02.015 ↗
31. In-situ nitrogen strengthening of selective laser melted Ti6Al4V with superior mechanical performance
32. Review on direct metal laser deposition manufacturing technology for the Ti-6Al-4V alloy10.1007/s00170-019-04851-3 ↗
33. situ tailoring microstructure in additively manufactured Ti-6Al-4V for superior mechanical performance10.1016/j.actamat.2016.12.027 ↗
34. Additive manufacturing of strong and ductile Ti–6Al–4V by selective laser melting via in situ martensite decomposition10.1016/j.actamat.2014.11.028 ↗
35. Microstructure and properties nonuniformity of Ti6Al4V component fabricated by high-power laser melting deposition10.1016/j.msea.2024.146604 ↗
36. A novel magnetic field assisted powder arc additive manufacturing for Ti60 titanium alloy: Method, microstructure and mechanical properties
37. Additive manufacturing of metallic components–Process, structure and properties10.1016/j.pmatsci.2017.10.001 ↗
38. On the role of the powder stream on the heat and fluid flow conditions during directed energy deposition of maraging steel—multiphysics modeling and experimental validation
39. Regulating oxide behavior and forming stability of arc-directed energy deposition in 7075 aluminum alloy via beam oscillation
40. Partially melted powder in laser based directed energy deposition: Formation mechanism and its influence on microstructure10.1016/j.ijmachtools.2023.104072 ↗
41. Enhanced strength-ductility synergy in laser directed energy deposited IN718 superalloys through heterogeneous deformation nanostructures10.1016/j.ijmachtools.2025.104280 ↗
42. Investigation of thermal-fluid dynamics in directed energy deposition of 316 L stainless steel with laser beam oscillation10.1016/j.ijheatmasstransfer.2025.127267 ↗
43. Ultra grain refinement and mechanical properties improvement of all-weld-metal for medium-thick Al-Li alloy via laser beam oscillation and in-situ alloying10.1016/j.optlastec.2023.109965 ↗
44. Steady state columnar and equiaxed growth of dendrites and eutectic10.1016/0025-5416(84)90201-5 ↗
45. Laser-directed energy-deposited Ti-6Al-4V: The anisotropy of its microstructure, mechanical properties, and fracture behavior10.3390/ma18102360 ↗
46. Molten pool behaviors and forming characteristics in wire-laser directed energy deposition with beam oscillation10.1016/j.jmatprotec.2024.118326 ↗
47. The Interdependence Theory: the relationship between grain formation and nucleant selection10.1016/j.actamat.2011.04.035 ↗
48. Drop and hump behaviors in robotic arc-directed energy deposition with vertical position
49. Tailoring the microstructure and mechanical properties of laser directed energy deposited Inconel 718 alloy via thermostatic substrate heating10.1016/j.msea.2024.146868 ↗
50. Tailoring laser directed energy deposited Ti6Al4V titanium alloy for superior and isotropic mechanical properties by interlayer pause—intertrack pause cooling strategy
51. Strengthening effect in laser metal deposited Ti6Al4V alloy via layer-by-layer ultrasonic impact treatment10.1016/j.msea.2023.145693 ↗
52. ASTM B381–13, Standard specification for titanium and titanium alloy forgings. ASTM International, 2013. https://www.astm.org/standards/b381.
53. Simultaneous improvement of strength and ductility of laser additively produced Ti6Al4V by adding tantalum10.1016/j.jallcom.2023.173171 ↗
54. Microstructure and high strength–ductility synergy of Ti–6Al–4V alloy induced by joule heat treatment10.1007/s10853-018-2794-2 ↗
55. Strengthening contributions of dislocations and twins in warm-rolled TWIP steels10.1016/j.ijplas.2021.103198 ↗
56. Gradient microstructure evolution in laser shock peened Ti6Al4V titanium alloy10.1016/j.surfcoat.2022.128378 ↗
57. Microstructural evolution and anisotropic regulation in tensile property of cold metal transfer additive manufactured Ti6Al4V alloys via ultrasonic impact treatment10.1016/j.msea.2022.144177 ↗
58. Modelling strengthening mechanisms in beta-type Ti alloys10.1016/j.msea.2019.04.027 ↗
59. High dislocation density–induced large ductility in deformed and partitioned steels10.1126/science.aan0177 ↗
60. Interdependent slip and twinning behaviors for improving cryogenic mechanical properties in Ti-6Al-3Nb-2Zr-1Mo alloy additively manufactured by electron beam wire-fed10.1016/j.ijplas.2025.104390 ↗
61. Coarsening of martensite with multiple generations of twins in laser additively manufactured Ti6Al4V10.1016/j.actamat.2021.116954 ↗
62. Achieving strength-ductility synergy in zirconium via ultra-dense twin-twin networks10.1016/j.actamat.2024.119825 ↗