journal article·2015-03

Indentation hardness and fatigue of the constituents of WC–Co composites

Marek Bľanda, Annamaria Duszová, Tamás Csanádi, Pavol Hvizdoš, František Lofaj, Ján Dusza

Publisher page

Abstract

Abstract The hardness, reduced modulus and indentation fatigue of the constituents of WC–Co cemented carbides have been investigated at a nanolevel using instrumented indentation in the range of applied loads from 0.25 mN to 50 mN. The influence of indentation load, microstructure, heat treatment and crystallographic orientation of WC grains/crystals has been studied. During random indentation a wide range of hardness values are connected with “mix-mode” indents, when under the indent, in its plastic/process zone not only one phase is present. Heat treatment has only a slight effect on the hardness of the constituent phases. An evident load–size effect was found during the indentation of WC grains but this was absent in the case of the Co binder. Significant influence of the crystallographic orientation of WC crystals on the hardness, indentation modulus and indentation fatigue has been found with enhanced properties in the basal plane.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (23)

Show source-provided references
1. Physical and chemical nature of cemented carbides
2. Deformation and fracture properties and the physical metallurgy of WC–Co hard metals10.1179/imr.1988.33.1.90 ↗
3. Morphology of WC grains in WC–Co alloys10.1016/j.msea.2007.09.019 ↗
4. Hardness anisotropy and slip in WC crystals
5. Plastic properties in tungsten monocarbide
6. Constituent phase nanoindentation of WC/Co and Ti(C,N) hard metals10.1016/0921-5093(95)10099-7 ↗
7. Nanoindentation study of WC–12Co hard metals obtained from nanocrystalline powders: evaluation of hardness and modulus on individual phases10.1016/j.msea.2010.01.026 ↗
8. Effect of crystal anisotropy on the mechanical properties of WC embedded in WC–Co cemented carbides
9. Hardness of hexagonal tungsten carbide crystals as a function of orientation10.1016/j.actamat.2012.07.056 ↗
10. Nanoindentation of WC–Co hard metals10.1016/j.jeurceramsoc.2012.12.018 ↗
11. Elevated temperature fatigue testing of hard metals using notched testpieces10.1016/j.ijrmhm.2007.01.007 ↗
12. On the fatigue crack growth behaviour of WC–Co cemented carbides: kinetics description, microstructural effects and fatigue sensitivity10.1016/S1359-6454(02)00071-X ↗
13. Contact fatigue behavior of PVD-coated hard metals10.1016/j.ijrmhm.2008.05.003 ↗
14. Indentation fatigue of WC–Co cemented carbides10.1016/j.ijrmhm.2013.04.006 ↗
15. Gurland · 1984 · 65
16. An improved technique for determining hardness and elastic modulus using load and displacement sensing indentation experiments10.1557/JMR.1992.1564 ↗
17. Indentation load-size effect in Al2O3–SiC nanocomposites10.2478/v10187-011-0047-y ↗
18. Grinding of WC–Co hard metals10.1016/S0043-1648(00)00561-5 ↗
19. The anisotropic work hardening of WC crystals10.1016/0956-7151(92)90104-M ↗
20. Hill · 1983 · 254
21. Defect interaction in deformed WC10.1016/0001-6160(84)90031-2 ↗
22. Indentation fatigue of WC grains in composite10.1016/j.jeurceramsoc.2014.02.022 ↗
23. Orientation dependent hardness and nanoindentation induced deformation mechanisms of WC crystals