Injection molding of tungsten powder treated by jet mill with high powder loading: A solution for fabrication of dense tungsten component at relative low temperature
Source abstract
Abstract
Abstract The greater demands on final product quality of powder metallurgy processing have led to an increased demand for metal powders with high quality. In this paper we report the successful preparation of tungsten powder with a near-spherical shape and surface morphology by jet milling process, with the disappearance of agglomeration and the improvement of dispersion, narrow particle size distribution of tungsten powder was achieved. The values of D10, D50 and D90 changed from 2.02 μm, 3.67 μm and 6.34 μm to the original tungsten powder to 1.36 μm, 2.13 μm and 3.19 μm for the treated tungsten powder, respectively. The process increases apparent density and tap density from 3.71 g/cm3, 5.54 g/cm3 to 5.71 g/cm3, 8.47 g/cm3. Due to the optimization of the powder characteristics, the powder loading of the feedstock was raised to 65 vol% for the treated powder. The sintered samples of 65 vol% powder loading is easy to get sinter densification with no cracks and has superior hardness and microstructure at a relative low temperature of 1900 °C.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (18)
Show source-provided references
1. Development of a powder metallurgy process for tungsten components10.1016/j.fusengdes.2008.06.022 ↗
2. Development of tungsten and tungsten alloys for DEMO divertor applications via MIM technology10.1016/j.jnucmat.2013.01.004 ↗
3. German · 1997
4. High energy milling on tungsten powders10.1016/j.ijrmhm.2014.06.025 ↗
5. Fabrication and characterization of pure tungsten using the hot-shock consolidation10.1016/j.ijrmhm.2013.09.008 ↗
6. The relationship between the green density and as-sintered density of nano-tungsten compacts10.1016/j.ijrmhm.2015.07.006 ↗
7. Dimension precision of metal injection molded pure tungsten10.1016/j.ijrmhm.2008.10.003 ↗
8. Experimental and numerical analysis of the particle size effect on the densification behaviour of metal injection moulded tungsten parts during sintering10.1016/j.powtec.2014.10.019 ↗
9. Powder injection molding – an innovative manufacturing method for He-cooled DEMO divertor components10.1016/j.fusengdes.2011.01.009 ↗
10. Effect of mixing on the rheology and particle characteristics of tungsten-based powder injection molding feedstock10.1016/S0921-5093(03)00146-1 ↗
11. Injection molding of surface modified powders with high solid loadings: a case for fabrication of translucent alumina ceramics10.1016/j.jeurceramsoc.2011.03.003 ↗
12. Effect of powder loading on metal injection molding stainless steels10.1016/j.jmatprotec.2006.10.039 ↗
13. Influence of process parameters on the characteristics of TiAl alloyed powders by fluidized bed jet milling10.1016/j.powtec.2013.11.013 ↗
14. A study of jet-milling and spray-drying process for the physicochemical and aerodynamic dispersion properties of amiloride HCl10.1016/j.powtec.2014.04.066 ↗
15. Influence of jet milling process parameters on particle size, phase formation and magnetic properties of MnBi alloy10.1016/j.jallcom.2014.12.202 ↗
16. Net shaping of tungsten components by micro powder injection moulding10.1016/j.fusengdes.2007.07.013 ↗
17. The charging efficiency and flow dynamics of micropowder during jet milling/electrostatic dispersion10.1016/j.powtec.2014.02.007 ↗
18. German · 2014