Conversion of W2C to WC phase during mechano-chemical synthesis of nano-size WC–Al2O3 powder using WO3–2Al–(1 + x)C mixtures
Source abstract
Abstract
Abstract Due to the weak properties of W2C phase, its formation during the process of WC synthesis should be prevented. The aim of the present study has been the mechano-chemical synthesis of a WC–Al2O3 composite powder free from undesirable W2C phase through the addition of excess carbon to the WO3–2Al–C initial mixture. Based on the thermodynamic calculations and results of the supplementary experiments in W–yC and W2C–C systems, the possibility of the conversion of W2C to WC phase through the addition of excess carbon has been investigated. It has been shown that production of a WC–Al2O3 composite powder by 360 min mechano-chemical treatment of an initial mixture of WO3–2Al–1.8C is possible. TEM observations and Williamson–Hall calculation revealed that the obtained WC–Al2O3 powder contains macro-size agglomerates in which each agglomerate consists of nano-size phases.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (36)
Show source-provided references
1. Lassner · 1999
2. Upadhyaya · 1998
3. Synthesis, sintering, and mechanical properties of nanocrystalline cemented tungsten carbide—a review10.1016/j.ijrmhm.2008.07.011 ↗
4. Yao
5. Vallance · 2008
6. Effects of ball milling time on the synthesis and consolidation of nanostructured WC–Co composites10.1016/j.ijrmhm.2009.05.006 ↗
7. El-Eskandarany · 2001
8. The science and technology of mechanical alloying10.1016/S0921-5093(00)01465-9 ↗
9. Production of nanostructured WC–Co powder by ball milling10.1016/j.ijrmhm.2008.06.005 ↗
10. Synthesis and characterizations of ball-milled nanocrystalline WC and nanocomposite WC–Co powders and subsequent consolidations10.1016/S0925-8388(00)01155-5 ↗
11. Fabrication of nanocrystalline WC and nanocomposite WC–MgO refractory materials at room temperature10.1016/S0925-8388(99)00508-3 ↗
12. Fabrication and characterizations of new nanocomposite WC/Al2O3 materials by room temperature ball milling and subsequent consolidation10.1016/j.jallcom.2004.08.064 ↗
13. Preparation of alumina–tungsten carbide nanocomposite by mechano-chemical reduction of WO3 with aluminum and graphite10.1016/j.jallcom.2009.11.019 ↗
14. Effect of the aluminum content on the behavior of mechanochemical reactions in the WO3–C–Al system10.1016/j.jallcom.2009.02.088 ↗
15. Control of carbon loss during synthesis of WC powder through ball milling of WO3–C–2Al mixture10.1016/j.jallcom.2009.06.169 ↗
16. Room temperature reduction of scheelite (CaWO4)10.1557/JMR.1999.0088 ↗
17. Novel route to submicrometer tungsten carbide10.1002/aic.690460109 ↗
18. Cutting performance and failure mechanisms of an Al2O3/WC/TiC micro- nano-composite ceramic tool10.1016/j.ijrmhm.2009.11.007 ↗
19. Bulk WC–Al2O3 composites prepared by spark plasma sintering10.1016/j.ijrmhm.2011.07.003 ↗
20. Influence of sintering temperature and holding time on the densification, phase transformation, microstructure and properties of hot pressing WC–40 vol.%Al2O3 composites10.1016/j.ceramint.2011.09.016 ↗
21. Master sintering curve of nanocomposite WC–MgO powder compacts10.1016/j.jallcom.2011.12.091 ↗
22. Two-step hot-pressing sintering of nanocomposite WC–MgO compacts10.1016/j.jeurceramsoc.2011.04.001 ↗
23. X-ray line broadening from filed aluminium and wolfram10.1016/0001-6160(53)90006-6 ↗
24. Self-sustaining reactions induced by ball milling10.1016/S0079-6425(01)00002-0 ↗
25. Ball milling-induced reduction of MoS2 with Al10.1007/s10853-006-0950-6 ↗
26. Effect of material characteristics on the ignition of the combustion reactions induced by ball milling10.1016/S0924-0136(01)01000-7 ↗
27. Metal–metal oxides prepared by MSR and SHS techniques10.1016/S0167-2738(01)00799-8 ↗
28. POWDER CELL—a program for the representation and manipulation of crystal structures and calculation of the resulting X-ray powder patterns10.1107/S0021889895014920 ↗
29. Characterization of milled Si3N4 powder using X-ray peak broadening and surface area analysis10.1007/BF00356667 ↗
30. Choice of collimators for a crystal spectrometer for neutron diffraction10.1016/0369-643X(58)90029-X ↗
31. Culity · 1978
32. Synthesis of Al2O3–NbC by reactive milling and production of nanocomposites10.1016/S0924-0136(03)00411-4 ↗
33. Synthesis of nanocrystalline cubic substoichiometric WC1−z powders by mechanochemical technology10.1023/A:1004880221909 ↗
34. Synthesis of Al2O3–WC composite powder by SHS process10.1023/A:1004764030163 ↗
35. Effect of C and milling parameters on the synthesis of WC powders by mechanical alloying10.1016/j.ijrmhm.2009.09.006 ↗
36. Synthesis of metastable tungsten carbide nanoparticles by mechanochemical alloying process10.4028/www.scientific.net/AMR.66.135 ↗