Crack deflection in tungsten carbide based laminates
Source abstract
Abstract
Abstract Laminate materials were manufactured by alternating WC–6%Co layers with equal thickness layers of one of the following compositions: WC–16%Co, WC–16%Ni, Co, a W–Ni–Fe alloy, and Ni. One composition used WC–6%Ni in place of WC–6%Co, layered with the W–Ni–Fe alloy. Flexure specimens, consisting of nine alternating layers, were fabricated with either WC–6%Co or WC–6%Ni on the tensile surface of the specimen. The ability of these composites to deflect or arrest cracks was investigated in four point bending. Two of the compositions, WC–6%Co/W–Ni–Fe and WC–6%Co/Ni, exhibited the ability to fail non-catastrophically, showing inelastic work of fracture as high as 34,400 J/m 2 .
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (17)
Show source-provided references
1. Brookes · 1996
2. Fracture resistant super hard materials and hardmetals composite with functionally designed microstructure10.1016/S0263-4368(01)00031-2 ↗
3. A simple way to make tough ceramics10.1038/347455a0 ↗
4. Fibrous monoliths: Non-brittle fracture from powder processed ceramics10.1016/0921-5093(94)06525-X ↗
5. Fibrous monolithic ceramics10.1111/j.1151-2916.1997.tb03148.x ↗
6. Fibrous monolithic ceramics: I, fabrication, microstructure, and indentation behavior10.1111/j.1151-2916.1993.tb07756.x ↗
7. Fibrous monolithic ceramics: II, flexural strength and fracture behavior of the silicon carbide/graphite system10.1111/j.1151-2916.1993.tb07757.x ↗
8. Crack deflection in ceramic laminates using porous interlayers10.1016/S0955-2219(98)00134-4 ↗
9. Crack bifurcation in laminar ceramic composites10.1111/j.1151-2916.1996.tb08003.x ↗
10. Kinking of a crack out of an interface10.1115/1.3176078 ↗
11. Microstructual aspects of the strength and hardness of cemented tungsten carbide
12. Askeland · 1994
13. Fabrication and crack deflection in ceramic laminates with porous interlayers10.1111/j.1151-2916.2000.tb01563.x ↗
14. Preparation, microstructure and mechanical properties of SiC–SiC and B4C–B4C laminates10.1016/j.jssc.2003.02.007 ↗
15. Effect of porous interlayers on crack deflection in ceramic laminates10.1016/S0955-2219(03)00338-8 ↗
16. Optimizing the mechanical properties of injection molded W–4.9%Ni–2.1%Fe in debinding10.1016/S0924-0136(97)00095-2 ↗
17. Fibrous monolithic ceramics: IV, mechanical properties and oxidation behavior of the alumina/nickel system10.1111/j.1151-2916.1994.tb05400.x ↗