journal article·2017-12

Influence of WC and cobalt additions on the microstructural and mechanical properties of TiCN-Cr 3 C 2 -nano-TiB 2 cermets fabricated by spark plasma sintering

E. Shankar, S. Balasivanandha Prabu

Publisher page

Abstract

Abstract This paper reports the effect of tungsten carbide (WC) and cobalt (Co) addition on the microstructural and mechanical properties of titanium carbonitride (TiCN) cermets modified by Cr3C2 and nano-TiB2 addition, processed by spark plasma sintering (SPS). The addition of the WC and Co was varied from 0 to 15 wt%. The microstructure, hardness and fracture toughness of the developed cermets were studied. The hardness and fracture toughness of the cermets increased to 52% and 33%, respectively with WC additions. With Co additions the hardness decreased by 13%, but the fracture toughness increased by 9%. The cermet with 60%TiCN-15%WC-15%Co-5%Cr2C3-5% nano-TiB2 composition has shown balanced improvement in hardness (19.1 GPa) and toughness (8.4 MPa·m1/2). The machining performed by this cermet, developed minimum cutting force and surface roughness on the machined surface of the EN24 workpiece material.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (27)

Show source-provided references
1. Microstructure and mechanical properties of ultrafine Ti(CN)-based cermets fabricated from nano/submicron starting powders10.1016/j.ceramint.2004.09.013 ↗
2. Effect of nano addition on the microstructures and mechanical properties of Ti(C, N)-based cermets10.1016/j.ceramint.2004.04.005 ↗
3. Effect of nano-micro TiN addition on the microstructure and mechanical properties of TiC based cermets10.1016/S0955-2219(02)00010-9 ↗
4. Effect of WC on the microstructure and mechanical properties of nano Ti(C,N)-based cermets10.1016/j.ijrmhm.2012.05.009 ↗
5. Phase evolution and microstructure characteristics of ultrafine Ti(C,N)-based cermet by spark plasma sintering10.1016/j.ijrmhm.2004.03.002 ↗
6. Fabrication of nanocomposite Ti(C,N)-based cermet by spark plasma sintering10.1016/j.matchemphys.2004.12.031 ↗
7. Effect of SiC nano-whisker addition on TiCN-based cermets prepared by spark plasma sintering10.1016/j.ijrmhm.2012.03.008 ↗
8. Microstructure evolution and phase transformation during spark plasma sintering of Ti(C,N)-based cermets10.1016/j.ijrmhm.2007.08.001 ↗
9. Effect of VC addition on sinterability and microstructure of ultrafine Ti(C, N)-based cermets in spark plasma sintering10.1016/j.jallcom.2007.05.091 ↗
10. Microstructure and mechanical properties of Ti(C, N) based cermets reinforced with different ceramic particles processed by spark plasma sintering10.1016/j.ceramint.2017.05.103 ↗
11. Ti (C, N) cermets—metallurgy and properties10.1016/0263-4368(95)00027-G ↗
12. Effect of WC content on the microstructure and mechanical properties of (Ti,W)(C,N)–Co cermets10.1016/j.ijrmhm.2007.01.003 ↗
13. Effect of WC and group IV carbides on the cutting performance of Ti(C,N) cermet tools10.1016/j.ijmachtools.2003.10.023 ↗
14. The effect of WC, Mo2C, TaC content on the microstructure and properties of ultra-fine TiC0.7N0.3 cermet10.1016/j.matdes.2006.03.005 ↗
15. Effect of WC content on the microstructure and mechanical properties of Ti(C0.5N0.5)–WC–Mo–Ni cermets10.1016/j.ijrmhm.2009.10.005 ↗
16. Development of TiCN-based cermets: mechanical properties and wear mechanism10.1016/j.ijrmhm.2012.07.001 ↗
17. Titanium diboride composite with improved sintering characteristics10.1016/j.ijrmhm.2014.06.008 ↗
18. Influence of hot pressing sintering temperature and time on microstructure and mechanical properties of TiB2/TiN tool material10.1016/j.msea.2012.03.002 ↗
19. Cutting and wearing characteristics of TiC-based cermets cutters with nano-TiN addition10.1016/j.jmatprotec.2004.07.087 ↗
20. The milling performances of TiC-based cermet tools with TiN nanopowders addition against normalized medium carbon steel AISI104510.1016/j.wear.2004.11.022 ↗
21. Crater wear mechanisms of Ti(C,N)–Ni–WC cermets during dry machining10.1016/j.ijrmhm.2006.12.001 ↗
22. Effects of Cr3C2 addition on the corrosion behavior of Ti(C, N)-based cermets
23. Effects of Cr3C2 addition on the erosion–corrosion behavior of Ti(C,N)-based cermets10.1016/j.ceramint.2013.01.016 ↗
24. Erosion–corrosion behavior of Ti(C,N)-based cermets with different TiN contents10.1016/j.ijrmhm.2013.10.006 ↗
25. Erosive wear behavior of Ti(C,N)-based cermets containing different Cr3C2 addition in slurry conditions10.1016/j.ijrmhm.2014.03.013 ↗
26. Indentation fracture of WC–Co cermets10.1007/BF00555296 ↗
27. Titanium carbonitride-based cermets: processes and properties10.1016/0921-5093(93)90588-6 ↗