Improvements in Surface Integrity and Rotating Bending Fatigue Strength of CuZn39Pb3 Brass via a Conventional Diamond-Burnishing Process
Source abstract
Abstract
CuZn39Pb3 leaded brass is one of the most widely used alloys in machining. Despite its good machinability, there is a lack of information in the literature on the effects of surface cold working on the surface microhardness, microhardness profile, introduced residual stresses, microstructure, and the operating behaviour of machined components. This article reveals the capabilities of conventional diamond burnishing (DB) (implemented under flood-lubrication conditions) to improve the surface integrity and high- and mega-cycle fatigue strength of CuZn39Pb3 cylindrical components such as axles and shafts. The results show that both the smoothing and hardening DB processes achieve mirror-like surfaces, introduce significant residual compressive stresses at depths greater than 0.5 mm, and significantly increase the fatigue strength in the high- and mega-cycle regions compared to the reference condition (turned and polished specimens). However, the surface microhardness is weakly affected by the degree of surface cold working. Given the almost identical microhardness profiles and the equivalent distribution in depth of the introduced residual stresses by the two DB processes, the possible reason for the more pronounced effect of the hardening process on the fatigue strength lies in the thicker affected layer and the reduced negative skewness introduced by this process.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Surface Treatment and Residual Stress · Erosion and Abrasive Machining · High Entropy Alloys Studies
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
Department of Material Science and Mechanics of Materials, Technical University of Gabrovo, 5300 Gabrovo, Bulgaria
Center of Competence “Smart Mechatronic, Eco-and Energy-Saving Systems and Technologies”, Technical University of Gabrovo, 5300 Gabrovo, Bulgaria
Department of Mechanical Engineering Equipment and Technologies, Technical University of Gabrovo, 5300 Gabrovo, Bulgaria
Department of Industrial Design and Textile Engineering, Technical University of Gabrovo, 5300 Gabrovo, Bulgaria
Funding
European Regional Development Fund
References (51)
Show source-provided references
1. Balevski, A. (1988). Metal Science, Technika.
2. The Mechanical Properties of Brass Alloys: A Review
3. Forging of Zinc Alloys—A Feasibility Study
4. Kaleycheva, J. (2018). Metal Science, Scientific and Technical Union of Mechanical Engineering “Industria 4.0”.
5. Influence of tool coating, tool material, and cutting speed on the machinability of low-leaded brass alloys in turning10.1080/10426914.2015.1127944 ↗
6. Machinability enhancement of lead-free brass alloys10.1016/j.procir.2014.03.018 ↗
7. Experimental investigation of machinability parameters in turning of CuZn39Pb3 brass alloy10.1016/j.prostr.2018.09.046 ↗
8. Multi-response optimization of CuZn39Pb3 brass alloy turning by implementing Grey Wolf algorithm10.3221/IGF-ESIS.50.49 ↗
9. Comparative study on the machinability of lead-free brass10.1016/j.jclepro.2017.02.098 ↗
10. Cutting forces, tool wear and surface finish in high speed diamond machining10.1016/j.precisioneng.2017.02.018 ↗
11. The friction and wear properties of CuZn39PB3 alloys under atmospheric and vacuum conditions10.1016/j.wear.2013.10.003 ↗
12. On the function of lead (Pb) in machining brass alloys10.1007/s00170-022-09205-0 ↗
13. Anastasov, K., Ichkova, M., Todorov, V., and Daskalova, P. (2025). The Effect of Optimised Combined Turning and Diamond Burnishing Processes on the Roughness Parameters of CuZn39Pb3 Alloys. Appl. Sci., 15.10.3390/app152413075 ↗
14. Effects of diamond burnishing on surface integrity, fatigue, wear, and corrosion of metal components—Review and perspectives10.1007/s00170-025-16158-7 ↗
15. Modeling and experimental validation of force—Surface roughness relation for smoothing burnishing with a spherical tool10.1016/j.ijmachtools.2007.03.002 ↗
16. Maximov, J., and Duncheva, G. (2025). Improvements in the Surface Integrity and Operating Behaviour of Metal Components Through Slide Burnishing with Non-Diamond-Based Deforming Elements: Review and Perspectives. Appl. Sci., 15.10.3390/app152212182 ↗
17. Finite Element Analysis and optimization of spherical motion burnishing of low-alloy steel10.1177/0954406211412024 ↗
18. Korzynski, M. (2013). Slide diamond burnishing. Nonconventional Finishing Technologies, Polish Scientific Publisher.
19. Skoczylas, A., Zaleski, K., and Matuszak, J. (2025). Evaluation of the Effectiveness of Surface Defect Removal by Slide Burnishing. Appl. Sci., 15.10.3390/app15137398 ↗
20. Skoczylas, A., and Klonica, M. (2023). Selected properties of the surface layer of C45 steel samples after slide burnishing. Materials, 16.10.3390/ma16196513 ↗
21. Kebede, F.T., Felho, C., and Sztankovics, I. (2025). Improving Surface Roughness of 42CrMo4 Low Alloy Steel Shafts by Applying Varying Feed in the Multi-Pass Slide Burnishing Process. Appl. Sci., 15.10.3390/app15169063 ↗
22. Smoothing, deep or mixed diamond burnishing of low-alloy steel components—Optimization procedures10.1007/s00170-019-04747-2 ↗
23. Slide diamond burnishing of tool steels with adhesive coatings and diffusion layers10.1179/1433075X12Y.0000000060 ↗
24. Structure and properties of burnished and nitrided AISI D2 tool steel
25. Maximov, J.T., Duncheva, G.V., Anchev, A.P., Dunchev, V.P., Argirov, Y.B., and Nikolova, M.P. (2023). Effects of heat treatment and diamond burnishing on fatigue behaviour and corrosion resistance of AISI 304 austenitic stainless steel. Appl. Sci., 13.10.3390/app13042570 ↗
26. Maximov, J.T., Duncheva, G.V., Anchev, A.P., Dunchev, V.P., and Argirov, Y.B. (2022). Effect of Diamond Burnishing on Fatigue Behaviour of AISI 304 Chromium-Nickel Austenitic Stainless Steel. Materials, 15.10.3390/ma15144768 ↗
27. Varga, G., Dezso, G., and Szigeti, F. (2022). Surface roughness improvement by sliding friction burnishing of parts produced by selective laser melting of Ti6Al4V titanium alloy. Machines, 10.10.3390/machines10050400 ↗
28. Surface Hardness Modification of Selective Laser Melted Ti6Al4V Parts by Sliding Friction Diamond Burnishing10.3311/PPme.21124 ↗
29. Impact of slide diamond burnishing additional parameters on fatigue behaviour of 2024-T3 Al alloy10.1111/ffe.12915 ↗
30. Effect of machining parameters on surface properties in slide diamond burnishing of aluminium matrix composites10.1016/j.matpr.2015.05.033 ↗
31. Multi-objective optimization of internal diamond burnishing process10.1080/10426914.2021.1981937 ↗
32. Enhancement of the wear resistance of CuAl9Fe4 sliding bearing bushings via diamond burnishing10.1016/j.wear.2022.204491 ↗
33. Investigation of the burnishing process with PCD tool on non-ferrous metals10.1007/s00170-003-1959-5 ↗
34. The effect of ball- and roller-burnishing on the surface roughness and hardness of some non-ferous metals10.1016/S0924-0136(97)00199-4 ↗
35. Burnishing force and number of passes for the optimum surface finish of brass components10.1016/S0924-0136(98)00058-2 ↗
36. Improvement in the wear resistance of brass components by the ball burnishing process10.1016/S0924-0136(99)00254-X ↗
37. Experimental investigation of the influence of burnishing tool passes on surface roughness and hardness of brass specimens10.17485/ijst/2011/v4i9.32 ↗
38. Experimental investigation of the influence of burnishing parameters on surface roughness and hardness of brass alloy
39. Effect of ball burnishing medium on the surface characteristics of free machining brass
40. Mechanical properties analysis of burnished brass10.12913/22998624/205836 ↗
41. Surface plastic deformation of leaded brass components using a Ferro-Tic Grade C cylindrical-ended deforming element
42. Maximov, J.T., and Duncheva, G.V. (2023). The correlation between surface integrity and operating behaviour of slide burnished components—A review and prospects. Appl. Sci., 13.10.3390/app13053313 ↗
43. Modeling of Residual Stress Distribution around Fastener Holes in Thin Plates after Symmetric Cold Expansion10.1007/s40430-013-0090-2 ↗
44. (1983). Metals—Fatigue Test Methods (Standard No. Bulgarian National Standard 5297:1983). (In Bulgarian).
45. A fast and elitist multiobjective genetic algorithm: NSGA-II10.1109/4235.996017 ↗
46. Vuchkov, I.N., and Vuchkov, I.I. (QStatLab Professional, 2009). QStatLab Professional, version 6.1.1.3; Statistical Quality Control Software, User’s Manual.
47. Correlation between standard roughness parameters skewness and kurtosis and tribological behaviour of contact surface10.1016/j.triboint.2011.11.008 ↗
48. Improvement in Wear Resistance Performance of CuAl8Fe3 Single-Phase Aluminum Bronze via Slide Diamond Burnishing10.1007/s11665-021-06389-6 ↗
49. Maximov, J., Duncheva, G., Anchev, A., Dunchev, V., and Argirov, Y. (2024). Improvement in Fatigue Strength of Chromium–Nickel Austenitic Stainless Steels via Diamond Burnishing and Subsequent Low-Temperature Gas Nitriding. Appl. Sci., 14.10.3390/app14031020 ↗
50. Ductility improvement of aluminum 1050A rolled sheet by a newly designed ball burnishing tool device10.1007/s00170-011-3598-6 ↗
51. The use of areal surface topography characterisation in relation to fatigue performance10.1051/matecconf/201816514013 ↗