Effect of Loading Size and Reaction Wood Proportion on Longitudinal Warping During Pressure Steaming
Source abstract
Abstract
This study evaluates the effect of loading size on the longitudinal warping of beech wood containing reaction wood. Reaction wood in hardwood species has properties that negatively affect not only the usability of wood products but also the processing of the wood in which it is found. To investigate these effects, steam pressure treatment and three levels of mechanical loading (700, 2000, 4000 kg·m−2) were used, along with the effect of the proportion of reaction wood. Steam pressure treatment generally caused greater warping, particularly in unloaded specimens, due to increased release of internal growth stresses. Mechanical loading effectively reduced deformation, with the most pronounced effects observed at 700 and 2000 kg·m−2; further increases in loading did not provide any significant additional benefits. Although the proportion of reaction wood ranged from 14% to 56%, there was no obvious statistical correlation with deformation, suggesting that the distribution and degree of development of reaction wood have a greater impact than its total content. Overall, hydrothermal treatment induces the release of internal stress, leading to warping, while moderate mechanical loading can successfully limit warping. Understanding these interactions is key to processing beech wood with reaction wood and to improving the quality of finished products.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Wood Treatment and Properties · Food Drying and Modeling · Natural Fiber Reinforced Composites
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
Department of Wood Technology, Faculty of Wood Sciences and Technology, Technical University in Zvolen, T. G. Masaryka 24, 96001 Zvolen, Slovakia
Funding
Slovak Research and Development Agency
References (22)
Show source-provided references
1. Relationship Between Growth Stress, Mechanical-Physical Properties and Proportion of Fibre with Gelatinous Layer in Chestnut (Castanea sativa Mill.)10.1515/HF.2003.028 ↗
2. Chemical reagent for detecting tension wood in selected tree species10.15376/biores.19.3.4335-4351 ↗
3. Variations in physical and mechanical properties between tension and opposite wood from three tropical rainforest species10.1007/s00226-010-0323-9 ↗
4. Kúdela, J., and Čunderlík, I. (2012). Bukové Drevo Štruktúra, Vlastnosti, Použitie, Technická Univerzita vo Zvolene (Technical University in Zvolen).
5. A model to explain microscopic mechanism of hygrothermal recovery in tension wood G-fiber10.1007/s00226-025-01706-x ↗
6. Vilkovský, P., Vilkovská, T., Klement, I., and Fúčela, M. (2025). Dimensional Stability of Beech Wood: The Influence of Taper, Slope of Annual Ring and Sawing Pattern. Polymers, 17.10.3390/polym17233158 ↗
7. Continuum contraction of tension wood fiber induced by repetitive hygrothermal treatment10.1007/s00226-015-0762-4 ↗
8. Čunderlík, I., Kúdela, J., and Bluskova, G. (1995). Relaxation of stresses in streamed beech tension wood. Lesotechničesko Obrazovanie v Bulgarija, TOM II. Visš Lesotechničeski Institute.
9. Mihulja, G., Poljak, D., and Sedlar, T. (2023). Joint Durability of Steam-Treated Beech Wood. Polymers, 15.10.3390/polym15153318 ↗
10. Gao, Z., and Huang, R. (2022). Effects of Pressurized Superheated Steam Treatment on Dimensional Stability and Its Mechanisms in Surface-Compressed Wood. Forests, 13.10.3390/f13081230 ↗
11. Ali, M.R., Abdullah, U.H., Ashaari, Z., Hamid, N.H., and Hua, L.S. (2021). Hydrothermal Modification of Wood: A Review. Polymers, 13.10.3390/polym13162612 ↗
12. The impact of drying and steaming processes on surface color changes of tension and normal beech wood10.1080/07373937.2018.1509219 ↗
13. Influence of steaming on selected wood properties of four hardwood species10.1007/s00107-007-0205-5 ↗
14. Physical, mechanical, and chemical properties of steamed beech wood
15. Bolam, F. (2018). The morphology, chemistry and pulping characteristics of reaction wood. Fundamentals of Papermaking Fibres, Transactions of the 1st Fundamental Research Symposium, Cambridge, 1957, FRC.
16. Surface physicochemical properties of surface-compressed wood subjected to superheated steam treatment under varying pressures10.1016/j.conbuildmat.2024.135444 ↗
17. Reduction of growth stresses in logs of Hieronyma alchorneoides Allemão from fast-growth plantations using steaming and heating: Effects on the quality of lumber10.1007/s13595-021-01090-z ↗
18. Warp Reduction in Young-Growth Ponderosa Pine Studs
19. Tronstad, S., Magnar, K., Sandland, K.M., and Folvik, K. (2005). Top loading. Measures for Improving Quality and Shape Stability of Sawn Softwood Timber During Drying and Under Service Conditions: Best Practice Manual to Improve Straightness of Sawn Timber, VTT Technical Research Centre of Finland.
20. (2007). Quality Sorting of Hardwood Logs (Standard No. STN EN 48 0056).
21. (1979). Determination of Moisture Content of the Physical Mechanical Tests (Standard No. STN EN 49 0103).
22. (1993). Wood. Determination of Density (Standard No. STN EN 49 0108).