Advancements in titanium nanocomposites: Microstructure and fretting wear resistance via spark plasma sintering
Source abstract
Abstract
This study investigated enhancing the wear resistance of Ti6Al4V alloys for medical applications by incorporating TiC nano-reinforcements using advanced spark plasma sintering (SPS). The addition of up to 2.5wt% TiC significantly improved the mechanical properties, including a notable 18.2% increase in hardness (HV 332). Fretting wear tests against 316L stainless steel (SS316L) balls demonstrated a 20wt%–22wt% reduction in wear volume in the Ti6Al4V/TiC composites compared with the monolithic alloy. Micro-structural analysis revealed that TiC reinforcement controlled the grain orientation and reduced the β-phase content, which contributed to enhanced mechanical properties. The monolithic alloy exhibited a Widmanstätten lamellar microstructure, while increasing the TiC content modified the wear mechanisms from ploughing and adhesion (0–0.5wt%) to pitting and abrasion (1wt%–2.5wt%). At higher reinforcement levels, the formation of a robust oxide layer through tribo-oxide treatment effectively reduced the wear volume by minimizing the abrasive effects and plastic deformation. This study highlights the potential of SPS-mediated TiC reinforcement as a transformative approach for improving the performance of Ti6Al4V alloys, paving the way for advanced medical applications.
Source: expertdata · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Titanium Alloys Microstructure and Properties · Aluminum Alloys Composites Properties · Advanced materials and composites
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (54)
Show source-provided references
1. M. Geetha, A.K. Singh, R. Asokamani, and A.K. Gogia, Ti based biomaterials, the ultimate choice for orthopaedic implants—A review, Prog. Mater. Sci., 54(2009), No. 3, p. 397.10.1016/j.pmatsci.2008.06.004 ↗
2. B. Lal, A. Dey, and M.F. Wani, Effect of frictional heating on mechanically mixed layers during dry sliding contact of Ti–6Al–4V alloys at high temperature in vacuum condition, Surf. Rev. Lett., 29(2022), No. 10, art. No. 2250127.10.1142/S0218625X2250127X ↗
3. C. Veiga, J.P. Davim, and A.J.R. Loureiro, Properties and applications of titanium alloys: A brief review, Rev. Adv. Mater. Sci., 32(2012), No. 2, p. 133.
4. J.A. Pachore, S.V. Vaidya, C.J. Thakkar, H.K.P. Bhalodia, and H.M. Wakankar, ISHKS joint registry: A preliminary report, Indian J. Orthop., 47(2013), No. 5, p. 505.10.4103/0019-5413.118208 ↗
5. P. Kovacs, J.A. Davidson, and K. Daigle, Correlation between the metal ion concentration and the fretting wear volume of orthopaedic implant metals, [in] K.R. St. John, eds., Particulate Debris from Medical Implants: Mechanisms of Formation and Biological Consequences, ASTM International, West Conshohocken, 1992.
6. A. Shanaghi, P.K. Chu, A.R.S. Rouhaghdam, R. Xu, and T. Hu, Structure and corrosion resistance of Ti/TiC coatings fabricated by plasma immersion ion implantation and deposition on nickel–titanium, Surf. Coat. Technol., 229(2013), p. 151.10.1016/j.surfcoat.2012.07.063 ↗
7. N. Oláh, Z. Fogarassy, M. Furkó, C. Balázsi, and K. Balázsi, Sputtered nanocrystalline ceramic TiC/amorphous C thin films as potential materials for medical applications, Ceram. Int., 41(2015), No. 4, p. 5863.10.1016/j.ceramint.2015.01.017 ↗
8. X. Nie, A. Leyland, and A. Matthews, Low temperature deposition of Cr(N)/TiO2 coatings using a duplex process of unbalanced magnetron sputtering and micro-arc oxidation, Surf. Coat. Technol., 133(2000), p. 331.10.1016/S0257-8972(00)00953-1 ↗
9. J.C. Sánchez-López, D. Martínez-Martínez, C. López-Cartes, and A. Fernández, Tribological behaviour of titanium carbide/amorphous carbon nanocomposite coatings: From macro to the micro-scale, Surf. Coat. Technol., 202(2008), No. 16, p. 4011.10.1016/j.surfcoat.2008.02.012 ↗
10. A.L. Yerokhin, X. Nie, A. Leyland, and A. Matthews, Characterisation of oxide films produced by plasma electrolytic oxidation of a Ti–6Al–4V alloy, Surf. Coat. Technol., 130(2000), No. 2–3, p. 195.10.1016/S0257-8972(00)00719-2 ↗
11. Y. Vangolu, A. Alsaran, and O.S. Yildirim, Wear properties of micro arc oxidized and hydrothermally treated Ti6Al4V alloy in simulated body fluid, Wear, 271(2011), No. 9–10, p. 2322.10.1016/j.wear.2010.12.039 ↗
12. S. Banfield, J.A.B. Wilson, G. Cassar, A. Leyland, A. Matthews, and J. Housden, An investigation into the effect of triode plasma oxidation (TPO) on the tribological properties of Ti6Al4V, Surf. Coat. Technol., 206(2011), No. 7, p. 1955.10.1016/j.surfcoat.2011.08.024 ↗
13. G. Cassar, J.C. Avelar-Batista Wilson, S. Banfield, J. Housden, A. Matthews, and A. Leyland, Surface modification of Ti–6Al–4V alloys using triode plasma oxidation treatments, Surf. Coat. Technol., 206(2012), No. 22, p. 4553.10.1016/j.surfcoat.2012.05.001 ↗
14. J. Chávez, L. Olmos, O. Jiménez, D. Bouvard, E. Rodríguez, and M. Flores, Sintering behaviour and mechanical characterisation of Ti64/xTiN composites and bilayer components, Powder Metall., 60(2017), No. 4, p. 257.10.1080/00325899.2017.1280585 ↗
15. M. Choi, E. Hong, J. So, et al., Tribological properties of biocompatible Ti–10W and Ti–7.5TiC–7.5W, J. Mech. Behav. Biomed. Mater., 30(2014), p. 214.10.1016/j.jmbbm.2013.11.014 ↗
16. L.J. Huang, L. Geng, H.Y. Xu, and H.X. Peng, In situ TiC particles reinforced Ti6Al4V matrix composite with a network reinforcement architecture, Mater. Sci. Eng. A, 528(2011), No. 6, p. 2859.10.1016/j.msea.2010.12.046 ↗
17. J.I. Matsushita, T. Suzuki, and A. Sano, High temperature strength of TiB2 ceramics, J. Ceram. Soc. Japan, 101(1993), No. 1177, p. 1074.10.2109/jcersj.101.1074 ↗
18. W.J. Zhang, H.H. Liu, H. Ding, and H. Fujii, Superplastic deformation mechanism of the friction stir processed fully lamellar Ti–6Al–4V alloy, Mater. Sci. Eng. A, 785(2020), art. No. 139390.10.1016/j.msea.2020.139390 ↗
19. B. Li, Y.F. Shen, and W.Y. Hu, Surface nitriding on Ti–6Al–4V alloy via friction stir processing method under nitrogen atmosphere, Appl. Surf. Sci., 274(2013), p. 356.10.1016/j.apsusc.2013.03.060 ↗
20. Z.Q. Yan, F. Chen, Y.X. Cai, and Y.K. Zheng, Microstructure and mechanical properties of in-situ synthesized TiB whiskers reinforced titanium matrix composites by high-velocity compaction, Powder Technol., 267(2014), p. 309.10.1016/j.powtec.2014.07.048 ↗
21. A.A.M. da Silva, J.F. dos Santos, and T.R. Strohaecker, Microstructural and mechanical characterisation of a Ti6Al4V/TiC/10p composite processed by the BE-CHIP method, Compos. Sci. Technol., 65(2005), No. 11–12, p. 1749.10.1016/j.compscitech.2005.03.005 ↗
22. J.Q. Qi, H.W. Wang, C.M. Zou, and Z.J. Wei, Influence of matrix characteristics on tensile properties of in situ synthesized TiC/TA15 composite, Mater. Sci. Eng. A, 553(2012), p. 59.10.1016/j.msea.2012.05.092 ↗
23. X.W. Tao, Z.J. Yao, S.S. Zhang, J. Liao, and J. Liang, Investigation on microstructure, mechanical and tribological properties of in-situ (TiB + TiC)/Ti composite during the electron beam surface melting, Surf. Coat. Technol., 337(2018), p. 418.10.1016/j.surfcoat.2018.01.054 ↗
24. P.G. Caceres, Effect of microstructure on the abrasive wear properties of infiltrated tungsten alloys, Mater. Charact., 49(2002), No. 1, p. 1.10.1016/S1044-5803(02)00201-2 ↗
25. J.A. Hawk and D.E. Alman, Abrasive wear of intermetallic-based alloys and composites, Mater. Sci. Eng. A, 239(1997), p. 899.10.1016/S0921-5093(97)00681-3 ↗
26. G. Wen, S.B. Li, B.S. Zhang, and Z.X. Guo, Reaction synthesis of TiB2–TiC composites with enhanced toughness, Acta Mater., 49(2001), No. 8, p. 1463.10.1016/S1359-6454(01)00034-9 ↗
27. B. Lal and A. Dey, Fretting wear characteristics of Ti6Al4V/TiC nano composites using response surface method, Tribol. Int., 193(2024), art. No. 109412.10.1016/j.triboint.2024.109412 ↗
28. G. Singh, N. Sharma, D. Kumar, and H. Hegab, Design, development and tribological characterization of Ti–6Al–4V/hydroxyapatite composite for bio-implant applications, Mater. Chem. Phys., 243(2020), art. No. 122662.10.1016/j.matchemphys.2020.122662 ↗
29. R.M. German, Sintering: From Empirical Observations to Scientific Principles, Butterworth-Heinemann, New York, 2014.
30. A. Elsayed, W. Li, O.A. El Kady, W.M. Daoush, E.A. Olevsky, and R.M. German, Experimental investigations on the synthesis of W–Cu nanocomposite through spark plasma sintering, J. Alloy. Compd., 639(2015), p. 373.10.1016/j.jallcom.2015.03.183 ↗
31. M. Shokouhimehr, S.A. Delbari, A.S. Namini, et al., Nanostructure and nanoindentation study of pulse electric-current sintered TiB2–SiC–Cf composite, Sci. Rep., 13(2023), No. 1, art. No. 379.10.1038/s41598-022-27186-8 ↗
32. K.D. Sattler, Handbook of Nanophysics: Clusters and Fullerenes, CRC Press, Boca Raton, 2010.10.1201/9781420075496 ↗
33. Y. Wen, L.C. Xie, Z. Wang, L.Q. Wang, W.J. Lu, and L.C. Zhang, Nanoindentation characterization on local plastic response of Ti–6Al–4V under high-load spherical indentation, J. Mater. Res. Technol., 8(2019), No. 4, p. 3434.10.1016/j.jmrt.2019.06.009 ↗
34. M.E. Maja, O.E. Falodun, B.A. Obadele, S.R. Oke, and P.A. Olubambi, Nanoindentation studies on TiN nanoceramic reinforced Ti–6Al–4V matrix composite, Ceram. Int., 44(2018), No. 4, p. 4419.10.1016/j.ceramint.2017.12.042 ↗
35. S. Demirci, T. Dikici, and R. Dalmis, Nanoindentation and corrosion behavior of additively manufactured Ti–6Al–4V alloy for biomaterial applications, J. Mater. Eng. Perform., 33(2024), No. 5, p. 2133.10.1007/s11665-023-08139-2 ↗
36. M.W. Bai, R. Namus, Y.D. Xu, D.K. Guan, M.W. Rainforth, and B.J. Inkson, In-situ Ti–6Al–4V/TiC composites synthesized by reactive spark plasma sintering: processing, microstructure, and dry sliding wear behaviour, Wear, 432(2019), art. No. 202944.10.1016/j.wear.2019.202944 ↗
37. K. Miyoshi, J.H. Sanders, C.H. Hager Jr., et al., Wear behavior of low-cost, lightweight TiC/Ti–6Al–4V composite under fretting: effectiveness of solid-film lubricant counterparts, Tribol. Int., 41(2008), No. 1, p. 24.10.1016/j.triboint.2007.04.006 ↗
38. N. Dalili, A. Edrisy, K. Farokhzadeh, J. Li, J. Lo, and A.R. Riahi, Improving the wear resistance of Ti–6Al–4V/TiC composites through thermal oxidation (TO), Wear, 269(2010), No. 7–8, p. 590.10.1016/j.wear.2010.06.006 ↗
39. C.H. Hager Jr., J.H. Sanders, and S. Sharma, Effect of high temperature on the characterization of fretting wear regimes at Ti6Al4V interfaces, Wear, 260(2006), No. 4–5, p. 493.10.1016/j.wear.2005.03.011 ↗
40. O.E. Falodun, B.A. Obadele, S.R. Oke, et al., Influence of spark plasma sintering on microstructure and wear behaviour of Ti–6Al–4V reinforced with nanosized TiN, Trans. Nonferrous Met. Soc. China, 28(2018), No. 1, p. 47.10.1016/S1003-6326(18)64637-0 ↗
41. A.C. Fischer-Cripps, Critical review of analysis and interpretation of nanoindentation test data, Surf. Coat. Technol., 200(2006), No. 14–15, p. 4153.10.1016/j.surfcoat.2005.03.018 ↗
42. M.M. Khan and A. Dey, Selection of optimal processing condition during abrasive wear of in-situ ZA-37/TiCp composites using MCDM technique, Ceram. Int., 47(2021), No. 14, p. 20090.10.1016/j.ceramint.2021.04.016 ↗
43. N. Singh, R. Ummethala, P.S. Karamched, et al., Spark plasma sintering of Ti6Al4V metal matrix composites: Microstructure, mechanical and corrosion properties, J. Alloy. Compd., 865(2021), art. No. 158875.10.1016/j.jallcom.2021.158875 ↗
44. S.C. Liu, W.T. Hu, J.Y. Xiang, et al., Mechanical properties of nanocrystalline TiC–ZrC solid solutions fabricated by spark plasma sintering, Ceram. Int., 40(2014), No. 7, p. 10517.10.1016/j.ceramint.2014.03.024 ↗
45. N. Tian, L.L. Dong, H.L. Wang, et al., Microstructure and tribological properties of titanium matrix nanocomposites through powder metallurgy using graphene oxide nanosheets enhanced copper powders and spark plasma sintering, J. Alloy. Compd., 867(2021), art. No. 159093.10.1016/j.jallcom.2021.159093 ↗
46. V. Amigó, M.D. Salvador, F. Romero, C. Solves, and J.F. Moreno, Microstructural evolution of Ti–6Al–4V during the sintering of microspheres of Ti for orthopedic implants, J. Mater. Process. Technol., 141(2003), No. 1, p. 117.10.1016/S0924-0136(03)00243-7 ↗
47. Z.J. Wei, L. Cao, H.W. Wang, and C.M. Zou, Microstructure and mechanical properties of TiC/Ti–6Al–4V composites processed by in situ casting route, Mater. Sci. Technol., 27(2011), No. 8, p. 1321.10.1179/026708310X12699498462922 ↗
48. W.H. Wei, Z.N. Shao, J. Shen, and X.M. Duan, Microstructure and mechanical properties of in situ formed TiC-reinforced Ti–6Al–4V matrix composites, Mater. Sci. Technol., 34(2018), No. 2, p. 191.10.1080/02670836.2017.1366737 ↗
49. U. Ramamurty and J.I. Jang, Nanoindentation for probing the mechanical behavior of molecular crystals–a review of the technique and how to use it, CrystEngComm, 16(2014), No. 1, p. 12.10.1039/C3CE41266K ↗
50. W.C. Oliver and G.M. Pharr, Measurement of hardness and elastic modulus by instrumented indentation: advances in understanding and refinements to methodology, J. Mater. Res., 19(2004), No. 1, p. 3.10.1557/jmr.2004.19.1.3 ↗
51. A.L. Rominiyi and P.M. Mashinini, Nanoindentation study of mechanical and wear properties of spark plasma sintered Ti–6Ni–xTiCN composites, Ceram. Int., 49(2023), No. 2, p. 2194.10.1016/j.ceramint.2022.09.186 ↗
52. M.M. Khan and A. Dey, Hybrid MCDM approach for examining the high-stress abrasive wear behaviour of in situ ZA-27/TiCp MMCs, Mater. Chem. Phys., 277(2022), art. No. 125319.10.1016/j.matchemphys.2021.125319 ↗
53. S.A. Alidokht, V.N.V. Munagala, and R.R. Chromik, Role of third bodies in friction and wear of cold-sprayed Ti and Ti–TiC composite coatings, Tribol. Lett., 65(2017), No. 3, art. No. 114.10.1007/s11249-017-0899-4 ↗
54. V.N.V. Munagala, T.B. Torgerson, T.W. Scharf, and R.R. Chromik, High temperature friction and wear behavior of cold-sprayed Ti6Al4V and Ti6Al4V–TiC composite coatings, Wear, 426(2019), p. 357.10.1016/j.wear.2018.11.032 ↗