Influence of Ageing on Abrasion Volume Loss, Density, and Structural Components of Subfossil Oak
Source abstract
Abstract
Subfossil oak wood has spent centuries or millennia in the aquatic medium (rivers, lakes, bogs, etc.) and, due to water anoxic conditions, its decomposition is very slow. As a result of its long residing in specific conditions, its chemical composition, appearance, as well as mechanical and tribological properties have changed. Because of its aesthetic and mechanical properties, subfossil wood is very attractive and often used to produce valuable objects. The main objective of this study was to test how abrasion wear resistance of subfossil oak is affected by ageing. The effects of ageing on wood density and on the structure of lignin and cellulose were tested, as well as the loss of volume during abrasion in correlation with these changes. A study was conducted on samples of recent (regular) pedunculate oak wood and on six subfossil pedunculate oak samples in the age range of 890 and nearly 6000 years. Abrasion wear resistance was expressed through the loss of volume recorded using the Taber abraser. The smallest abrasion volume loss was measured for the recent oak specimens. Linear regression analyses showed that there was a very strong negative linear relationship between the age of subfossil oak and its abrasion volume loss. There was also a strong, but positive and significant linear correlation between subfossil oak age and density. Ageing also affected the structural composition of wood. Results obtained by Fourier Transform Infrared spectroscopy indicated a reduction of the relative crystalline fraction of subfossil wood in recent oak. The degradation of lignin in subfossil oak samples progressed more slowly over time than cellulose degradation. There was a negative correlation between age and the ratio of cellulose and lignin degradation; however, that relationship was found statistically insignificant. Similar results were obtained for the relationship between abrasion wear resistance and changes in the structural composition of the studied samples of subfossil oak wood.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Wood Treatment and Properties · Lignin and Wood Chemistry · Cultural Heritage Materials Analysis
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
Department of Materials, Faculty of Mechanical Engineering and Naval Architecture, University of Zagreb, Ivana Lučića 5, 10 000 Zagreb, Croatia
Division of Botany, Department of Biology, Faculty of Science, University of Zagreb, Marulićev trg 20/II, 10 000 Zagreb, Croatia
Division for Silviculture, Croatian Forest Research Institute, Cvjetno naselje 41, 10 450 Jastrebarsko, Croatia
References (40)
Show source-provided references
1. Physikalische, chemische und strukturelle Eigenschaften von rezentem und subfossilem Eichenholz10.1007/BF02607307 ↗
2. Comparison some physical and mechanical properties of abonos and recent oak (Quercus robur L.)
3. Broda, M., and Hill, C.A.S. (2021). Conservation of Waterlogged Wood—Past, Present and Future Perspectives. Forests, 12.10.3390/f12091193 ↗
4. Effects of aging on wood: A literature review10.1007/s00226-015-0766-0 ↗
5. Comparison between 10,000-year old and contemporary spruce lignin10.1007/s00226-008-0222-5 ↗
6. Aging and fossilization of wood and its components10.1007/BF00223468 ↗
7. Mössbauer studies of subfossil oak
8. Unique 6000 year old abonos furniture
9. Annual ring orientation effect on bending strength of subfossil elm wood10.1007/s10086-016-1596-x ↗
10. Effects of microstructural orientation on the abrasive wear resistance of subfossil elm wood in three orthogonal planes10.1016/j.wear.2017.03.001 ↗
11. The bending modulus of elasticity of subfossil elm wood
12. Kubovský, I., Kačíková, D., and Kačík, F. (2020). Structural changes of oak wood main components caused by thermal modification. Polymers, 12.10.3390/polym12020485 ↗
13. Use of a simple abrasive-wear resistance test device to assess the suitability of selected hardwoods for wood flooring
14. Micro-mechanical properties of Oak wood and comparison with standard-sized samples
15. Mania, P., and Tomczak, A. (2020). Properties of oak roundwood with and without frost cracks. Forests, 11.10.3390/f11050538 ↗
16. Bijak, S., and Lachowicz, H. (2021). Impact of tree age and size on selected properties of black locust (Robinia pseudoacacia L.) wood. Forests, 12.10.3390/f12050634 ↗
17. (2021). Standard Terminology Relating to Wear and Erosion (Standard No. ASTM G40-21a).
18. Abrasive wear properties of compressed sugi wood10.1007/BF00766642 ↗
19. Horvat, I. (1967). Drvnoindustrijski Priručnik, Tehnička knjiga.
20. Physical and mechanical properties of subfossil oak (Quercus, sp.) wood
21. The changes in chemical composition and properties of subfossil oak deposited in holocene sediments
22. Comparison of the chemical composition of the fossil and recent oak wood
23. Shrinkage and colour restoration of oakwood buried in the ground
24. Einfluß der Holzfeuchte auf die Druckfestigkeit von rezentem und subfossilem Eichenholz (Quercus robur L.)10.1515/hfsg.1990.44.3.211 ↗
25. Natural decay of archaeological oak wood versus artificial degradation processes—An FT-IR spectroscopy and X-ray diffraction study10.1016/j.saa.2018.10.057 ↗
26. Quantitative investigation of wood composition by integrated FT-IR and thermogravimetric methods
27. Monitoring wood degradation during weathering by cellulose crystallinity10.3390/ma5101910 ↗
28. (2022, January 19). Wikipedia, the Free Encyclopedia: Blank Maps. Available online: https://en.wikipedia.org/wiki/File:Blank_map_of_Europe_(with_disputed_regions).svg.
29. Schweingruber, F.H. (1990). Anatomy of European Woods, Paul Haupt.
30. Changes in physical properties of oak wood from historical constructions during service life/Spremembe fizikalnih lastnosti hrastovega lesa iz zgodovinskih konstrukcij v življenjski dobi
31. (2014). Physical and Mechanical Properties of Wood—Test Methods for Small Clear Wood Specimens—Part 1: Determination of Moisture Content for Physical and Mechanical Tests (Standard No. ISO 13061-1:2014).
32. (2014). Physical and Mechanical Properties of Wood—Test Methods for Small Clear Wood Specimens—Part 2: Determination of Density for Physical and Mechanical Tests (Standard No. ISO 13061-2:2014).
33. Nikolić, T. (2021, December 10). Flora Croatica Database. Prirodoslovno-Matematički Fakultet, Sveučilište u Zagrebu. Available online: https://hirc.botanic.hr/fcd.
34. Resolving the taxonomic status of the mysterious “green oak” (Quercus × viridis Trinajstić) from Croatia based on phylogenetic analysis
35. Šilić, Č. (2005). Dendroflora atlas (trees and shrubs) of Bosnia i Hercegovina. Matica Hrvat. Čitluk, 134–139.
36. The age and density of ancient and modern oak wood in streams and sediments10.1163/22941932-90000340 ↗
37. The selected properties of fossil oak wood from medieval burgh in P£oñsk
38. The effect of the natural degradation process on the cellulose structure of Moroccan hardwood fiber: A survey on spectroscopy and structural properties10.13171/mjc8319050801ab ↗
39. Structural analysis of photodegraded wood by means of FTIR spectroscopy10.1016/S0141-3910(03)00051-X ↗